Soliant LLC has been awarded the Global Plastics Environmental Conference (GPEC®) 2008 Achievement Award for "Enabling Technologies in Processes and Procedures" for developing Fluorex® bright film. The film is currently used on a variety of plastic substrates to provide a chrome finish comparable to chrome plating.
Soliant LLC has been awarded the Global Plastics Environmental Conference (GPEC®) 2008 Achievement Award for "Enabling Technologies in Processes and Procedures" for developing Fluorex® bright film. The film is currently used on a variety of plastic substrates to provide a chrome finish comparable to chrome plating.
According to the company, this sustainable alternative to chrome plating offers low emissions, excellent impact performance and 100% recyclability. The film is used in insert molding, extrusion lamination and thick sheet thermoforming.
Soliant met all GPEC Award criteria for "Sustainability and Recycling for a Greener Environment". The award was presented by the Plastics Environmental Division of the Society of Plastics Engineers (SPE) at a banquet during the GPEC conference March 11-12 in Orlando, FL.
For more information, visit www.paintfilm.com.
Soliant LLC has been awarded the Global Plastics Environmental Conference (GPEC®) 2008 Achievement Award for "Enabling Technologies in Processes and Procedures" for developing Fluorex® bright film. The film is currently used on a variety of plastic substrates to provide a chrome finish comparable to chrome plating.
According to the company, this sustainable alternative to chrome plating offers low emissions, excellent impact performance and 100% recyclability. The film is used in insert molding, extrusion lamination and thick sheet thermoforming.
Soliant met all GPEC Award criteria for "Sustainability and Recycling for a Greener Environment". The award was presented by the Plastics Environmental Division of the Society of Plastics Engineers (SPE) at a banquet during the GPEC conference March 11-12 in Orlando, FL.