www.pcimag.com/articles/90994-underwriters-labs-and-atlas-form-alliance

Underwriters Labs and Atlas Form Alliance

May 1, 2010

NORTHBROOK, IL – Underwriters Laboratories (UL), a third-party safety testing and certification provider, has entered into an alliance with Atlas Material Testing Technology, a leader in accelerated weathering instruments and weathering testing services. This alliance benefits both companies with increased global testing capacity and expertise in accelerated aging performance. It enables them to provide faster testing and certification turnaround time for manufacturers specializing in solar energy products.