When the Windgap Bridge in Western Pennsylvania was last painted in 1986, the Allegheny County Department of Public Works Bridge Division hoped their choice of an experimental paint system would deliver long-term performance. But they had no idea the new aliphatic polyester polyurethane coating system they selected would far exceed their greatest expectations. After more than two decades of use, the coating on the busy Windgap Bridge still looks great.
The coating system, manufactured by Tnemec, utilized polyurethane resin technology developed by Bayer MaterialScience. Not only was it easy to apply, the new coating system exhibited a number of advantages that would eventually prove the coating system to be extremely cost-effective.
Because polyurethane resin was a key component in the coating system, it promised to outlast alkyds and vinyl systems. Fast drying, highly corrosion resistant, and able to withstand temperature drops during the curing process, this polyurethane system was also highly resistant to abrasion, wet conditions, corrosive fumes, chemical contact and graffiti.
Although the Department of Public Works originally specified a phenolic zinc-rich primer for the bridge, they agreed with Tnemec’s recommendation of a moisture-cured polyurethane zinc-rich primer instead. An intermediate coat of Tnemec Series 27HB Typoxy catalyzed epoxy was applied next, followed by a topcoat of Tnemec Series 70 Endura-Shield, a two-component aliphatic polyester polyurethane.
For more than 21 years, the Windgap Bridge has stood up to rugged use. Located just west of downtown Pittsburgh, the bridge has been subjected to plenty of traffic, tough weather conditions, and emissions from various sources. Yet inspection report after inspection report proves the bridge coating remains in excellent condition.
According to Carl Angeloff, P.E., Head - NAFTA Business Development and Manager - BD Corrosion, Bayer MaterialScience, the coating system was inspected immediately after the initial application, then annually for the first five years of use. KTA-Tator, an independent inspection firm, examined twelve different locations across the underside of the bridge each time, and checked for coating thickness, adhesion, and gloss. Minimal changes were noted throughout the five-year exposure period.
In April 2007, 21 years after the initial application, KTA-Tator conducted another inspection and confirmed that the coating system was still in excellent condition. The company’s report states, “The overall rate of rusting and the coating breakdown (0.03% or less of the painted surface area) is considered to be low, especially for a structure that is subject to the Pennsylvania winter freeze/thaw cycling and the frequent application of corrosive de-icing salts.” KTA-Tator’s report further notes that although leakage in the expansion joints of the concrete on the bridge deck caused minor corrosion to the adjoining painted steel, these were the only areas of corrosion on the bridge.
Jim Machen, consultant for KTA-Tator, notes that the coating system never needed to be touched up during its service life. In fact, he sees very little maintenance down the road. “If minor touch ups are made within the next five years, I think it’s likely that the coating system will remain intact for another 15 years,” predicts Machen. “After that, the bridge may only need an overcoat.”
Two other bridges in Western Pennsylvania – the Sutersville Bridge and the Hillcrest Bridge – were constructed shortly after the Windgap Bridge, and were also painted with the high-performance paint system. Field evaluations over the years have shown the coatings on these surfaces were also holding up well. For the Allegheny County Department of Public Works, this reliable coating system bridges the gap between long-term performance and cost-effectiveness.
For more information, visit www.bayermaterialsciencenafta.com, www.tnemec.com, or www.kta.com.
The coating system, manufactured by Tnemec, utilized polyurethane resin technology developed by Bayer MaterialScience. Not only was it easy to apply, the new coating system exhibited a number of advantages that would eventually prove the coating system to be extremely cost-effective.
Because polyurethane resin was a key component in the coating system, it promised to outlast alkyds and vinyl systems. Fast drying, highly corrosion resistant, and able to withstand temperature drops during the curing process, this polyurethane system was also highly resistant to abrasion, wet conditions, corrosive fumes, chemical contact and graffiti.
Although the Department of Public Works originally specified a phenolic zinc-rich primer for the bridge, they agreed with Tnemec’s recommendation of a moisture-cured polyurethane zinc-rich primer instead. An intermediate coat of Tnemec Series 27HB Typoxy catalyzed epoxy was applied next, followed by a topcoat of Tnemec Series 70 Endura-Shield, a two-component aliphatic polyester polyurethane.
For more than 21 years, the Windgap Bridge has stood up to rugged use. Located just west of downtown Pittsburgh, the bridge has been subjected to plenty of traffic, tough weather conditions, and emissions from various sources. Yet inspection report after inspection report proves the bridge coating remains in excellent condition.
According to Carl Angeloff, P.E., Head - NAFTA Business Development and Manager - BD Corrosion, Bayer MaterialScience, the coating system was inspected immediately after the initial application, then annually for the first five years of use. KTA-Tator, an independent inspection firm, examined twelve different locations across the underside of the bridge each time, and checked for coating thickness, adhesion, and gloss. Minimal changes were noted throughout the five-year exposure period.
In April 2007, 21 years after the initial application, KTA-Tator conducted another inspection and confirmed that the coating system was still in excellent condition. The company’s report states, “The overall rate of rusting and the coating breakdown (0.03% or less of the painted surface area) is considered to be low, especially for a structure that is subject to the Pennsylvania winter freeze/thaw cycling and the frequent application of corrosive de-icing salts.” KTA-Tator’s report further notes that although leakage in the expansion joints of the concrete on the bridge deck caused minor corrosion to the adjoining painted steel, these were the only areas of corrosion on the bridge.
Jim Machen, consultant for KTA-Tator, notes that the coating system never needed to be touched up during its service life. In fact, he sees very little maintenance down the road. “If minor touch ups are made within the next five years, I think it’s likely that the coating system will remain intact for another 15 years,” predicts Machen. “After that, the bridge may only need an overcoat.”
Two other bridges in Western Pennsylvania – the Sutersville Bridge and the Hillcrest Bridge – were constructed shortly after the Windgap Bridge, and were also painted with the high-performance paint system. Field evaluations over the years have shown the coatings on these surfaces were also holding up well. For the Allegheny County Department of Public Works, this reliable coating system bridges the gap between long-term performance and cost-effectiveness.