Painting & Coating Industry (PCI) logo Powder coating summit logo
search
cart
facebook twitter linkedin youtube
  • Sign In
  • Create Account
  • Sign Out
  • My Account
Painting & Coating Industry (PCI) logo Powder coating summit logo
  • NEWS
    • Latest News
    • Market Trends & Reports
    • Finishing News
    • Price Alerts
    • Subscribe to Newsletters
    • Global Top 10/ PCI 25
    • Weekly Featured Article
    • COATLE Word Game
  • PRODUCTS
    • Product News
    • Featured Products
    • Must See Products and Services
  • MATERIALS
    • Additives
    • Resins/Polymers
    • Pigments
    • Equipment
    • Distributors
  • TECHNOLOGIES
    • Adhesives
    • Architectural Coatings
    • Finishing Articles
    • Finishing Technologies
    • Finishing Equipment
    • Industrial Coatings
    • Nanotechnology
    • Powder Coatings
    • Solventborne
    • Special Purpose Coatings
    • Sustainability
    • UV Coatings
    • Waterborne
  • RESOURCES
    • Columns
      • Did you know?
      • Distribution Dive
      • Formulating With Mike
      • Innovation Insights
      • Powder Coating Perspectives
      • TiO2 Insider
    • Blogs
      • Editor's Viewpoint
      • Industry Insights
    • Coatings Supplier Handbook
    • Podcasts and Videos
      • COAT-IT! Podcast
      • Videos/PCI TV
    • PCI Store
    • Classifieds
    • eBooks
    • Sponsor Insights
    • White Papers
    • COATLE Word Game
  • EVENTS
    • Coatings Trends & Technologies Summit
    • Paint and Coatings Academy
    • Webinars
    • Calendar of Events
    • Lifetime Achievement Award
  • DIRECTORIES
    • Buyer's Guide
    • Equipment Directory
    • Materials Directory
  • EMAGAZINE
    • Current Issue
    • eMagazine Archive
    • China Issue Archive
    • Editorial Advisory Board
  • CONTACT
    • Contact Us
    • Advertise
    • Subscribe to eMagazine
    • Subscribe to Newsletters
  • SIGN UP!
Breaking News

ASTM Proposes Two New Testing Standards

July 31, 2011

W. CONSHOHOCKEN, PA - ASTM International has announced two new proposed standards, a standard that addresses test panel preparation and rating specifically for corrosion testing of building projects, and a standard that will provide insight into the relationship between temperature and viscosity.

ASTM WK 30920, Guide for Corrosion Test Panel Preparation and Rating of Coil-Coated Building Products, is being developed by Subcommittee D01.53 on Coil Coated Metal, part of ASTM International Committee D01 on Paint and Related Coatings, Materials and Applications.

According to Ted Best, Scientist, Valspar Corp., and D01.53 member, the standardization of test panel configurations and ratings would allow benchmark comparisons across a broad range of products that includes substrates, pretreatments and coatings. Producers will be able to use the proposed standard, once it has been approved, to develop new products, while users will employ it to verify and compare product performance.

“These comparisons lead to better understanding of product performance as a function of environment, better service life predictions and shorter product development cycles,” said Best.

All interested parties are welcome to join in the development of ASTM WK 30920. “Coil coaters and metal building manufacturers are especially welcome for the valuable input they can provide based on their experience and understanding of market requirements,” said Best.

The viscosity of paints, inks and many related liquid materials varies considerably with temperature. In some cases viscosity can decrease by 10 percent with every 1 °C increase in temperature. A proposed new ASTM standard will provide insight into the relationship between temperature and viscosity.

ASTM WK 33642, Test Method for Measurement of Viscosity of Paints, Inks or Related Liquid Materials as a Function of Temperature, is being developed by Subcommittee D01.24 on Physical Properties of Liquid Paints and Paint Materials, part of ASTM International Committee D01 on Paint and Related Coatings, Materials and Applications.

“It is useful to know the extent of variation, but we do not know of any ASTM standard that establishes the viscosity-temperature variation for these materials,” said Clifford Schoff, Ph.D., Schoff Associates, and Chairman of D01.24. “The relationship has important implications for viscosity measurement in general and specifically for processes such as hot spray and for sagging and leveling on baking.”

The proposed standard will give instruction on how to prepare a viscosity-temperature table or curve. This will be useful when ambient conditions do not allow the measurement at the exact temperature stated in a specification or regulation.

“In addition, knowledge of the viscosity dependence on temperature for a given material will indicate the degree of temperature control required in order to do accurate and precise viscosity measurements,” said Schoff. “Another practical application would be to compare viscosity-temperature behavior of different formulations to better understand the effect of additives or components.”

Schoff says D01.24 welcomes interested parties to join in the ongoing revision of the ASTM WK 33642 draft and also to participate in interlaboratory testing to establish the precision of the proposed standard. In addition to ASTM WK 33642, the subcommittee is also beginning work on a standard for measuring the yield stress of paints, ink and related liquids. Participants are sought for this activity as well.

