Evonik: TEGO® Foamex 823 is a defoamer emulsion for waterborne coatings and printing inks. Due to its outstanding balance between defoaming power and compatibility, it is widely suitable in a variety of systems and applications. It reduces complexity in the lab and production, as it allows for the use of one defoamer instead of using a large number of specialty defoamers.