www.pcimag.com/articles/99222-fabrication-service
New Products

Fabrication Service

Charles Ross & Son Co.

June 1, 2014

 Providing one-stop fabrication service, Ross designs and builds storage tanks, pressure vessels and reactors for virtually any process or application. An example is a 300-gallon holding tank designed for 75 psig internal pressure at 350 °F and rated for full vacuum. It is equipped with a 50-psig baffled and insulated jacket and featured stainless steel type 316L wetted parts polished to 180 grit finish with all internal welds ground smooth and flush.  E-mail sales@mixers.com