NeoRadâ„¢ U-6288 is a 100-percent UV-curable resin that offers broad formulating latitude and high matte efficiency, working with most common matting agents.

DSM NeoResins+: NeoRadâ„¢ U-6288 is a 100-percent UV-curable resin that offers broad formulating latitude and high matte efficiency, working with most common matting agents. Matte coatings and varnishes produced with this resin do not burnish, and exhibit superior chemical and abrasion resistance. Because of its low viscosity, the resin has improved flow and more effective pigment wetting.