Painting & Coating Industry (PCI) logo Powder coating summit logo
search
cart
facebook twitter linkedin youtube
  • Sign In
  • Create Account
  • Sign Out
  • My Account
Painting & Coating Industry (PCI) logo Powder coating summit logo
  • NEWS
    • Latest News
    • Market Trends & Reports
    • Finishing News
    • Price Alerts
    • Subscribe to Newsletters
    • Global Top 10/ PCI 25
    • Weekly Featured Article
    • COATLE Word Game
  • PRODUCTS
    • Product News
    • Featured Products
    • Must See Products and Services
  • MATERIALS
    • Additives
    • Resins/Polymers
    • Pigments
    • Equipment
    • Distributors
  • TECHNOLOGIES
    • Adhesives
    • Architectural Coatings
    • Finishing Articles
    • Finishing Technologies
    • Finishing Equipment
    • Industrial Coatings
    • Nanotechnology
    • Powder Coatings
    • Solventborne
    • Special Purpose Coatings
    • Sustainability
    • UV Coatings
    • Waterborne
  • RESOURCES
    • Columns
      • Did you know?
      • Distribution Dive
      • Formulating With Mike
      • Innovation Insights
      • Powder Coating Perspectives
      • TiO2 Insider
    • Blogs
      • Editor's Viewpoint
      • Industry Insights
    • Coatings Supplier Handbook
    • Podcasts and Videos
      • COAT-IT! Podcast
      • Videos/PCI TV
    • PCI Store
    • Classifieds
    • eBooks
    • Sponsor Insights
    • White Papers
    • COATLE Word Game
  • EVENTS
    • Coatings Trends & Technologies Summit
    • Paint and Coatings Academy
    • Webinars
    • Calendar of Events
    • Lifetime Achievement Award
  • DIRECTORIES
    • Buyer's Guide
    • Equipment Directory
    • Materials Directory
  • EMAGAZINE
    • Current Issue
    • eMagazine Archive
    • China Issue Archive
    • Editorial Advisory Board
  • CONTACT
    • Contact Us
    • Advertise
    • Subscribe to eMagazine
    • Subscribe to Newsletters
  • SIGN UP!
Paint and Coatings AdditivesSpecial Purpose CoatingsNanotechnology in CoatingsSolventborne CoatingsWaterborne Coatings

New Aspects in the Sustainability of Nanoparticle-Modified Coatings

By Robert H. McMullin
June 1, 2011
The demand for enhanced scratch and wear resistance in today’s clear and pigmented coatings is increasing. The idea of an everlasting surface that retains its initial properties is the driving force for the ongoing research in this field. This article discusses the different mechanisms for increasing the life cycle of solventborne and waterborne coatings by incorporation of predispersed nanoparticle oxides. These nano oxides provide better wear and UV protection, and are not released as nanoparticles into the environment.

Nanotechnology

Figure 1 Click to enlarge

Simply stated, a nanometer is a metric unit of length equal to one billionth of a meter. Nanotechnology is the study of the controlling parameters of materials in atomic and molecular scale. Generally, nanotechnology deals with structures of 100 nanometers or less in at least one dimension, and involves developing materials or devices of that size.

Nanoparticles are just like any other solid inorganic or organic particle that we try to incorporate into a resin matrix. If we just mix the particle into the solution, it will sink to the bottom because the solid particle has no compatible surface with the solution. It is similar to trying to float rocks on the surface of a lake. The rock is much denser than the water, and the water doesn’t have the required matrix to hold the rock at the surface.

Figure 1 represents the dispersion of nanoparticles into liquid media with a proper wetting and dispersing additive. This is imperative for the functionality of these solid particles in today’s coatings systems. More energy must be used to disperse nanoparticles than micro pigments because of their small size and high surface energies.

Figure 2 Click to enlarge

Once these solid nanoparticles are stabilized by steric hindrance or charge stabilization, they are easily mixed (1000 rpm for 2 min) into any compatible resin, clear or pigmented coating. Figure 2 shows the structures of controlled flocculation and deflocculation.

