Modifier

October 1, 2011

Croda: Priamine 1075 is a high-purity dimer diamine that can be used as a bio-based modifier of polyamide plastics or co-polyamide elastomers to make them flexible, even at low temperatures. It exhibits extreme hydrophobicity, allowing for faster drying and the reduction of moisture absorption. Providing improved adhesion to various substrates, it reduces the melt viscosity at equal molecular weight.