Painting & Coating Industry (PCI) logo Powder coating summit logo
search
cart
facebook twitter linkedin youtube
  • Sign In
  • Create Account
  • Sign Out
  • My Account
Painting & Coating Industry (PCI) logo Powder coating summit logo
  • NEWS
    • Latest News
    • Market Trends & Reports
    • Finishing News
    • Price Alerts
    • Subscribe to Newsletters
    • Global Top 10/ PCI 25
    • Weekly Featured Article
    • COATLE Word Game
  • PRODUCTS
    • Product News
    • Featured Products
    • Must See Products and Services
  • MATERIALS
    • Additives
    • Resins/Polymers
    • Pigments
    • Equipment
    • Distributors
  • TECHNOLOGIES
    • Adhesives
    • Architectural Coatings
    • Finishing Articles
    • Finishing Technologies
    • Finishing Equipment
    • Industrial Coatings
    • Nanotechnology
    • Powder Coatings
    • Solventborne
    • Special Purpose Coatings
    • Sustainability
    • UV Coatings
    • Waterborne
  • RESOURCES
    • Columns
      • Did you know?
      • Distribution Dive
      • Formulating With Mike
      • Innovation Insights
      • Powder Coating Perspectives
      • TiO2 Insider
    • Blogs
      • Editor's Viewpoint
      • Industry Insights
    • Coatings Supplier Handbook
    • Podcasts and Videos
      • COAT-IT! Podcast
      • Videos/PCI TV
    • PCI Store
    • Classifieds
    • eBooks
    • Sponsor Insights
    • White Papers
    • COATLE Word Game
  • EVENTS
    • Coatings Trends & Technologies Summit
    • Paint and Coatings Academy
    • Webinars
    • Calendar of Events
    • Lifetime Achievement Award
  • DIRECTORIES
    • Buyer's Guide
    • Equipment Directory
    • Materials Directory
  • EMAGAZINE
    • Current Issue
    • eMagazine Archive
    • China Issue Archive
    • Editorial Advisory Board
  • CONTACT
    • Contact Us
    • Advertise
    • Subscribe to eMagazine
    • Subscribe to Newsletters
  • SIGN UP!

A New Class of Weather-Fast Pigments

April 1, 2005
Every day, color formulators are challenged to select affordable pigments for coatings required for durable applications. Their choices are restricted due to environmental and performance concerns. Rockwood Pigments offers a novel chemistry that provides unique solutions in the yellow and orange color space.

A New Pigment Chemistry

The Solaplex™ range is a new class of inorganic pigment, CI Pigment Yellow 216. This soft, spherical complex consists of a tin-zinc-titania compound. This range is free of encapsulation and surface treatment and, thus, is compatible with a wide range of polymers and vehicles. The pigment is shown in the scanning electron micrograph (SEM) (Figure 1).

Unique Color Space

The Solaplex range occupies a unique color space, as shown in Figure 2, that consists of yellow, mid yellow and orange. These pigments exhibit opaque, clean, high-chroma shades in mass tone and clean in reduced shades. The color and shade intensity lies between lead chromates and conventional nickel and chrome titanates.

Solaplex inorganic pigments are ideal alone or in combination with high-performance organic pigments and titanium dioxide to produce a full color palette.

This range is an excellent alternative to lead-based formulations due to its low metamerism. The Solaplex range reflectance curve follows closely that of lead chromate. Color data is exhibited in Table 1.

Product Performance

In addition to the unique color space, the inorganic chemistry of Solaplex pigments gives exceptional performance, excellent opacity and hiding power. Chemical resistance, excellent weather fastness and light fastness are also key benefits for high performance and exterior coatings.

Acid Resistance

Color formulators need to select pigments that are chemically inert for demanding applications. This is a major issue for coil coating applications, which require pigments that are resistant to acid rain and sulfur dioxide. In a Kesternich sulfur dioxide exposure test, the Solaplex range was compared to a series of weather-fast, conventional inorganic pigments. Solaplex pigments were found to have equivalent resistance to nickel and chrome titanate and superior resistance to bismuth vanadate, as reflected in exposure panels in Figure 3.