Dispersed Nanoparticles Enhance the Coating's Life Cycle

Additives containing alumina, silica, ceria and zinc oxide nanoparticles can provide improved wear and UV resistance for solvent, waterborne and UV coatings.  These nanoparticles are predispersed in different media and easily incorporated with low shear into aqueous, solventborne, or solvent-free UV-curing systems. They work by setting up a network within the resin matrix to make the coating more resistant to damage from daily marring and scratching.

Dispersed nanoparticles (alumina, zinc oxide and silica) can also improve corrosion resistance. This is accomplished through cathodic protection. This is a technique used to inhibit corrosion of buried or immersed structures by supplying an electrical charge that suppresses the electrochemical reaction. If correctly applied, corrosion can be stopped completely. In its simplest form, it is achieved by attaching a sacrificial anode, thus making the iron or steel the cathode in the cell formed. Due to the large surface area, nanoparticles are often more efficient than micro particles, resulting in lower concentration necessary to obtain good results.

Surfaces exposed to direct sunlight usually suffer from solar UV radiation that destroys organic compounds such as binders, polymers, organic pigments and substrates. Zinc oxide and cerium oxide nanoparticles can stop solar degradation by absorption of the UV radiation. They absorb UV light and transfer it into vibration and heat. By transferring the UV light, the level of energy is lowered and does not destroy the polymer matrix. This absorption method also protects the substrate by not allowing UV radiation to penetrate through the coating. Different from organic UV absorbers, inorganic UV absorbers do not suffer from UV light, resulting in long-term protection.

Typically, low dosages of nanoparticles, 0.5-2.0%, provide significant and long-term scratch, mar, wear, corrosion and UV resistance without adversely affecting gloss, color, clarity or other physical properties of the coatings.

Figure 3 Click to enlarge

Nano Stabilization

BYK has practiced the concept of pigment stabilization since the 1870s, and has developed over 300 different types of wetting and dispersing additives over the last 50 years to meet industry needs. From the simple cook process to controlled polymerization, we have developed additives and unique processes for stabilizing different types of nanoparticles.

Once these nanoparticles are stabilized with BYK’s propriety boundary phase technology, they can be predispersed in different media and easily incorporated with low shear into aqueous, solventborne or solvent-free UV-curing systems, or compounded into plastics.

Initially, I theorized that these nanoparticles were being totally coated (encapsulated) by the wetting, dispersing or silicone additive, similar to what happens to micronized pigment particles (creating a + charge around the pigment surface).

In 2006, I proposed that the nanoparticles form structural lines of particles similar to a string or strand of pearls throughout the clear resin matrix, thus forming a structure that strengthens the resin matrix. This string structure also gives the resin greater elasticity to endure the scratch and marring, rather than making the resin harder. This theory was confirmed in 2010 by the work of Matt Lane at Sandia National Laboratories, Albuquerque, NM (Figure 3).(1) This added credence to our work with dispersing nanoparticles and how these predispersed nanoparticles function within the coating.

Figure 4 Click to enlarge

Nanoparticles must be uniformly distributed throughout the coating to provide the resin or coating with a continuous, solid, protective network layer of Al2O3 or SiO2. This is the unique nano advantage. As a coating is worn away, additional layers of nanoparticles remain to resist continued scratching. The nanoparticles also form a unique elastomeric structure within the coating. This structure resists objects from entering the surface of the coating and promotes the reflow of the coating, thus preventing severe damage to the coating (Figure 4).

The nano silica and alumina particles not only offer scratch resistance but can provide greater wear resistance, better adhesion and anti-staining because the nanoparticles create a denser, more compact film structure.

Figure 5 Click to enlarge

Under normal conditions we consider a scratch and mar coating failure to occur when a coating loses 10% of it’s original gloss. The control had a starting gloss at 85º, while the nanocoating started at 90º gloss. Figure 5 shows that the control lost over 10% of its gloss after 150 cycles. The control continued to have the surface damaged until the gloss was below 20º after 800 cycles. This gives an indication that the control is not good for long-term scratch and mar resistance

The same coating with the addition of 2% silica in TPGDA did not lose 10% of its gloss until 1100 cycles. The nanocoating continued to have a gloss above 70º at 2000 cycles. This shows that the nanocoating was ten times better in scratch and mar resistance than the control. This is a good example of nanoparticles being able to improve the life cycle of the coating.

