LEHIGH VALLEY, Pa. - On March 31, Air Products, Lehigh Valley, Pa., completed the acquisition of Tomah3 Products of Milton, Wis., for approximately $115 million in cash. The acquisition, initially announced on March 22, increases the size of Air Products' Performance Materials business and will capitalize on the company's surface-science expertise and high-growth-market opportunities. Tomah3 produces specialty surfactants and processing aids.

Tomah employs approximately 90 people and has production facilities located in Milton, Wis., and Reserve, La. The Milton plant produces amine-based surfactants, while the Reserve facility produces alcohol ethoxylate surfactants.

LEHIGH VALLEY, Pa. - Air Products has also announced that it has consolidated its efforts to commercialize its nanotechnology offerings and strengthen its strategy around the sale of nanoparticle dispersions through a technology acquisition from its Nanogate Advanced Materials GmbH (NAM) joint venture. Air Products purchased NAM's nanoparticle dispersion production and related dispersion technologies and assets located in Saarbrücken, Germany. Air Products' initial nanoparticle dispersion offerings include zinc oxide, silver, and indium and antimony tin oxides in a variety of organic, aqueous and 100-percent-solids systems.

The process of making nanoparticle dispersions compatible with the systems they are being incorporated into is a critical requirement to gain the maximum benefit from the use of nanoparticles in many applications, including several markets for formulated systems such as coatings, adhesives, inks and composites, that Air Products currently serves.

You must register or login in order to post comments.

Multimedia

Videos

Image Galleries

Podcasts

PCI Top 5 - January 12, 2012
PCI's Podcast series on the five most e-mailed/shared articles and stories for the week.

More Podcasts

THE MAGAZINE

PCI Magazine

February 2012 cover

2012 February

PCI's new issue is now available. Check it out!

TABLE OF CONTENTS SUBSCRIBE

Coating Technology

What resources do you refer to when learning about coatings technology?
See Poll Results Poll Archive

THE PCI STORE

Power Coatings
CD Verison: Powder Coatings - Foundation for the Novice Formulator by Kevin Biller for $29.95 plus shipping
ON CD - Powder Coatings have been the fastest growing finishing technology for the past 30 years. In spite of this tremendous growth and the technology advances that come with it, very few technical tools have been provided for the formulator.
More Products

Clear Seas Research

Clear Seas ResearchWith access to over one million professionals and more than 60 industry-specific publications,Clear Seas Research offers relevant insights from those who know your industry best. Let us customize a market research solution that exceeds your marketing goals.

Virtual Brochures

PageCollageClick to the Virtual Brochures page to view multiple catagories that list downloadable product literature from leading industry suppliers.

STAY CONNECTED

Facebook Twitter  LinkedIn