Company News / Breaking News

Continental Airlines Uses Non-Toxic Surface Pretreatment

Pantheon Chemical’s non-toxic surface pretreatment, PreKote, has been selected by Continental Airlines for use in its aircraft-repainting program.

PHOENIX - Pantheon Chemical’s non-toxic surface pretreatment, PreKote, has been selected by Continental Airlines for use in its aircraft-repainting program. The airline’s decision to use hexavalent chromium-free PreKote marks a shift in the aerospace industry to eliminate toxins used in the pretreatment of aircraft.

            Continental Airlines was the first commercial airline to test the technology following the United States Air Force’s success with PreKote. A 22-month performance analysis validated the in-service performance of PreKote, showing excellent adhesion and paint-quality results. In addition, the PreKote process used on Continental aircraft at Leading Edge Aviation Services cut process time, eliminated hazardous chemicals, improved worker health and safety conditions, and reduced wastewater.

            For more information, visit www.pantheonchemical.com.

You must register or login in order to post comments.

Multimedia

Videos

Image Galleries

Podcasts

PCI Top 5 - January 12, 2012
PCI's Podcast series on the five most e-mailed/shared articles and stories for the week.

More Podcasts

THE MAGAZINE

PCI Magazine

February 2012 cover

2012 February

PCI's new issue is now available. Check it out!

TABLE OF CONTENTS SUBSCRIBE

Coating Technology

What resources do you refer to when learning about coatings technology?
See Poll Results Poll Archive

THE PCI STORE

Power Coatings
CD Verison: Powder Coatings - Foundation for the Novice Formulator by Kevin Biller for $29.95 plus shipping
ON CD - Powder Coatings have been the fastest growing finishing technology for the past 30 years. In spite of this tremendous growth and the technology advances that come with it, very few technical tools have been provided for the formulator.
More Products

Clear Seas Research

Clear Seas ResearchWith access to over one million professionals and more than 60 industry-specific publications,Clear Seas Research offers relevant insights from those who know your industry best. Let us customize a market research solution that exceeds your marketing goals.

Virtual Brochures

PageCollageClick to the Virtual Brochures page to view multiple catagories that list downloadable product literature from leading industry suppliers.

STAY CONNECTED

Facebook Twitter  LinkedIn