The newest version of this company’s viscometer is available for ink, polymer, resin and other high-temperature lines.
The newest version of this company’s viscometer is available for ink, polymer, resin and other high-temperature lines. The new ceramic technology allows viscosity measurements up to 370ºC with rapid changeovers. Cambridge Applied Systems, contact Art MacNeill, 981-393-6500.