WARSAW, Poland – LOT Polish Airlines (Polskie Linie Lotnicze LOT) has chosen a new chrome-free aerospace primer coatings system by PPG for corrosion resistance because it is eco-friendly and a preferred PPG topcoat for superior gloss and shine to repaint three Embraer E175 jets and a 737-400 airplane.
High-solids DESOPRIME™ 7065 chrome-free polyurethane primer applied over Desoprime CFWP 7530 chrome-free wash primer pretreatment are designed to work together to inhibit corrosion. The LOT Polish Airlines aircraft also are being painted with high-solids DESOTHANE® HS 8800 buffable topcoat by PPG.