www.pcimag.com/articles/97349-radtech-forms-new-uv-led-group

RadTech Forms New UV LED Group
January 6, 2013
BETHESDA, MD – RadTech - The Association for UV and EB Technologies has formed a new committee devoted to UV LED technology. The group’s first meeting is scheduled for Thursday, February 28, in Redondo Beach, CA, in conjunction with the industry trade event, uv.eb WEST.
“UV LED technology has the potential to play an essential role in radiation curing industrial applications,” says Beth Rundlett of DSM and committee co-chair. “RadTech’s technical efforts will further promote UV LED development and its full integration into everyday industrial processes.”
Those interested in participating in the upcoming survey should contact RadTech. All are welcome to the first RadTech UV LED meeting. Visit www.radtech.org for details.