www.pcimag.com/articles/91310-tester-1
Tester
November 1, 2010
Paul N. Gardner Co., Inc.: The Buchholz Indentation Tester BH2000 consists of a calibrated slip-on weight with a special cutter, an illuminated microscope, a level gage, a digital dual timer, two markers with template and three AAA batteries. The weight is positioned on the test specimen for a set period of time. The length of the indentation on the coating is an indication of the hardness of the surface.
Call 800/762.2478.