Painting & Coating Industry (PCI) logo Powder coating summit logo
search
cart
facebook twitter linkedin youtube
  • Sign In
  • Create Account
  • Sign Out
  • My Account
Painting & Coating Industry (PCI) logo Powder coating summit logo
  • NEWS
    • Latest News
    • Market Trends & Reports
    • Finishing News
    • Price Alerts
    • Subscribe to Newsletters
    • Global Top 10/ PCI 25
    • Weekly Featured Article
    • COATLE Word Game
  • PRODUCTS
    • Product News
    • Featured Products
    • Must See Products and Services
  • MATERIALS
    • Additives
    • Resins/Polymers
    • Pigments
    • Equipment
    • Distributors
  • TECHNOLOGIES
    • Adhesives
    • Architectural Coatings
    • Finishing Articles
    • Finishing Technologies
    • Finishing Equipment
    • Industrial Coatings
    • Nanotechnology
    • Powder Coatings
    • Solventborne
    • Special Purpose Coatings
    • Sustainability
    • UV Coatings
    • Waterborne
  • RESOURCES
    • Columns
      • Did you know?
      • Distribution Dive
      • Formulating With Mike
      • Innovation Insights
      • Powder Coating Perspectives
      • TiO2 Insider
    • Blogs
      • Editor's Viewpoint
      • Industry Insights
    • Coatings Supplier Handbook
    • Podcasts and Videos
      • COAT-IT! Podcast
      • Videos/PCI TV
    • PCI Store
    • Classifieds
    • eBooks
    • Sponsor Insights
    • White Papers
    • COATLE Word Game
  • EVENTS
    • Coatings Trends & Technologies Summit
    • Paint and Coatings Academy
    • Webinars
    • Calendar of Events
    • Lifetime Achievement Award
  • DIRECTORIES
    • Buyer's Guide
    • Equipment Directory
    • Materials Directory
  • EMAGAZINE
    • Current Issue
    • eMagazine Archive
    • China Issue Archive
    • Editorial Advisory Board
  • CONTACT
    • Contact Us
    • Advertise
    • Subscribe to eMagazine
    • Subscribe to Newsletters
  • SIGN UP!

Mother of Pearl Secret Revealed

By Lynn Yarris
March 2, 2009
Robby Gordon’s No. 7 car featured the logo and shimmering brilliant look of Planet Color®, the custom color paint system from Sherwin-Williams Automotive Finishes Corp.



In addition to its iridescent beauty, mother of pearl, or nacre, the inner lining of the shells of abalone, mussels and certain other mollusks, is also renowned for an amazing strength and toughness that has been a long-standing mystery. Now, scientists have brought to light a new aspect of nacre's nanostructural architecture using the polarized x-ray beams and nanoscale imaging capabilities of the Advanced Light Source (ALS), a national synchrotron facility at the U.S. Department of Energy's Lawrence Berkeley National Laboratory (Berkeley Lab).

Pupa Gilbert, a physics professor at the University of Wisconsin-Madison who led this research, says "Nacre is a biomineral composed of thin layers of crystalline aragonite tablets separated by even thinner layers of organic material. Our studies have revealed that the aragonite tablet crystals in nacre are misoriented with respect to each other. This unique structural arrangement was a surprise and could play a role in nacre's remarkable resistance to fracture."

Approximately 95-percent of nacre's composition is aragonite, a hard but brittle calcium carbonate mineral, yet nacre is 3,000 times tougher than aragonite. No human-synthesized composite can outperform its component materials by such a wide margin. Hence nacre has been intensely studied, particularly in the ceramics and nanotechnology industries where brittleness remains a major limitation. The goal is to learn how nacre formation occurs in nature so that new microstructures might be engineered for ceramics and other materials that would increase their toughness. However, researchers in the past lacked the tools needed to study the dynamics of nacre formation at the nanoscale. Now, new capabilities at the ALS, including polarized beams of x-rays, have made this possible.

Gilbert and her colleagues reported their findings in the Journal of the American Chemical Society, in a paper entitled: "Gradual Ordering in Red Abalone Nacre." Co-authoring the paper with Gilbert were Rebecca Metzler, Dong Zhou and Susan Coppersmith, of the University of Wisconsin, and Andreas Scholl, Andrew Doran, Anthony Young, Martin Kunz and Nobumichi Tamura of Berkeley Lab.

