New Biomaterial Impedes Bacteria on Metal Surfaces May 15, 2016 No Comments Researchers at Ben-Gurion University of the Negev (BGU) have developed an innovative anti-biofilm coating that has significant anti-adhesive potential for a variety of medical and industrial applications.Read More