Painting & Coating Industry (PCI) logo Powder coating summit logo
search
cart
facebook twitter linkedin youtube
  • Sign In
  • Create Account
  • Sign Out
  • My Account
Painting & Coating Industry (PCI) logo Powder coating summit logo
  • NEWS
    • Latest News
    • Market Trends & Reports
    • Finishing News
    • Price Alerts
    • Subscribe to Newsletters
    • Global Top 10/ PCI 25
    • Weekly Featured Article
    • COATLE Word Game
  • PRODUCTS
    • Product News
    • Featured Products
    • Must See Products and Services
  • MATERIALS
    • Additives
    • Resins/Polymers
    • Pigments
    • Equipment
    • Distributors
  • TECHNOLOGIES
    • Adhesives
    • Architectural Coatings
    • Finishing Articles
    • Finishing Technologies
    • Finishing Equipment
    • Industrial Coatings
    • Nanotechnology
    • Powder Coatings
    • Solventborne
    • Special Purpose Coatings
    • Sustainability
    • UV Coatings
    • Waterborne
  • RESOURCES
    • Columns
      • Did you know?
      • Distribution Dive
      • Formulating With Mike
      • Innovation Insights
      • Powder Coating Perspectives
      • TiO2 Insider
    • Blogs
      • Editor's Viewpoint
      • Industry Insights
    • Coatings Supplier Handbook
    • Podcasts and Videos
      • COAT-IT! Podcast
      • Videos/PCI TV
    • PCI Store
    • Classifieds
    • eBooks
    • Sponsor Insights
    • White Papers
    • COATLE Word Game
  • EVENTS
    • Coatings Trends & Technologies Summit
    • Paint and Coatings Academy
    • Webinars
    • Calendar of Events
    • Lifetime Achievement Award
  • DIRECTORIES
    • Buyer's Guide
    • Equipment Directory
    • Materials Directory
  • EMAGAZINE
    • Current Issue
    • eMagazine Archive
    • China Issue Archive
    • Editorial Advisory Board
  • CONTACT
    • Contact Us
    • Advertise
    • Subscribe to eMagazine
    • Subscribe to Newsletters
  • SIGN UP!
Breaking News

CSB Issues Report on Explosion/Recommends New Safety Standards

August 1, 2010

WASHINGTON D.C. – A U.S. Chemical Safety Board (CSB) case study released on the 2009 explosion and fire at the Veolia ES Technical Solutions L.L.C. facility in West Carrollton, OH, calls on the industry to improve safety standards covering hazardous waste processing, handling and storage facilities. The board also recommended that fire-protection codes be revised to require companies to determine safe distances between occupied buildings and potentially hazardous operating areas.

The accident occurred on May 4, 2009, when flammable vapor was released from a waste recycling process, ignited and violently exploded. The blast seriously injured two workers and damaged 20 nearby residences and five businesses. CSB investigators found that the north wall of the lab and operations building, where the victims were injured, was less than 30 feet from the waste recycling processing area where the flammable vapor was released.

CSB Chairman Rafael Moure-Eraso said, “This accident should not have happened. Our report notes that OSHA cited the company for inadequate attention to process safety management practices in the handling of flammable liquids. But in case of an accident, I believe it is absolutely critical that buildings at chemical facilities be sited safe distances from process equipment to maximize the safety of workers. We are making recommendations that would help ensure that operating areas with occupied buildings such as control rooms be sufficiently separated from process areas containing flammable liquids and gases that have the potential to explode.”

The Board issued a recommendation to the National Fire Protection Association (NFPA), which develops codes and standards for industry, urging NFPA to require companies to perform engineering analyses to determine safe separation distances between buildings occupied by administrative and other personnel not essential to process operations, and buildings housing the potentially hazardous process equipment.

The Board also revised a previous recommendation to the Environmental Technology Council, a hazardous waste industry trade group, to petition the NFPA to develop a standard specific to hazardous waste treatment, storage and disposal facilities. This would include guidance on reducing the likelihood of fires, explosions and releases of hazardous waste.

Moure-Eraso noted, “The Environmental Technology Council did not respond adequately to our 2007 recommendation, which we issued following an explosion and massive fire at the Environmental Quality hazardous waste facility in Apex, NC, to work for more stringent standards in the hazardous waste industry. I strongly urge the industry to act now. These facilities, by their nature, contain wide varieties of flammable and toxic materials that can cause significant injury to workers and threaten the wellbeing of nearby communities. Facility owners and operators need stricter technical requirements to improve the safety of life and property.”

The report notes that after a normal run of the tetrahydrafuran (THF) solvent recovery process at the Veolia facility, the unit operator began a routine shutdown. Completing the process required blowing nitrogen back through the circulation piping to clean it, prior to closing valves.

CSB lead investigator Johnnie Banks said, “At the time of the shutdown, witnesses reported hearing the sound of a sudden, loud vapor release and smelling a very strong odor of THF solvent, which knocked several employees to their knees. It was a matter of just a couple of minutes until the highly flammable vapor ignited.”

The vapor drifted to the laboratory and operations building and found an ignition source inside the building. A worker in the control room reported being enveloped in a fireball that went through the building. The first explosion knocked over a bank of lockers, severely injuring an employee and pinning him underneath.

Because of the extensive fire damage, the CSB was unable to conclusively determine the exact initiating event for the vapor release, concluding that one of two possible scenarios likely occurred. In the first scenario, air may have been drawn into a tank containing THF residue and peroxides, causing increased pressure in the tank and forcing flammable vapor from the tank to escape through a manway cover or a vacuum breaker.