Nanoparticles Improve Corrosion Resistance

Nanoparticles are uniformly distributed throughout the coating, thus providing the resin or coating with a continuous, solid, protective network layer of Al2O3 or SiO2. The nanoparticles also form a unique elastomeric structure within the coating, and create a denser, more compact film structure. Cathodic protection is a technique used to inhibit corrosion by supplying an electrical charge that suppresses the electrochemical reaction. If correctly applied, corrosion can be stopped completely. In its simplest form it is achieved by attaching a sacrificial anode, thus making the iron, steel or aluminum the cathode in the cell formed. Nanoparticles have a large amount of electrons -on their surface, which can create this sacrificial anode. This again is one of my theories of the functioning of nanoparticles for corrosion resistance.

Figure 6 Click to enlarge

Figure 6 shows that under 40X magnification, the creepage of the rust on the control panel was at least five times larger than the coating with the nanoparticles added. When you look at the magnification of the nanocoating, you can see there is almost no creepage after 580 h of salt spray. This was an automotive OEM clearcoat coating over ED coating on steel. The nanoparticles were post added to the formula and sprayed. This shows that nanoparticles can add a longer life to the automotive OEM coating.

Figure 7 shows a water-reducible, direct-to-metal primer. The primer with no corrosion control additives showed complete failure after 260 h of salt spray. The standard corrosion package at 500 h salt spray showed heavy rust, and when scratched showed a 2 millimeter under creepage. The nanocoating showed almost no rust after 500 h, and when scratched had no under creepage. Helping to slow down corrosion is another way nanoparticles increase the life cycle of a coating.

Figure 7 Click to enlarge

Amongst inorganic UV absorbers, zinc oxide and cerium oxide stand out with almost complete adsorption of UV-A, B and C. Reduction of particle size from micron to nanoscale enables the formulator to formulate clear coatings or adhesives that can both enhance the appearance of substrates as well as provide long-term protection for wood, metal and plastic substrates against UV degradation. Inorganic UV absorbers can outperform chemical UV absorbers because they are more permanent within the resin or coating, whereas the chemical UV absorbers gradually degrade over time within the resin (Figure 8).

Safety of Nanodispersions

Questions regarding the impact of released nanoparticles from use and wear remain. BYK worked with the German Government and NIST to evaluate nanoparticles in coatings. Two studies have been completed. The first study provided results by Tabor abrader. The article, titled Method for the Characterization of the Abrasion-Induced Nanoparticle Release into Air from Surface Coatings, was published September 30, 2008, in Elsevier Aerosol Science. The study concluded, “During the abrasion test no significant release of particle concentrations (<100 nm) was generated in the aerosol flow. Therefore the nanoparticles are probably embedded in the generated wear. This could be confirmed with SEM, TEM and EDX. The nanoparticles were clearly visible and embedded in the resin and showed the characteristic morphology of the zinc oxide.”
 

Figure 8 Click to enlarge

The second study provided results by sanding. The article, titled Characterization of Nanoparticle Release from Surface Coatings by Simulation of a Sanding Process, was published August 2, 2010, via the internet http://annhyg.oxfordjournals.org. “This conclusion agrees with the first study, that during abrasion test no significant release of particle concentrations (<100 nm) was generated.”

The studies were conducted by the Research Group Mechanical Process Engineering, Institute of Process Engineering and Environmental Technology, Techhnische Universitat Dresden, by Daniel Gohler, Michael Stintz, Lars Hillemann and Manuel Vorbau.

Conclusion

Based on our studies, we conclude that predispersions of nanoparticles:
 

  • Are easy to mix into coatings;

  • Provide homogeneous distribution of nanoparticles in the coating film;

  • Prevent coating damage by innovative, immediate reflow effect;

  • Absorb the impacting energy like a shock absorber;

  • Do not increase the brittleness or reduce chemical resistance;

  • Are suitable for all systems, from low to high polarity.

This is why we believe predispersed nanoparticles can be very beneficial to the life cycle of coatings. Nanoparticles have a lot to offer to the coatings industry. This is new technology, and we can truly say, “We have only scratched the surface.” There is much more still undiscovered.

