Powder Coating
Fluon® ETFE powders from AGC Chemicals Americas Inc. are ideal for seamless rotolining of industrial equipment used in chemical processing applications in the food, petroleum and potable water/wastewater industries. Rotolining vessels with ETFE is superior to traditional sheet lining methods because the free-flowing powder naturally conforms to interiors and does not typically require welding and sealing. Fluon ETFE is a melt-processable copolymer of tetrafluoroethylene and ethylene. These powders possess outstanding physical toughness and high resistance to heat and chemical attack. They provide excellent bonding to metal, a seamless interior lining with a uniform thickness, the ability to conform to the interior of virtually any size and shape vessel, the option of post machining of critical surfaces, lining thickness up to 0.250”, and a mold-free process for reduced mold and tooling costs.
Visit www.agcchem.com.