The FireJet FJ100 air-cooled products from Phoseon Technology are for UV LED curing. These new UV light sources provide high irradiance in a small form factor, making them easy to integrate into space-limited environments. The products are available in multiple wavelengths (365, 385, 395, and 405nm), multiple curing lengths (75mm, 150mm, and 225mm) all with 20mm wide curing window. They are ideally suited for electronics manufacturing and assembly, wood coatings, and wide-format printing applications where small form factor but high-peak irradiance is vitally important.

"By simply placing the lamps end-to-end, the FJ100 products scale to length, providing greater flexibility and service options," said Joe Becker, Product Marketing Manager. "These quiet, air-cooled products easily integrate into low-noise environments where water cooling is prohibitive."