www.pcimag.com/articles/90871-curative
Curative
June 1, 2010
Versamine® S 23 meets the need for benzyl alcohol, nonylphenol and bisphenol-A-free curatives with conventional or plural-component spray capability and that have excellent coating performance properties.
Cognis: Versamine® S 23 meets the need for benzyl alcohol, nonylphenol and bisphenol-A-free curatives with conventional or plural-component spray capability and that have excellent coating performance properties. It is designed to be used as a stand-alone curing agent due to its rapid cure response. Epoxy coatings based on Versamine S 23 have excellent chemical resistance properties.
Visit www.cognis.com
Visit www.cognis.com