www.pcimag.com/articles/94220-molecular-sieve-desiccant

Molecular Sieve Desiccant

August 4, 2006


SPHINX ADSORBENTS, INC.: A new molecular sieve desiccant has been introduced for industrial desiccant dryers used in drying chemicals, plastics, fuels and gases. The desiccant reportedly features a high surface area, with high porosity to optimize adsorption, and provides a high crush strength to minimize loss from abrasion. Capable of purifying and drying in one operation, this molecular sieve desiccant has uniform bead sizes to prevent adsorbent segregation and is offered in cans, drums and supersacks. It can be supplied in several grades with precise pore sizes to match application requirements, and can be regenerated for repeated use. Call 413.736.5020 or visit www.sphinxadsorbents.com .