Painting & Coating Industry (PCI) logo Powder coating summit logo
search
cart
facebook twitter linkedin youtube
  • Sign In
  • Create Account
  • Sign Out
  • My Account
Painting & Coating Industry (PCI) logo Powder coating summit logo
  • NEWS
    • Latest News
    • Market Trends & Reports
    • Finishing News
    • Price Alerts
    • Subscribe to Newsletters
    • Global Top 10/ PCI 25
    • Weekly Featured Article
    • COATLE Word Game
  • PRODUCTS
    • Product News
    • Featured Products
    • Must See Products and Services
  • MATERIALS
    • Additives
    • Resins/Polymers
    • Pigments
    • Equipment
    • Distributors
  • TECHNOLOGIES
    • Adhesives
    • Architectural Coatings
    • Finishing Articles
    • Finishing Technologies
    • Finishing Equipment
    • Industrial Coatings
    • Nanotechnology
    • Powder Coatings
    • Solventborne
    • Special Purpose Coatings
    • Sustainability
    • UV Coatings
    • Waterborne
  • RESOURCES
    • Columns
      • Did you know?
      • Distribution Dive
      • Formulating With Mike
      • Innovation Insights
      • Powder Coating Perspectives
      • TiO2 Insider
    • Blogs
      • Editor's Viewpoint
      • Industry Insights
    • Coatings Supplier Handbook
    • Podcasts and Videos
      • COAT-IT! Podcast
      • Videos/PCI TV
    • PCI Store
    • Classifieds
    • eBooks
    • Sponsor Insights
    • White Papers
    • COATLE Word Game
  • EVENTS
    • Coatings Trends & Technologies Summit
    • Paint and Coatings Academy
    • Webinars
    • Calendar of Events
    • Lifetime Achievement Award
  • DIRECTORIES
    • Buyer's Guide
    • Equipment Directory
    • Materials Directory
  • EMAGAZINE
    • Current Issue
    • eMagazine Archive
    • China Issue Archive
    • Editorial Advisory Board
  • CONTACT
    • Contact Us
    • Advertise
    • Subscribe to eMagazine
    • Subscribe to Newsletters
  • SIGN UP!

Epoxy Floor Coating Producer Eliminates Processing Step - Prevents Pigment Float and Flocculation

January 18, 2006
Series 22 colorant formulation from Ferro Corporation is said to prevent float and flocculation of pigments, increasing uniformity of coloration achieved using "4800 Epoxy Colorseal" from Versatile Building Products. Versatile Building Products Inc. (VBP) manufactures treatment and repair products for cement, concrete and stone floors. These range from epoxy and polyurethane coating systems for commercial and residential applications to stains, sealers, mortar and substrate repair materials.



Versatile Building Products Inc. (VBP) manufactures treatment and repair products for cement, concrete and stone floors. These range from epoxy and polyurethane coating systems for commercial and residential applications to stains, sealers, mortar and substrate repair materials. Many of these durable products are offered in colors and special effects such as faux granite.

One such product is the company's 4800 Epoxy Colorseal, a chemical- and abrasion-resistant topcoat for concrete floors specifically formulated to reduce or eliminate color variations associated with epoxy coatings. These variations, explains Mark Glendrange, VBP's technical director, are due to the "float and flocculation" of pigments that occurs in the coating following application, until the point of cure.

Float occurs when pigments, which are lighter than other additives in a blend, rise to the surface of the resin, while flocculation is caused by the tendency of pigments to agglomerate. Both float and flocculation, and the color variations they cause, increase over time in activated, uncured resin, so the first portions of a batch applied to a concrete floor undergo color changes many times greater than the portions applied last.

The company overcame float and flocculation problems by switching from in-house processing of dry pigments to purchasing newly developed "Series 22" epoxy color dispersions from Ferro Corporation. According to Glendrange, the formulation exhibits significantly greater pigment stability, eliminating the patchy appearance of coatings associated with conventional liquid and paste dispersions.

VBP previously purchased pigments and additives, ground them to size, and blended them with the epoxy topcoat. Glendrange says the process was time-consuming and difficult. Among the problems encountered was the time it took to grind pigments and additives to the right particle size, a process that's challenging since some pigments are much larger or have greater densities than others. Titanium dioxide (white), for example, is thousands of times larger than carbon (black), with which it is blended to produce one of the three shades of gray VBP supplies in the 4800 Epoxy Colorseal line. Differences in particle size and density can also cause minute metering errors that affect color quality.

The total cost of grinding and dispersing of pigments in a blend was considerable. "Capitalizing equipment for dispersion of pigment can be prohibitive," Glendrange says. "There are also expenses associated with the safe handling of pigments and additives, especially in dust containment, downtime required for material changeover and equipment cleaning, and the use and disposal of regulated chemicals like solvents for cleaning."

"We decided it made more sense to source colorants for the 4800 Epoxy Colorseal line that were already sized and dispersed in a carrier," he notes, "and Ferro offered considerable expertise in this area."

The colorant is comprised of pigments that are broken down into individual particles and wet-out in suspension, preventing re-agglomeration while increasing opacity of the original pigment by 50% to 80%.

The carrier resin is a proprietary, highly stable, 100%-solids, bisphenol A epoxy resin that is reactive with all epoxy formulations. VBP orders four base colors from which it custom blends the 10 colors in the topcoat line: white, black, yellow, blue, green, red, umber, and three shades of gray. The company maintains an inventory of standard colors, and does custom color for an extra charge. Technicians weigh the colorants with a gram scale and produce batches of up to 150 gallons, which are usually supplied in 1.5-gallon pails.

