July 2, 2012
Three binder systems for use in cool roof coating applications allow greater formulation flexibility across different applications. Designed for the most demanding applications, the AC III Binder System uses a Kynar Aquatec® FMA-12 PVDF-based topcoat and ENCOR® Flex 187 all-acrylic basecoat to provide the highest possible level of performance and durability. The AC II Binder System utilizes a proprietary ENCOR Flex 187 all-acrylic polymer.

This base and topcoat system delivers excellent performance and meets ASTM D-6083, Standard Specification for Liquid Applied Acrylic Coating Used in Roofing. The AC I Binder System is an ENCOR Flex 3186 styrene acrylic system that provides a good mix of performance and value for less demanding applications.