This paper was presented at the 38th Annual Waterborne Symposium, February 2011, in New Orleans.

For more information, contact Robert McMullin at Robert.mcmullin@altana.com.


Appendix

Testing Procedures
The incorporation of additives into the coating formulations was as follows:

  • The additives were post added using a Dispermat CV with a 40 mm Cowles blade at 600 rpm for 2 min. In case of combination of wax and nano, the wax was added first at 600 rpm for 2 min and then nano at 600 rpm for 2 min.

  • Additives dosage

Nano Al2O3 or SiO2, wax, acrylates and silicones

All additives dosages mentioned are based on total formula weight (tfw).

Application
Substrate: Masonite board (for abrasion test), Leneta chart (for scratch test), hot rolled steel, cold rolled steel and aluminum panels (for corrosion testing).
Application tool: wire-wound bar, draw down bars and low-pressure, high-volume spray.
Coats: 3 on Masonite board and 1 on Leneta chart, 1 coat on metal panels.
Thickness: 4 mil wet of each coat. Thickness of dry film depends of percent solids of coating.
Dry time: 2 h between each coat and at least 48 h after final coat for corrosion testing seven days before scribing and placing into salt spray.
Sanding: after 2 h drying of 1st and 2nd coat, with a very fine sandpaper (220 grit) to ensure proper adhesion of additional coats.

Scratch Test
Each sample drawdown was evaluated for scratch resistance with 20 double rubs using 9 micron polishing paper pads on abrasion tester (dry) from BYK-Gardner. Gloss (20º) (60º) was measured (statistical average of 5 readings) using micro-TRI-gloss from BYK-Gardner before and after scratching the panels. Percent gloss retention was also calculated as follows

% Gloss Retention =   100  x  Gloss (60º) of scratched area

                        Original gloss (60º)

% Gloss Retention = 100 x     Gloss (20º) of scratched area

                        Original gloss (20º)

Testing for scratch covers both areas of mar and scratch

Abrasion Test
ISO 9352 or ASTM D 1044.
Taber Abraser (from TABER Industries)
CS-10 abrading wheel, 1000 gm load, 100, 250, 500, 750, and 1000 cycles

Pendulum Hardness Test – König
After allowing the coating to dry for 8 h, and 48 h, a König pendulum hardness test was run. More objective than using pencil hardness testing.

Light Microscopy
A light microscopic image of each sample coating was taken after scratch test. Images were taken by MOTIC lens at 40X magnification.

KEYWORDS: Corrosion Control

Share This Story

Looking for a reprint of this article?
From high-res PDFs to custom plaques, order your copy today!

Manager Nanotechnology, NAFTA, BYK USA Inc., Wallingford, CT

Recommended Content

JOIN TODAY
to unlock your recommendations.

Already have an account? Sign In

  • pci1022-Kinaltek-Lead-1170.jpg

    A Novel Pigment Production Technology

    Following an extensive R&D program that demonstrated...
    Paint and Coating Pigments
    By: Jawad Haidar and Nitin Soni
  • pci global top 10

    2025 Global Top 10: Top Paint and Coatings Companies

    The following is PCI’s annual ranking of the top 10...
    Paint and Coating Market Reports
    By: Courtney Bassett
  • 2025 pci 25

    2025 PCI 25: Top Paint and Coatings Companies

    PCI's annual ranking of the top 25 North American paint...
    Global Top 10 and PCI 25
    By: Courtney Bassett
You must login or register in order to post a comment.

Report Abusive Comment

Manage My Account
  • eMagazine
  • Newsletters
  • Online Registration
  • Subscription Customer Service

More Videos

Sponsored Content

Sponsored Content is a special paid section where industry companies provide high quality, objective, non-commercial content around topics of interest to the PCI audience. All Sponsored Content is supplied by the advertising company and any opinions expressed in this article are those of the author and not necessarily reflect the views of PCI or its parent company, BNP Media. Interested in participating in our Sponsored Content section? Contact your local rep!

close
  • wooden kitchen set and shelving
    Sponsored bySirca North America

    Leveraging Coatings to Meet ESG Goals in Manufacturing

  • man woodworking in workshop
    Sponsored byGemini Industries, Inc.

