www.pcimag.com/articles/95388-nanocoatings-offer-long-term-gloss-retention-posted-3-5-07

Nanocoatings Offer Long-Term Gloss Retention - Posted 3/5/07

March 5, 2008

The Zyvere nanotechnology-based coatings from Nanovere Technologies are permanent, self-cleaning and car key resistant. According to the company, the coatings provide 100% gloss retention even after five years. The coatings reportedly offer 53% higher scratch resistance compared to conventional topcoats, along with a 6H pencil hardness; 60% better cleanability; and 476% higher chemical resistance. The nanocoatings were specifically designed to be applied over automotive OEM coatings, aftermarket finishes, aerospace paint, industrial coatings and marine coating surfaces.

For more information, call 877.998.3737, e-mail alliances@nanovere.com or visit www.nanocoatings.com.