Dispersion, Weathering and Performance of Inorganic Color Pigments

High performance inorganic color pigments have advantages when it comes to dispersion and weathering performance when compared to other pigments. Color stability and predictability improves color matching and production repeatability. The highly inert and colorful pigments in the CICP chemistries provide long lasting color for the most demanding applications.

Mark Ryan, Marketing Manager, Shepherd Color