Aircraft Prize Refinished with ANAC Coatings - Posted 12/12/07

A 1977 Cessna Cardinal 177B aircraft, being given away by the world's largest pilots association, U.S.-based Aircraft Owners and Pilots Association (AOPA), in its annual sweepstakes, has been refurbished with coatings donated by ANAC (Akzo Nobel Aerospace Coatings) through its distributor network.

The sweepstakes, which features a different restored aircraft each year, is the mainspring of the annual membership drive with every member entered. The members, who own and operate primarily single and twin-engine planes for business and personal use, are able to follow the progress of the work on line and through AOPA's publications, taking notes for their own projects. AOPA has a membership of 414,000, two thirds of all pilots in the U.S.

The paint design, applied by Advanced Aircraft Refinishers of Georgia, was created by Scheme Designers, owned and operated by Craig Barnett of Cresskill, New Jersey, who also works with OEMs on paint schemes. His inspiration for this project was the Cessna Cardinal logo, originally displayed on the tail in a smaller form.

After the complete disassembly of the airframe into more than 280 parts, each piece of the airplane was put through a thorough the paint refurbishing process to ensure that the best possible protective finish was achieved.

Following the removal of the existing paint layers, the surfaces were chemically cleaned and a conversion coating applied. A zinc chromate epoxy primer was followed by ANAC's Alumigrip Matterhorn White topcoat, producing a superb, high-gloss finish.The white was then masked for the application of the red, gold and black trim, all in ANAC paints. The paints were donated by ANAC distributor Aero Performance.

The fully restored airplane has been on display at aviation events around the U.S.

For more information visit www.aopa.org or www.anac.com.
You must register or login in order to post comments.

Multimedia

Videos

Image Galleries

American Coating Show 2012

The American Coatings Show and Conference, held every two years, took place May 7-10 at the Indiana Convention Center in Indianapolis, IN, in the heart of the Manufacturing Belt, the oldest and largest concentration of industrial companies in the Midwest.

Podcasts

PCI Top 5 - January 12, 2012
PCI's Podcast series on the five most e-mailed/shared articles and stories for the week.

More Podcasts

THE MAGAZINE

PCI Magazine

PCI may 2012 cover

2012 May

Check out PCI's May issue!!

TABLE OF CONTENTS SUBSCRIBE

2012 Sales Growth

What is your projected sales growth for 2012?
See Poll Results Poll Archive

THE PCI STORE

PCI-June-2011-Coversmall.gif
PCI Additives Handbook

Encyclopedia of information on the properties and uses of coatings additives.

More Products

Clear Seas Research

Clear Seas ResearchWith access to over one million professionals and more than 60 industry-specific publications,Clear Seas Research offers relevant insights from those who know your industry best. Let us customize a market research solution that exceeds your marketing goals.

Virtual Brochures

PageCollageClick on the Virtual Brochures page to view multiple categories that list downloadable product literature from leading industry suppliers.

STAY CONNECTED

Facebook Twitter  LinkedIn YouTube