Nacre in the ALS Spotlight

The ALS is an electron synchrotron that accelerates electrons to energies of 1.9 billion electron volts (GeV), focuses them into a tight beam and sends this beam around a storage ring for several hours. While in the storage ring, beams of ultraviolet and x-ray light are extracted from the electron beam through the use of either bending, wiggler, or undulator magnetic devices. These beams are a hundred million times brighter than those from the best x-ray tubes and can be tuned to match a range of scientifically important wavelengths.

ALS Beamline 11.0.1 features one of the world's best photoemission electron microscopes, the PEEM-3, which is powered by an elliptically polarizing undulator. Shining a beam on a sample in the PEEM-3 causes the sample's atoms, molecules or crystals to emit electrons that are then imaged to reveal the location and structural arrangement of the emitting atoms, molecules and crystals.

"We used PEEM-3 to study the nacre of red abalone (Haliotis rufescens) and obtained unprecedented details and quantitative information about the location, size, and relative orientation of individual aragonite tablets," says Gilbert. "PEEM-3 gave us exquisite nanoscale spatial resolution and a large field of view that could include hundreds of tablets at once with negligible radiation damage."

Co-author Scholl, who manages PEEM-3 at ALS Beamline 11.0.1, says "PEEM-3's ability to control polarization, one of the new features that we can offer our users, was essential for determining the crystal orientation of the aragonite tablets. Polarized x-rays interact differently with an oriented crystal depending on the relative orientation of crystal axis and x-ray polarization. Also essential was PEEM-3's very high spatial resolution because of the nanometer dimensions of the crystallites and the organic spacer material."

Competition for Space

Under the probing polarized light of PEEM-3, Gilbert and her colleagues obtained measurements of aragonite crystal orientation, tablet size and tablet stacking direction. These measurements revealed that different orientations of the aragonite crystals result in different tablet growth rates. In turn, these different table growth rates give rise to self-ordering, which progressively selects faster and faster growing tablets. Furthermore, this self-ordering takes place gradually over a distance of approximately 50 microns.

"Our results suggest that at least one aspect of nacre formation, the self-ordering of the aragonite tablets occurs independently of biological or organic-molecule control," said Gilbert. "Although this discovery shakes the generally accepted idea of organic-mineral templation in biomineralization, it is typical of evolving kinetic systems in nature to select for the fastest growing elements of a material."

From these results Gilbert and co-author Coppersmith hypothesized a "competition for space" theoretical model of nacre assembly, based on the gradual, kinetic selection of faster tablet growth rates and a small probability of nucleating new crystal orientations. The results of their model were found to be in remarkable agreement with side-view and in-plane experimental data.

One crucial piece that was still missing from the picture of nacre formation that Gilbert and her coauthors were putting together was information of the quantitative extent of the aragonite crystal misorientation both near and far from the boundary between nacre and the prismatic outer layer of the shell. According to Gilbert's hypothesis, the degree of orientational order of the aragonite tablets should increase with distance from the nacre-prismatic boundary. For this information, she turned to ALS Beamline 12.3.2, the x-ray microdiffraction facility.

Explains coauthor Tamura, who manages the x-ray microdiffraction beamline, "Our facility is capable of measuring with high spatial resolution and accuracy the orientation of individual aragonite tablets in nacre using a technique called white beam x-ray microdiffraction. For this study, we were able to do the measurements in a few hours and the crystal orientation numbers came out once we analyzed the data – the angular spread of the aragonite crystals misorientation goes from 24 degrees at the prismatic boundary down to 6 degrees a few tens of microns away."

The next step in this research, Gilbert says, is to extend the nacre study from red abalone, which is a gastropod mollusk, to the shells of other mollusks, including bivalves, such as certain oysters and mussels, and cephalopods, such as nautilus. Nacre in red abalone and nautilus is of a type known as "columnar," while the nacre in bivalves is of a type known as "sheet." It is already known that the formation mechanism for sheet nacre differs from that for columnar nacre.

Says Gilbert, "We are now working to acquire more PEEM-3 data on other nacre-forming shells, and simultaneously develop two separate theoretical models for nacre formation, one for sheet nacre and one for columnar nacre. These will be much more sophisticated models than what we have now."

This research was supported by awards from both the National Science Foundation and the U.S. Department of Energy's Office of Science.

About Berkeley Lab
Berkeley Lab is a U.S. Department of Energy national laboratory located in Berkeley, California. It conducts unclassified scientific research and is managed by the University of California.

Share This Story

Looking for a reprint of this article?
From high-res PDFs to custom plaques, order your copy today!

Berkeley, CA

Recommended Content

JOIN TODAY
to unlock your recommendations.

