www.pcimag.com/articles/94737-equipment-three-angle-gloss-meter

EQUIPMENT: Three-Angle Gloss Meter

February 1, 2007
Paul N. Gardner Co., Inc.: The Novo-Gloss Trio three-angle gloss meter offers continuous read operation to provide information on gloss variations on large surfaces in seconds.



Paul N. Gardner Co., Inc.: The Novo-Gloss Trio three-angle gloss meter offers continuous read operation to provide information on gloss variations on large surfaces in seconds. It can be calibrated on a standard that matches a particular facility’s sample for improved gloss control. Additional standards are available, from matte to mirror finish. The instrument provides automatic calculation of batch statistics, as well as USB download of the data to Novo-Soft for further analysis, reporting and storage. It conforms to ISO 2813; STM D523, ASTM D2457; DIN 67530; JIS 8741. Call 800.762.2478 or visit www.gardco.com.