In the second possible scenario, CSB investigators believe a line hose, intended to send pressurized nitrogen into a different tank, may have instead been connected to a tank containing unprocessed, flammable liquid. When the nitrogen was applied, it forced flammable vapor out through the tank vent. In either scenario, the vapor drifted to the operations building and ignited, causing the injuries.

In addition to issuing recommendations to NFPA and the hazardous waste industry, the board also issued recommendations to Veolia, which is rebuilding the plant. The CSB called on the company to restrict occupancy in buildings in close proximity to the operating plant to personnel trained in the safe operation and orderly shutdown of the plant. The board also called on the Center for Chemical Process Safety, a division of the American Institute of Chemical Engineers, to revise control-room siting guidelines to address the characteristics of all Class 1B flammable liquids.

Share This Story

Looking for a reprint of this article?
From high-res PDFs to custom plaques, order your copy today!

Recommended Content

JOIN TODAY
to unlock your recommendations.

Already have an account? Sign In

  • pci1022-Kinaltek-Lead-1170.jpg

    A Novel Pigment Production Technology

    Following an extensive R&D program that demonstrated...
    Paint and Coating Pigments
    By: Jawad Haidar and Nitin Soni
  • pci global top 10

    2025 Global Top 10: Top Paint and Coatings Companies

    The following is PCI’s annual ranking of the top 10...
    Global Top 10 and PCI 25
    By: Courtney Bassett
  • 2025 pci 25

    2025 PCI 25: Top Paint and Coatings Companies

    PCI's annual ranking of the top 25 North American paint...
    Global Top 10 and PCI 25
    By: Courtney Bassett
You must login or register in order to post a comment.

Report Abusive Comment

Manage My Account
  • eMagazine
  • Newsletters
  • Online Registration
  • Subscription Customer Service

More Videos

Sponsored Content

Sponsored Content is a special paid section where industry companies provide high quality, objective, non-commercial content around topics of interest to the PCI audience. All Sponsored Content is supplied by the advertising company and any opinions expressed in this article are those of the author and not necessarily reflect the views of PCI or its parent company, BNP Media. Interested in participating in our Sponsored Content section? Contact your local rep!

close
  • wooden kitchen set and shelving
    Sponsored bySirca North America

    Leveraging Coatings to Meet ESG Goals in Manufacturing

  • man woodworking in workshop
    Sponsored byGemini Industries, Inc.

    Waterborne Coatings Aren't the Future -- They're the New Performance Benchmark

Popular Stories

Akzo, SW, Nippon Logos

AkzoNobel Rejects Cash Offer From Nippon Paint, Sherwin-Williams

BASF SE Logo

BASF Announces Strategic Business Sale

AkzoSWNipponEndTalks

Nippon Paint, Sherwin-Williams End AkzoNobel Pursuit

POB-Point-and-Shoot

PCI Buyers Guide

Submit a Request for Proposal (RFP) to suppliers of your choice with details on what you need with a click of a button

Start your RFP

Browse our Buyers Guide for manufacturers and distributors of all types of coatings products and much more!

Find Suppliers

Events

September 4, 2025

N-Butylpyrrolidone (NBP) as a Green Solvent to Replace N-Methylpyrrolidone (NMP) in Industrial Coating Applications

ON DEMAND: EPA published a regulation proposal around N-methylpyrrolidone (NMP) in June 2024 to ban or limit NMP in many applications, such as paints and coatings and their removers. N-butylpyrrolidone (NBP) is a powerful and versatile solvent for a variety of industries looking for alternatives to substance of very high concern (SVHC)-listed solvents.

September 15, 2026

Coatings Trends & Technologies Summit

The Coatings Trends & Technologies (CTT) Summit is an annual conference for both liquid and powder coatings formulators and manufacturers to discuss innovations in coatings technology. This event combines high-quality technical presentations, a resource-rich exhibit hall, and dedicated networking opportunities to connect scientific minds, foster innovation, and cultivate game-changing new ideas!

View All Submit An Event

Poll

Longest-running laboratory experiment

What is the longest-running laboratory experiment?
View Results Poll Archive

Products

Automotive Paints and Coatings, 2nd Edition

Now in its second edition and still the only book of its kind, this is an authoritative treatment of all stages of the coating process.

See More Products
Inside the AI Shift in Coatings - See the article now

Related Articles

  • CSB Issues Final Report on Barton Solvents Explosion

    See More
  • CSB Issues Final Report on Barton Solvents Explosion

    See More
  • CSB Issues Final Report on Barton Solvents Explosion

    See More

Related Products

See More Products
  • pci may 2020

    PCI May 2020 Issue

  • pci july 2019

    PCI July 2019 Issue

See More Products
×

Keep the info flowing with our eNewsletters!

Get the latest industry updates tailored your way.

JOIN TODAY!
  • RESOURCES
    • Advertise
    • Contact Us
    • Directories
    • Store
    • Want More
    • Manufacturing Division
  • SIGN UP TODAY
    • Create Account
    • eMagazine
    • Newsletters
    • Customer Service
    • Manage Preferences
  • SERVICES
    • Marketing Services
    • Reprints
    • Market Research
    • List Rental
    • Survey & Sample
  • STAY CONNECTED
    • LinkedIn
    • Facebook
    • Youtube
    • X (Twitter)
  • PRIVACY
    • PRIVACY POLICY
    • TERMS & CONDITIONS
    • DO NOT SELL MY PERSONAL INFORMATION
    • PRIVACY REQUEST
    • ACCESSIBILITY

Copyright ©2026. All Rights Reserved BNP Media, Inc. and BNP Media II, LLC.

Design, CMS, Hosting & Web Development :: ePublishing