Painting & Coating Industry (PCI) logo Powder coating summit logo
search
cart
facebook twitter linkedin youtube
  • Sign In
  • Create Account
  • Sign Out
  • My Account
Painting & Coating Industry (PCI) logo Powder coating summit logo
  • NEWS
    • Latest News
    • Market Trends & Reports
    • Finishing News
    • Price Alerts
    • Subscribe to Newsletters
    • Global Top 10/ PCI 25
    • Weekly Featured Article
    • COATLE Word Game
  • PRODUCTS
    • Product News
    • Featured Products
    • Must See Products and Services
  • MATERIALS
    • Additives
    • Resins/Polymers
    • Pigments
    • Equipment
    • Distributors
  • TECHNOLOGIES
    • Adhesives
    • Architectural Coatings
    • Finishing Articles
    • Finishing Technologies
    • Finishing Equipment
    • Industrial Coatings
    • Nanotechnology
    • Powder Coatings
    • Solventborne
    • Special Purpose Coatings
    • Sustainability
    • UV Coatings
    • Waterborne
  • RESOURCES
    • Columns
      • Did you know?
      • Distribution Dive
      • Formulating With Mike
      • Innovation Insights
      • Powder Coating Perspectives
      • TiO2 Insider
    • Blogs
      • Editor's Viewpoint
      • Industry Insights
    • Coatings Supplier Handbook
    • Podcasts and Videos
      • COAT-IT! Podcast
      • Videos/PCI TV
    • PCI Store
    • Classifieds
    • eBooks
    • Sponsor Insights
    • White Papers
    • COATLE Word Game
  • EVENTS
    • Coatings Trends & Technologies Summit
    • Paint and Coatings Academy
    • Webinars
    • Calendar of Events
    • Lifetime Achievement Award
  • DIRECTORIES
    • Buyer's Guide
    • Equipment Directory
    • Materials Directory
  • EMAGAZINE
    • Current Issue
    • eMagazine Archive
    • China Issue Archive
    • Editorial Advisory Board
  • CONTACT
    • Contact Us
    • Advertise
    • Subscribe to eMagazine
    • Subscribe to Newsletters
  • SIGN UP!
Breaking News

Dow Breakthrough Enables Better Paint with Less TiO2

March 23, 2011

TROY, MI – The Editors and Publisher of PCI Magazine had the privilege of meeting today with representatives of Dow Coating Materials (DCM) to learn about Dow’s latest tool for coatings formulators, EVOQUE™ Pre-Composite Polymer Technology. This revolutionary development for paint and coatings promises to change the way formulators think about hiding and the use of TiO2.

“Hiding is at the heart of every paint formulation, and without TiO2, we would not have paint as we know it today,” said Joan Schuller, General Manager, North America, Dow Coating Materials. “But TiO2 has been stretched to its limits, both in terms of hiding efficiency and supply.” EVOQUE Pre-Composite Polymer Technology improves particle distribution and light scattering efficiency of TiO2, facilitating improvements in hiding efficiency and allowing for up to 20 percent less TiO2 used in the formulation. Additional benefits include improved barrier properties such as stain and corrosion resistance.

Depending on their formulation goals, paint manufacturers can use EVOQUE Pre-Composite Polymer Technology to reduce TiO2 content or improve hiding while they improve paint performance. The technology may also help formulators reduce the carbon footprint of their end products by reducing the energy footprint that comes from mining, processing and transporting TiO2 to their formulation plants. DCM is conducing lifecycle analysis, which will be verified by a third party, to quantify the full spectrum of sustainability advantages that may result from using EVOQUE Pre-Composite Polymer Technology.

“EVOQUE Pre-Composite Polymer Technology gives formulators new options and more flexibility when tailoring paint performance to meet the demands of specific markets and applications,” said Ashok Kalyana, North America Strategic Marketing Manager, Dow Coating Materials. “For example, formulators can use EVOQUE Pre-Composite Polymer Technology to increase the hiding performance and market value of premium paints. They can also use EVOQUE Pre-Composite Polymer Technology to maintain equal hiding and improve paint performance while reducing TiO2 content and raw material cost. It truly provides flexibility to the formulators in designing performance in their paint lines.”

EVOQUE Pre-Composite Polymer Technology is compatible with ROPAQUE™ Opaque Polymers, which were successfully introduced by DCM 30 years ago. EVOQUE Pre-Composite Polymer Technology works in tandem with ROPAQUE Opaque Polymers to further increase hiding efficiency and reduce TiO2.

Titanium dioxide, or TiO2, is the world’s most widely used white pigment due to its brightness and high refractive index. In typical paint formulations, however, the efficiency of TiO2 is limited by uneven particle distribution. This effect can be due to poor dispersion and crowding. Adding more TiO2 helps, but only up to a point before formulators reach a level of diminishing hiding returns.

“We decided to take a different approach,” said Dave Fasano, Research Scientist. “Instead of using more TiO2 to improve hiding, we looked at ways to make it more efficient.”

EVOQUE Pre-Composite Polymers surround and attach to the surface of TiO2 particles. As the two materials come together, they form a composite that makes TiO2 better dispersed and more resistant to crowding.

“In effect, we’re making every particle of TiO2 work smarter,” said Fasano. “That opens up a whole new range of options that formulators do not have with TiO2 alone. Depending on the formulation, EVOQUE Pre-Composite Polymer Technology can also impart improved stain resistance and removal, as well as primer-like properties such as tannin, marker stain blocking or corrosion resistance.”

