New Technology Enables Powder Coating for Plastics, Composites and Other Nonmetallic Substrates
MONTROSE, CO – InnoVoc Solutions, a division of Gordon Composites, Inc., announced a breakthrough technology for powder coating plastics, composites and other nonconductive substrates. This licensed technology makes nonmetallic substrates temporarily conductive using a surface treatment that emits no VOCs or other hazardous byproducts.