www.pcimag.com/articles/94338-basf-building-aeoa-plant-in-la

BASF Building AEOA Plant in La.

April 11, 2006
BASF is building an alkylethanolamine (AEOA) plant at its U.S. Verbund site in Geismar, Louisiana. The new plant, scheduled to come on line in 2007, complements existing amine production facilities at Geismar. The site currently manufactures some 20 different specialty amines. The new Geismar plant increases BASF's worldwide production capacities for these important intermediates by about 40 percent. BASF also operates AEOA plants at its Verbund site in Ludwigshafen, Germany.

AEOAs are mainly used as precursors for flocculants applied in water treatment. In addition they are utilized in the coatings industry where they act as binders between pigments and resins.