www.pcimag.com/articles/99493-multi-source-viewing-systems

Multi-Source Viewing Systems
GTI Graphic Technology
August 8, 2014
GTI Graphic Technology's MiniMatcher series is ideal for the viewing of paints, inks, coatings, consumer goods, plastics, packaging and more. The ASTM D1729-2009 compliant MiniMatcher series includes up to five unique light sources and has viewing areas ranging from 13"H x 18"W x 10"D to 22"H x 60"W x 23"D.