Ford’s David Bauer To Receive Tess Award

David R. Bauer will receive the prestigious Roy W. Tess Award in Coatings for 2000.

WASHINGTON — David R. Bauer, Ford Motor Co., will receive the prestigious Roy W. Tess Award in Coatings for 2000, a prize sponsored by the Division of Polymeric Materials: Science and Engineering of the American Chemical Society.

Bauer is senior staff technical specialist in the Materials Science Department of Ford’s Research Laboratory. He is regarded as an expert on the mechanisms and kinetics of cure; network structure in high-solids coatings; flow control and coatings rheology; polymer photodegradation and stabilization; plastics characterization; and coating service-life prediction. He has authored more than 100 technical papers on coatings and plastics research, and delivered the 1996 Mattiello Lecture of the Federation of Societies for Coatings Technology. The Tess Award will be presented by PMSE Division Chairman Christopher Ober on Aug. 21, during the 220th meeting of the American Chemical Society in Washington.

Bauer’s research credits include extensive use of infrared spectroscopy to study the crosslinking kinetics of melamine-formaldehyde resins and isocyanates, and he was the first to apply network models to calculate crosslink densities from chemical measurements. He also carried out fundamental measurements of coating rheology, and developed quantitative relationships between rheological parameters, coating-formulation parameters and sag-control agents. His work led to a comprehensive model of coating flow, from application to cure. Bauer also has made significant contributions to the study of coating degradation and stabilization, and was the first to measure the rate of crosslink hydrolysis in acrylic-melamine coatings, a process crucial to acid-etch resistance. His research also has focused on the interaction of light and water in the degradation chemistries of coatings; coatings photooxidation kinetics and stabilization by HALS additives; and development of coating-failure models.

Bauer has a Ph.D. in chemical physics from Stanford University. He joined Ford in 1977, and worked for 22 years in the coatings and plastics areas.

You must register or login in order to post comments.

Multimedia

Videos

Image Galleries

American Coating Show 2012

The American Coatings Show and Conference, held every two years, took place May 7-10 at the Indiana Convention Center in Indianapolis, IN, in the heart of the Manufacturing Belt, the oldest and largest concentration of industrial companies in the Midwest.

Podcasts

PCI Top 5 - January 12, 2012
PCI's Podcast series on the five most e-mailed/shared articles and stories for the week.

More Podcasts

THE MAGAZINE

PCI Magazine

PCI may 2012 cover

2012 May

Check out PCI's May issue!!

TABLE OF CONTENTS SUBSCRIBE

iPad

Do you own/use an iPad?
If yes, do you use your iPad for business or personal reasons?
Have you purchased a business app within the last 6 months?
See Poll Results Poll Archive

THE PCI STORE

PCI-June-2011-Coversmall.gif
PCI Additives Handbook

Encyclopedia of information on the properties and uses of coatings additives.

More Products

Clear Seas Research

Clear Seas ResearchWith access to over one million professionals and more than 60 industry-specific publications,Clear Seas Research offers relevant insights from those who know your industry best. Let us customize a market research solution that exceeds your marketing goals.

Virtual Brochures

PageCollageClick on the Virtual Brochures page to view multiple categories that list downloadable product literature from leading industry suppliers.

STAY CONNECTED

Facebook Twitter  LinkedIn YouTube