EVOQUE Pre-Composite Polymer Technology is acrylic based, and early testing indicates excellent durability properties for this platform. These properties are further enhanced by removal of some of the TiO2, which participates in some of the photochemical processes that degrade films. Samples of paint formulated using EVOQUE Pre-Composite Polymer Technology are undergoing exterior exposure testing, and they are performing well. Dow anticipates offering EVOQUE Pre-Composite Polymer Technology for exterior waterborne paints by 2012.

Dow expects full commercialization of EVOQUE Pre-Composite Polymer Technology during the third quarter of 2011, with rapid expansion of the line in 2012.

For additional information about EVOQUE Pre-Composite Polymer Technology, visit www.dow.com/hiding.  
 

Share This Story

Looking for a reprint of this article?
From high-res PDFs to custom plaques, order your copy today!

Recommended Content

JOIN TODAY
to unlock your recommendations.

Already have an account? Sign In

  • pci1022-Kinaltek-Lead-1170.jpg

    A Novel Pigment Production Technology

    Following an extensive R&D program that demonstrated...
    Paint and Coating Pigments
    By: Jawad Haidar and Nitin Soni
  • pci global top 10

    2025 Global Top 10: Top Paint and Coatings Companies

    The following is PCI’s annual ranking of the top 10...
    Paint and Coating Market Reports
    By: Courtney Bassett
  • 2025 pci 25

    2025 PCI 25: Top Paint and Coatings Companies

    PCI's annual ranking of the top 25 North American paint...
    Paint and Coating Market Reports
    By: Courtney Bassett
You must login or register in order to post a comment.

Report Abusive Comment

Manage My Account
  • eMagazine
  • Newsletters
  • Online Registration
  • Subscription Customer Service

More Videos

Sponsored Content

Sponsored Content is a special paid section where industry companies provide high quality, objective, non-commercial content around topics of interest to the PCI audience. All Sponsored Content is supplied by the advertising company and any opinions expressed in this article are those of the author and not necessarily reflect the views of PCI or its parent company, BNP Media. Interested in participating in our Sponsored Content section? Contact your local rep!

close
  • wooden kitchen set and shelving
    Sponsored bySirca North America

    Leveraging Coatings to Meet ESG Goals in Manufacturing

  • man woodworking in workshop
    Sponsored byGemini Industries, Inc.

    Waterborne Coatings Aren't the Future -- They're the New Performance Benchmark

Popular Stories

Akzo, SW, Nippon Logos

AkzoNobel Rejects Cash Offer From Nippon Paint, Sherwin-Williams

BASF SE Logo

BASF Announces Strategic Business Sale

AkzoSWNipponEndTalks

Nippon Paint, Sherwin-Williams End AkzoNobel Pursuit

POB-Point-and-Shoot

PCI Buyers Guide

Submit a Request for Proposal (RFP) to suppliers of your choice with details on what you need with a click of a button

Start your RFP

Browse our Buyers Guide for manufacturers and distributors of all types of coatings products and much more!

Find Suppliers

Events

September 4, 2025

N-Butylpyrrolidone (NBP) as a Green Solvent to Replace N-Methylpyrrolidone (NMP) in Industrial Coating Applications

ON DEMAND: EPA published a regulation proposal around N-methylpyrrolidone (NMP) in June 2024 to ban or limit NMP in many applications, such as paints and coatings and their removers. N-butylpyrrolidone (NBP) is a powerful and versatile solvent for a variety of industries looking for alternatives to substance of very high concern (SVHC)-listed solvents.

September 15, 2026

Coatings Trends & Technologies Summit

The Coatings Trends & Technologies (CTT) Summit is an annual conference for both liquid and powder coatings formulators and manufacturers to discuss innovations in coatings technology. This event combines high-quality technical presentations, a resource-rich exhibit hall, and dedicated networking opportunities to connect scientific minds, foster innovation, and cultivate game-changing new ideas!

View All Submit An Event

Poll

Longest-running laboratory experiment

What is the longest-running laboratory experiment?
View Results Poll Archive

Products

Automotive Paints and Coatings, 2nd Edition

Now in its second edition and still the only book of its kind, this is an authoritative treatment of all stages of the coating process.

See More Products
Inside the AI Shift in Coatings - See the article now

Related Articles

  • Dow Breakthrough Enables Better Paint with Less TiO2

    See More
  • New Binder Permits Up to 50% Less TiO2 for Waterborne Traffic Paints

    See More
  • Nanotechnology Enables Breakthrough Coatings With Improved Resistance to Chipping, Scratching and Water Spotting

    See More

Related Products

See More Products
  • durability.jpg

    Increasing the Durability of Paint and Varnish Coatings in Building Products and Construction 1st Edition

See More Products
×

Keep the info flowing with our eNewsletters!

Get the latest industry updates tailored your way.

JOIN TODAY!
  • RESOURCES
    • Advertise
    • Contact Us
    • Directories
    • Store
    • Want More
    • Manufacturing Division
  • SIGN UP TODAY
    • Create Account
    • eMagazine
    • Newsletters
    • Customer Service
    • Manage Preferences
  • SERVICES
    • Marketing Services
    • Reprints
    • Market Research
    • List Rental
    • Survey & Sample
  • STAY CONNECTED
    • LinkedIn
    • Facebook
    • Youtube
    • X (Twitter)
  • PRIVACY
    • PRIVACY POLICY
    • TERMS & CONDITIONS
    • DO NOT SELL MY PERSONAL INFORMATION
    • PRIVACY REQUEST
    • ACCESSIBILITY

Copyright ©2026. All Rights Reserved BNP Media, Inc. and BNP Media II, LLC.

Design, CMS, Hosting & Web Development :: ePublishing