Air Products Debuts Thermal Spray Cooling Technology - Posted 11/14/07

Air Products has introduced a new thermal spray cooling technology to the North American market that uses cryogenic nitrogen vapor (-320°F) to maintain part temperature during thermal spray coating applications. The company’s U.S. patent-pending technology makes high-quality thermal spray coatings possible by maintaining part temperature within a pre-defined narrow range, even for heat-intensive spraying processes. The technology can enable the user to apply coatings faster and at a lower cost than traditional cooling methods.

Air Products has introduced a new thermal spray cooling technology to the North American market that uses cryogenic nitrogen vapor (-320°F) to maintain part temperature during thermal spray coating applications. The company’s U.S. patent-pending technology makes high-quality thermal spray coatings possible by maintaining part temperature within a pre-defined narrow range, even for heat-intensive spraying processes. The technology can enable the user to apply coatings faster and at a lower cost than traditional cooling methods.

Exposing a part to too much heat can negatively impact coating adhesion, substrate and coating hardness, fatigue life, corrosion resistance and dimensional tolerances. One method used by thermal spray applicators to keep part temperatures within a closely set range is forced air cooling combined with inter-pass breaks. This traditional practice, however, increases downtime and reduces productivity as well as wastes powder and process gases.

“Air Products recognized that thermal spray applicators needed a better solution to maintaining part temperature,” said Dr. Rana Ghosh, project manager, cryogenic cooling applications at Air Products. “In response, we developed a thermal spray cooling technology that can maintain a part’s temperature within a much tighter range during the spray operation versus traditional cooling methods by varying the cooling intensity to match the heat generated in the spraying process. Use of our technology can improve part quality, lower costs by reducing powder and process gas waste and enabling the use of inexpensive flexible masking, and allow better utilization of the thermal spray equipment and booth.”

Air Products’ thermal spray cooling nozzles can be mounted directly on the robotic arm next to the thermal spraying gun. During spray application, the cryogenic vapor jet follows the thermal spray plume to maintain the part’s temperature within the specified range. Multiple cooling lines can provide additional part cooling, if needed. The part is continuously monitored by a thermal imaging camera and/or infrared sensors that provide temperature feedback to the computer-controlled cooling nozzles, which allows the cooling system to automatically maintain the substrate temperature set by the spray booth operator. The part temperature history also can be recorded and archived for future audit purposes.

Compatible with existing thermal spray systems, Air Products’ technology offers a variety of system designs for application-specific use. The technology can be used in the aerospace, automotive, and heavy industries; oil fields; and job shops. Currently used by a major aircraft parts service facility, Air Products’ technology has cut in half the spraying time and the amount of powder and process gases consumed in the coating of aircraft landing gear axles.

For more information, visit www.airproducts.com.
You must register or login in order to post comments.

Multimedia

Videos

Image Galleries

American Coating Show 2012

The American Coatings Show and Conference, held every two years, took place May 7-10 at the Indiana Convention Center in Indianapolis, IN, in the heart of the Manufacturing Belt, the oldest and largest concentration of industrial companies in the Midwest.

Podcasts

PCI Top 5 - January 12, 2012
PCI's Podcast series on the five most e-mailed/shared articles and stories for the week.

More Podcasts

THE MAGAZINE

PCI Magazine

PCI may 2012 cover

2012 May

Check out PCI's May issue!!

TABLE OF CONTENTS SUBSCRIBE

2012 Sales Growth

What is your projected sales growth for 2012?
See Poll Results Poll Archive

THE PCI STORE

PCI-June-2011-Coversmall.gif
PCI Additives Handbook

Encyclopedia of information on the properties and uses of coatings additives.

More Products

Clear Seas Research

Clear Seas ResearchWith access to over one million professionals and more than 60 industry-specific publications,Clear Seas Research offers relevant insights from those who know your industry best. Let us customize a market research solution that exceeds your marketing goals.

Virtual Brochures

PageCollageClick on the Virtual Brochures page to view multiple categories that list downloadable product literature from leading industry suppliers.

STAY CONNECTED

Facebook Twitter  LinkedIn YouTube