www.pcimag.com/articles/93543-extruder-purging
Extruder Purging
June 1, 2005
Nakan FEP 950 WN 000 grade has been developed specially to clean and purge the extruders used by manufacturers of thermosetting resin paint. A small quantity of the formulation (between 5 and 10 kg) is introduced straight into the extruder between two color changes to purge the equipment. The formulation mixes directly with color pigment residues, thereby cleaning up the machine.
Resilium by Arkema
resilium.info@arkemagroup.com
www.resilium.be