Exterior Weathering

Exterior coatings for the agricultural, construction, engineering, marine and automotive markets require excellent fastness to light, weather and gloss, in full shades (masstone) and reduced shades (tint). Panels with Solaplex pigments were exposed to two years outdoors in Florida in full shade and reduced shade and accelerated weathering (Figures 4 and 5). Results indicate that the Solaplex range is equivalent to titanates after two years exterior Florida weathering in full and reduced shade. Solaplex pigments also exhibited superior gloss retention.

Performance

High performance is of paramount importance to color formulators in the coatings industry. Pigments sometimes must endure harsh environments during processing and in use and, thus, need to be robust to resist change.

The soft, spherical pigment particles of the Solaplex range are less abrasive and are easy to disperse. The low oil absorption allows for high pigment loading without adverse effects on rheology and gloss. Formulations using Solaplex pigments have been found to reduce orange peel effect, particularly in powder coatings.

Controlled particle size distribution of the Solaplex range results in pigments with clean undertone and excellent hiding power. High hiding power and opacity make them suitable for use with transparent high-performance organic pigments. Physical and chemical properties of the pigments are detailed in Table 2.

Applications

The overall durability and temperature stability make Solaplex pigments useful for a wide range of application in coatings and plastics. The chemical resistance of Solaplex pigments makes them suitable for use in acid-catalyzed and acidic environments.

Applications such as exterior and masonry paints, architectural and coil coating are particularly important; here Solaplex pigments provide a unique range of coloring options in the yellow and orange color area with excellent durability.

In the automotive coatings market, the novel color area, opacity and superior weathering are seen as a real benefit compared to organic pigments.

In addition, the combination of Solaplex™ pigments with high performance organic pigments give the most cost-effective alternative to lead chromate-based colors in applications such as powder coatings.

New Options

Solaplex technology is a new chemistry that provides unique color options to the formulator. It offers an environmentally acceptable alternative to pigments containing lead, chromium and molybdenum. In addition, Solaplex pigments are heat stable, light fast and resistant to acid, alkalis and weathering.

Their wide compatibility in full shade and reduced shade make Solaplex pigments a perfect partner with which to formulate cost-effective colors, either as single pigments, or in combination with inorganic or high-performance organic pigments. The ease of dispersion, bright, clean shades and excellent hiding power place these novel pigments in a class of their own in the coatings market.

For more information, visit www.rpigments.com. For a Solaplex brochure, technical data sheet and/or product sample, contact Larry Lane at 800/638.4444, ext. 423, or email info.us@rpigments.com.

Share This Story

Looking for a reprint of this article?
From high-res PDFs to custom plaques, order your copy today!

Recommended Content

JOIN TODAY
to unlock your recommendations.

Already have an account? Sign In

  • pci1022-Kinaltek-Lead-1170.jpg

    A Novel Pigment Production Technology

    Following an extensive R&D program that demonstrated...
    Paint and Coating Pigments
    By: Jawad Haidar and Nitin Soni
  • pci global top 10

    2025 Global Top 10: Top Paint and Coatings Companies

    The following is PCI’s annual ranking of the top 10...
    Paint and Coating Market Reports
    By: Courtney Bassett
  • 2025 pci 25

    2025 PCI 25: Top Paint and Coatings Companies

    PCI's annual ranking of the top 25 North American paint...
    Paint and Coating Market Reports
    By: Courtney Bassett
You must login or register in order to post a comment.

Report Abusive Comment

Manage My Account
  • eMagazine
  • Newsletters
  • Online Registration
  • Subscription Customer Service

More Videos

Sponsored Content

Sponsored Content is a special paid section where industry companies provide high quality, objective, non-commercial content around topics of interest to the PCI audience. All Sponsored Content is supplied by the advertising company and any opinions expressed in this article are those of the author and not necessarily reflect the views of PCI or its parent company, BNP Media. Interested in participating in our Sponsored Content section? Contact your local rep!

close
  • wooden kitchen set and shelving
    Sponsored bySirca North America

    Leveraging Coatings to Meet ESG Goals in Manufacturing

  • man woodworking in workshop
    Sponsored byGemini Industries, Inc.