Already have an account? Sign In

  • pci1022-Kinaltek-Lead-1170.jpg

    A Novel Pigment Production Technology

    Following an extensive R&D program that demonstrated...
    Paint and Coating Pigments
    By: Jawad Haidar and Nitin Soni
  • pci global top 10

    2025 Global Top 10: Top Paint and Coatings Companies

    The following is PCI’s annual ranking of the top 10...
    Paint and Coating Market Reports
    By: Courtney Bassett
  • 2025 pci 25

    2025 PCI 25: Top Paint and Coatings Companies

    PCI's annual ranking of the top 25 North American paint...
    Paint and Coating Market Reports
    By: Courtney Bassett
You must login or register in order to post a comment.

Report Abusive Comment

Manage My Account
  • eMagazine
  • Newsletters
  • Online Registration
  • Subscription Customer Service

More Videos

Sponsored Content

Sponsored Content is a special paid section where industry companies provide high quality, objective, non-commercial content around topics of interest to the PCI audience. All Sponsored Content is supplied by the advertising company and any opinions expressed in this article are those of the author and not necessarily reflect the views of PCI or its parent company, BNP Media. Interested in participating in our Sponsored Content section? Contact your local rep!

close
  • wooden kitchen set and shelving
    Sponsored bySirca North America

    Leveraging Coatings to Meet ESG Goals in Manufacturing

  • man woodworking in workshop
    Sponsored byGemini Industries, Inc.

    Waterborne Coatings Aren't the Future -- They're the New Performance Benchmark

Popular Stories

Akzo, SW, Nippon Logos

AkzoNobel Rejects Cash Offer From Nippon Paint, Sherwin-Williams

BASF SE Logo

BASF Announces Strategic Business Sale

AkzoSWNipponEndTalks

Nippon Paint, Sherwin-Williams End AkzoNobel Pursuit

POB-Point-and-Shoot

PCI Buyers Guide

Submit a Request for Proposal (RFP) to suppliers of your choice with details on what you need with a click of a button

Start your RFP

Browse our Buyers Guide for manufacturers and distributors of all types of coatings products and much more!

Find Suppliers

Events

September 4, 2025

N-Butylpyrrolidone (NBP) as a Green Solvent to Replace N-Methylpyrrolidone (NMP) in Industrial Coating Applications

ON DEMAND: EPA published a regulation proposal around N-methylpyrrolidone (NMP) in June 2024 to ban or limit NMP in many applications, such as paints and coatings and their removers. N-butylpyrrolidone (NBP) is a powerful and versatile solvent for a variety of industries looking for alternatives to substance of very high concern (SVHC)-listed solvents.

September 15, 2026

Coatings Trends & Technologies Summit

The Coatings Trends & Technologies (CTT) Summit is an annual conference for both liquid and powder coatings formulators and manufacturers to discuss innovations in coatings technology. This event combines high-quality technical presentations, a resource-rich exhibit hall, and dedicated networking opportunities to connect scientific minds, foster innovation, and cultivate game-changing new ideas!

View All Submit An Event

Poll

Longest-running laboratory experiment

What is the longest-running laboratory experiment?
View Results Poll Archive

Products

Automotive Paints and Coatings, 2nd Edition

Now in its second edition and still the only book of its kind, this is an authoritative treatment of all stages of the coating process.

See More Products
Inside the AI Shift in Coatings - See the article now

Related Articles

  • Secret Screening Solutions Revealed

    See More
  • The Mother of Invention

    See More
  • A World of Color Revealed on Iphone

    See More

Related Products

See More Products
  • Handbook of Adhesives and Surface Preparation

  • Principles and Applications of Emulsion Polymerization

  • Failure Analysis of Paints and Coatings, Revised Edition

See More Products
×

Keep the info flowing with our eNewsletters!

Get the latest industry updates tailored your way.

JOIN TODAY!
  • RESOURCES
    • Advertise
    • Contact Us
    • Directories
    • Store
    • Want More
    • Manufacturing Division
  • SIGN UP TODAY
    • Create Account
    • eMagazine
    • Newsletters
    • Customer Service
    • Manage Preferences
  • SERVICES
    • Marketing Services
    • Reprints
    • Market Research
    • List Rental
    • Survey & Sample
  • STAY CONNECTED
    • LinkedIn
    • Facebook
    • Youtube
    • X (Twitter)
  • PRIVACY
    • PRIVACY POLICY
    • TERMS & CONDITIONS
    • DO NOT SELL MY PERSONAL INFORMATION
    • PRIVACY REQUEST
    • ACCESSIBILITY

Copyright ©2026. All Rights Reserved BNP Media, Inc. and BNP Media II, LLC.

Design, CMS, Hosting & Web Development :: ePublishing