"Colorseal topcoat is typically applied with a brush, roller or squeegee in thicknesses of 4 to 10 mils. The high pigment loadings and stability of the colorant improves handling and application of the topcoat, which increases the quality and value of our product," says Glendrange.

"Some epoxy coatings are not user-friendly. That's one thing VBP has done much to change. A company can make the best coating in the world, but if a contractor can't work with it, it's worthless."

For more information contact Versatile Building Products Inc., 20420 South Susana Rd., Carson, CA 90810; phone 800/535.3325; www.garagecoatings.com; or Ferro Corp., 54 Kellogg Ct., Edison, NJ 08817-2509; phone 800/882.1456 x 2835; www.ferro.com.

Share This Story

Looking for a reprint of this article?
From high-res PDFs to custom plaques, order your copy today!

Recommended Content

JOIN TODAY
to unlock your recommendations.

Already have an account? Sign In

  • pci1022-Kinaltek-Lead-1170.jpg

    A Novel Pigment Production Technology

    Following an extensive R&D program that demonstrated...
    Paint and Coating Pigments
    By: Jawad Haidar and Nitin Soni
  • pci global top 10

    2025 Global Top 10: Top Paint and Coatings Companies

    The following is PCI’s annual ranking of the top 10...
    Paint and Coating Market Reports
    By: Courtney Bassett
  • 2025 pci 25

    2025 PCI 25: Top Paint and Coatings Companies

    PCI's annual ranking of the top 25 North American paint...
    Global Top 10 and PCI 25
    By: Courtney Bassett
You must login or register in order to post a comment.

Report Abusive Comment

Manage My Account
  • eMagazine
  • Newsletters
  • Online Registration
  • Subscription Customer Service

More Videos

Sponsored Content

Sponsored Content is a special paid section where industry companies provide high quality, objective, non-commercial content around topics of interest to the PCI audience. All Sponsored Content is supplied by the advertising company and any opinions expressed in this article are those of the author and not necessarily reflect the views of PCI or its parent company, BNP Media. Interested in participating in our Sponsored Content section? Contact your local rep!

close
  • wooden kitchen set and shelving
    Sponsored bySirca North America

    Leveraging Coatings to Meet ESG Goals in Manufacturing

  • man woodworking in workshop
    Sponsored byGemini Industries, Inc.

    Waterborne Coatings Aren't the Future -- They're the New Performance Benchmark

Popular Stories

Akzo, SW, Nippon Logos

AkzoNobel Rejects Cash Offer From Nippon Paint, Sherwin-Williams

BASF SE Logo

BASF Announces Strategic Business Sale

AkzoSWNipponEndTalks

Nippon Paint, Sherwin-Williams End AkzoNobel Pursuit

POB-Point-and-Shoot

PCI Buyers Guide

Submit a Request for Proposal (RFP) to suppliers of your choice with details on what you need with a click of a button

Start your RFP

Browse our Buyers Guide for manufacturers and distributors of all types of coatings products and much more!

Find Suppliers

Events

September 4, 2025

N-Butylpyrrolidone (NBP) as a Green Solvent to Replace N-Methylpyrrolidone (NMP) in Industrial Coating Applications

ON DEMAND: EPA published a regulation proposal around N-methylpyrrolidone (NMP) in June 2024 to ban or limit NMP in many applications, such as paints and coatings and their removers. N-butylpyrrolidone (NBP) is a powerful and versatile solvent for a variety of industries looking for alternatives to substance of very high concern (SVHC)-listed solvents.

September 15, 2026

Coatings Trends & Technologies Summit

The Coatings Trends & Technologies (CTT) Summit is an annual conference for both liquid and powder coatings formulators and manufacturers to discuss innovations in coatings technology. This event combines high-quality technical presentations, a resource-rich exhibit hall, and dedicated networking opportunities to connect scientific minds, foster innovation, and cultivate game-changing new ideas!

View All Submit An Event

Poll

Longest-running laboratory experiment

What is the longest-running laboratory experiment?
View Results Poll Archive

Products

Automotive Paints and Coatings, 2nd Edition

Now in its second edition and still the only book of its kind, this is an authoritative treatment of all stages of the coating process.

See More Products
Inside the AI Shift in Coatings - See the article now

Related Articles

  • Industry's First Water-Based Epoxy Floor Coating System for Static Control

    See More
  • New Web Site Indexes Epoxy-Floor Articles

    See More
  • New Web Site Indexes Epoxy-Floor Articles

    See More

Related Products

See More Products
  • biological.jpg

    Biological and Biomedical Coatings Handbook: Processing and Characterization

  • Powder Coatings Processing (Virtual Course - 6/25/26)

  • Pigment Dispersion (Virtual Course - 11/19/26)

See More Products
×

Keep the info flowing with our eNewsletters!

Get the latest industry updates tailored your way.

JOIN TODAY!
  • RESOURCES
    • Advertise
    • Contact Us
    • Directories
    • Store
    • Want More
    • Manufacturing Division
  • SIGN UP TODAY
    • Create Account
    • eMagazine
    • Newsletters
    • Customer Service
    • Manage Preferences
  • SERVICES
    • Marketing Services
    • Reprints
    • Market Research
    • List Rental
    • Survey & Sample
  • STAY CONNECTED
    • LinkedIn
    • Facebook
    • Youtube
    • X (Twitter)
  • PRIVACY
    • PRIVACY POLICY
    • TERMS & CONDITIONS
    • DO NOT SELL MY PERSONAL INFORMATION
    • PRIVACY REQUEST
    • ACCESSIBILITY

Copyright ©2026. All Rights Reserved BNP Media, Inc. and BNP Media II, LLC.

Design, CMS, Hosting & Web Development :: ePublishing