    Waterborne Coatings Aren't the Future -- They're the New Performance Benchmark

Popular Stories

Akzo, SW, Nippon Logos

AkzoNobel Rejects Cash Offer From Nippon Paint, Sherwin-Williams

BASF SE Logo

BASF Announces Strategic Business Sale

AkzoSWNipponEndTalks

Nippon Paint, Sherwin-Williams End AkzoNobel Pursuit

POB-Point-and-Shoot

PCI Buyers Guide

Submit a Request for Proposal (RFP) to suppliers of your choice with details on what you need with a click of a button

Start your RFP

Browse our Buyers Guide for manufacturers and distributors of all types of coatings products and much more!

Find Suppliers

Events

September 4, 2025

N-Butylpyrrolidone (NBP) as a Green Solvent to Replace N-Methylpyrrolidone (NMP) in Industrial Coating Applications

ON DEMAND: EPA published a regulation proposal around N-methylpyrrolidone (NMP) in June 2024 to ban or limit NMP in many applications, such as paints and coatings and their removers. N-butylpyrrolidone (NBP) is a powerful and versatile solvent for a variety of industries looking for alternatives to substance of very high concern (SVHC)-listed solvents.

September 15, 2026

Coatings Trends & Technologies Summit

The Coatings Trends & Technologies (CTT) Summit is an annual conference for both liquid and powder coatings formulators and manufacturers to discuss innovations in coatings technology. This event combines high-quality technical presentations, a resource-rich exhibit hall, and dedicated networking opportunities to connect scientific minds, foster innovation, and cultivate game-changing new ideas!

View All Submit An Event

Poll

Longest-running laboratory experiment

What is the longest-running laboratory experiment?
View Results Poll Archive

Products

Automotive Paints and Coatings, 2nd Edition

Now in its second edition and still the only book of its kind, this is an authoritative treatment of all stages of the coating process.

See More Products
Inside the AI Shift in Coatings - See the article now

Related Articles

  • Tuesday’s Keynote Address Discusses the Future of Sustainability in the Coatings Industry

    See More
  • When New Product Development in the Coatings Industry is Hampered by a Catch 22

    See More
  • Sustainability in the Coatings Industry: 2018 Calls for Commitment, Measurement and Delivery

    See More

Related Products

See More Products
  • Adhesion, Surface Aspects & Coatings Defects (Virtual Course - 10/22/26)

  • durability.jpg

    Increasing the Durability of Paint and Varnish Coatings in Building Products and Construction 1st Edition

  • Failure Analysis of Paints and Coatings, Revised Edition

See More Products

Related Directories

  • BASF Corp., Dispersions, Resins & Additives

    BASF offers a strong portfolio of industry-leading additives for the Coatings Industry to deliver eco-efficient solutions that meet performance requirements. The BASF Performance and Formulation additives portfolio encompasses a technology base of dispersing agents, wetting agents and surface modifiers, defoamers, rheology modifiers, film forming agents, antioxidants, light stabilizers and UV absorbers.
×

Keep the info flowing with our eNewsletters!

Get the latest industry updates tailored your way.

JOIN TODAY!
  • RESOURCES
    • Advertise
    • Contact Us
    • Directories
    • Store
    • Want More
    • Manufacturing Division
  • SIGN UP TODAY
    • Create Account
    • eMagazine
    • Newsletters
    • Customer Service
    • Manage Preferences
  • SERVICES
    • Marketing Services
    • Reprints
    • Market Research
    • List Rental
    • Survey & Sample
  • STAY CONNECTED
    • LinkedIn
    • Facebook
    • Youtube
    • X (Twitter)
  • PRIVACY
    • PRIVACY POLICY
    • TERMS & CONDITIONS
    • DO NOT SELL MY PERSONAL INFORMATION
    • PRIVACY REQUEST
    • ACCESSIBILITY

Copyright ©2026. All Rights Reserved BNP Media, Inc. and BNP Media II, LLC.

Design, CMS, Hosting & Web Development :: ePublishing