www.pcimag.com/articles/93931-coating-2005-exhibitors-highlights-heat-exchangers
Calorplast heat exchangers are made of PVDF, PP, PE and PFA, and are designed for heating or cooling in corrosive applications. They are available as immersion, tube-plate, flexible, compact shell and tube, and gas/ liquid exchangers. Features include all-welded thermoplastic construction, superior corrosion resistance, chemical inertness, no stray currents, low fouling characteristics, customized configurations, durable construction and a large heat transfer area within confined volume.
George Fischer
800-854-4090; www.georgefischer.com
Booth 1604