    Waterborne Coatings Aren't the Future -- They're the New Performance Benchmark

Popular Stories

Akzo, SW, Nippon Logos

AkzoNobel Rejects Cash Offer From Nippon Paint, Sherwin-Williams

BASF SE Logo

BASF Announces Strategic Business Sale

AkzoSWNipponEndTalks

Nippon Paint, Sherwin-Williams End AkzoNobel Pursuit

POB-Point-and-Shoot

PCI Buyers Guide

Submit a Request for Proposal (RFP) to suppliers of your choice with details on what you need with a click of a button

Start your RFP

Browse our Buyers Guide for manufacturers and distributors of all types of coatings products and much more!

Find Suppliers

Events

September 4, 2025

N-Butylpyrrolidone (NBP) as a Green Solvent to Replace N-Methylpyrrolidone (NMP) in Industrial Coating Applications

ON DEMAND: EPA published a regulation proposal around N-methylpyrrolidone (NMP) in June 2024 to ban or limit NMP in many applications, such as paints and coatings and their removers. N-butylpyrrolidone (NBP) is a powerful and versatile solvent for a variety of industries looking for alternatives to substance of very high concern (SVHC)-listed solvents.

September 15, 2026

Coatings Trends & Technologies Summit

The Coatings Trends & Technologies (CTT) Summit is an annual conference for both liquid and powder coatings formulators and manufacturers to discuss innovations in coatings technology. This event combines high-quality technical presentations, a resource-rich exhibit hall, and dedicated networking opportunities to connect scientific minds, foster innovation, and cultivate game-changing new ideas!

View All Submit An Event

Poll

Longest-running laboratory experiment

What is the longest-running laboratory experiment?
View Results Poll Archive

Products

Automotive Paints and Coatings, 2nd Edition

Now in its second edition and still the only book of its kind, this is an authoritative treatment of all stages of the coating process.

See More Products
Inside the AI Shift in Coatings - See the article now

Related Articles

  • PPG Receives DOE Award to Develop New Class of Pigments for Cool Coatings

    See More
  • Sirrus and BASF to Develop New Class of Automotive Coatings

    See More
  • RadLaunch Announces Start-up Technology Accelerator Class of 2020

    See More

Related Products

See More Products
  • corrosion of linings.jpg

    Corrosion of Linings & Coatings: Cathodic and Inhibitor Protection and Corrosion Monitoring

  • durability.jpg

    Increasing the Durability of Paint and Varnish Coatings in Building Products and Construction 1st Edition

See More Products

Related Directories

  • Shepherd Color Co.

    The Shepherd Color Company produces a wide range of high-performance complex inorganic color pigments (CICPs) used in a variety of industries. These pigments are an extraordinary class of inorganic pigments that offer stable, long-lasting color for many applications. They have unbeatable weatherability, heat and chemical resistance, are non-warping and easy to disperse.
×

Keep the info flowing with our eNewsletters!

Get the latest industry updates tailored your way.

JOIN TODAY!
  • RESOURCES
    • Advertise
    • Contact Us
    • Directories
    • Store
    • Want More
    • Manufacturing Division
  • SIGN UP TODAY
    • Create Account
    • eMagazine
    • Newsletters
    • Customer Service
    • Manage Preferences
  • SERVICES
    • Marketing Services
    • Reprints
    • Market Research
    • List Rental
    • Survey & Sample
  • STAY CONNECTED
    • LinkedIn
    • Facebook
    • Youtube
    • X (Twitter)
  • PRIVACY
    • PRIVACY POLICY
    • TERMS & CONDITIONS
    • DO NOT SELL MY PERSONAL INFORMATION
    • PRIVACY REQUEST
    • ACCESSIBILITY

Copyright ©2026. All Rights Reserved BNP Media, Inc. and BNP Media II, LLC.

Design, CMS, Hosting & Web Development :: ePublishing