The AEB E-Beam Lab Unit is a compact and modular electron beam laboratory unit for evaluating the use of E-beams in a variety of curing, sterilization, materials modification and research, and process development applications. The system features a solid-state power supply and emitter subsystem that is designed to achieve up to 200 µm penetration without the active pumping and large footprint of conventional E-beam systems. Providing an 8.5" x 10" sample tray and an adjustable chamber for processing samples up to 2.5" H, the unit uses a touch-screen controller for changing the power and dose and is scalable in production environments.

Advanced Electron Beams, Inc.
(978) 658-8600
www.aeb.com