ASTM International welcomes and encourages participation in the development of its standards. For more information on becoming an ASTM member, visit www.astm.org/JOIN.

Share This Story

Looking for a reprint of this article?
From high-res PDFs to custom plaques, order your copy today!

Recommended Content

JOIN TODAY
to unlock your recommendations.

Already have an account? Sign In

  • pci1022-Kinaltek-Lead-1170.jpg

    A Novel Pigment Production Technology

    Following an extensive R&D program that demonstrated...
    Paint and Coating Pigments
    By: Jawad Haidar and Nitin Soni
  • pci global top 10

    2025 Global Top 10: Top Paint and Coatings Companies

    The following is PCI’s annual ranking of the top 10...
    Paint and Coating Market Reports
    By: Courtney Bassett
  • 2025 pci 25

    2025 PCI 25: Top Paint and Coatings Companies

    PCI's annual ranking of the top 25 North American paint...
    Paint and Coating Market Reports
    By: Courtney Bassett
You must login or register in order to post a comment.

Report Abusive Comment

Manage My Account
  • eMagazine
  • Newsletters
  • Online Registration
  • Subscription Customer Service

More Videos

Sponsored Content

Sponsored Content is a special paid section where industry companies provide high quality, objective, non-commercial content around topics of interest to the PCI audience. All Sponsored Content is supplied by the advertising company and any opinions expressed in this article are those of the author and not necessarily reflect the views of PCI or its parent company, BNP Media. Interested in participating in our Sponsored Content section? Contact your local rep!

close
  • wooden kitchen set and shelving
    Sponsored bySirca North America

    Leveraging Coatings to Meet ESG Goals in Manufacturing

  • man woodworking in workshop
    Sponsored byGemini Industries, Inc.

    Waterborne Coatings Aren't the Future -- They're the New Performance Benchmark

Popular Stories

Akzo, SW, Nippon Logos

AkzoNobel Rejects Cash Offer From Nippon Paint, Sherwin-Williams

BASF SE Logo

BASF Announces Strategic Business Sale

AkzoSWNipponEndTalks

Nippon Paint, Sherwin-Williams End AkzoNobel Pursuit

POB-Point-and-Shoot

PCI Buyers Guide

Submit a Request for Proposal (RFP) to suppliers of your choice with details on what you need with a click of a button

Start your RFP

Browse our Buyers Guide for manufacturers and distributors of all types of coatings products and much more!

Find Suppliers

Events

September 4, 2025

N-Butylpyrrolidone (NBP) as a Green Solvent to Replace N-Methylpyrrolidone (NMP) in Industrial Coating Applications

ON DEMAND: EPA published a regulation proposal around N-methylpyrrolidone (NMP) in June 2024 to ban or limit NMP in many applications, such as paints and coatings and their removers. N-butylpyrrolidone (NBP) is a powerful and versatile solvent for a variety of industries looking for alternatives to substance of very high concern (SVHC)-listed solvents.

September 15, 2026

Coatings Trends & Technologies Summit

The Coatings Trends & Technologies (CTT) Summit is an annual conference for both liquid and powder coatings formulators and manufacturers to discuss innovations in coatings technology. This event combines high-quality technical presentations, a resource-rich exhibit hall, and dedicated networking opportunities to connect scientific minds, foster innovation, and cultivate game-changing new ideas!

View All Submit An Event

Poll

Longest-running laboratory experiment

What is the longest-running laboratory experiment?
View Results Poll Archive

Products

Automotive Paints and Coatings, 2nd Edition

Now in its second edition and still the only book of its kind, this is an authoritative treatment of all stages of the coating process.

See More Products
Inside the AI Shift in Coatings - See the article now

Related Articles

  • ASTM Proposes Several New Testing Standards

    See More
  • ASTM Proposes New Standard for Non-Destructive Lead Paint Testing

    See More
  • ASTM Introduces Two New Standards

    See More

Related Products

See More Products
  • pci may 2020

    PCI May 2020 Issue

See More Products
×

Keep the info flowing with our eNewsletters!

Get the latest industry updates tailored your way.

JOIN TODAY!
  • RESOURCES
    • Advertise
    • Contact Us
    • Directories
    • Store
    • Want More
    • Manufacturing Division
  • SIGN UP TODAY
    • Create Account
    • eMagazine
    • Newsletters
    • Customer Service
    • Manage Preferences
  • SERVICES
    • Marketing Services
    • Reprints
    • Market Research
    • List Rental
    • Survey & Sample
  • STAY CONNECTED
    • LinkedIn
    • Facebook
    • Youtube
    • X (Twitter)
  • PRIVACY
    • PRIVACY POLICY
    • TERMS & CONDITIONS
    • DO NOT SELL MY PERSONAL INFORMATION
    • PRIVACY REQUEST
    • ACCESSIBILITY

Copyright ©2026. All Rights Reserved BNP Media, Inc. and BNP Media II, LLC.

Design, CMS, Hosting & Web Development :: ePublishing