Award Winners Recognized at 2012 Waterborne Symposium
NEW ORLEANS - The 39th Annual Waterborne Symposium took place February 13-17, 2012 at the New Orleans Marriott, New Orleans, LA. The Waterborne 2012 Awards Ceremony, held in conjunction with the symposium, recognized the winners of the PCI Award for Technical Excellence, the Shelby F. Thames Best Paper Award and the Best Student Paper Award. Also recognized at the ceremony were winners of the student poster competition.
The PCI Award for Technical Excellence was given to Matthew Linares, Evonik Degussa Corp., for his paper “Novel Matting Agent for Low Gloss UV Coatings.” Co-Authors were Hans-Dieter Christian, Reinhard Behl, Andreas Feller and Maria Nargiello.