Painting & Coating Industry (PCI) logo Powder coating summit logo
search
cart
facebook twitter linkedin youtube
  • Sign In
  • Create Account
  • Sign Out
  • My Account
Painting & Coating Industry (PCI) logo Powder coating summit logo
  • NEWS
    • Latest News
    • Market Trends & Reports
    • Finishing News
    • Price Alerts
    • Subscribe to Newsletters
    • Global Top 10/ PCI 25
    • Weekly Featured Article
    • COATLE Word Game
  • PRODUCTS
    • Product News
    • Featured Products
    • Must See Products and Services
  • MATERIALS
    • Additives
    • Resins/Polymers
    • Pigments
    • Equipment
    • Distributors
  • TECHNOLOGIES
    • Adhesives
    • Architectural Coatings
    • Finishing Articles
    • Finishing Technologies
    • Finishing Equipment
    • Industrial Coatings
    • Nanotechnology
    • Powder Coatings
    • Solventborne
    • Special Purpose Coatings
    • Sustainability
    • UV Coatings
    • Waterborne
  • RESOURCES
    • Columns
      • Did you know?
      • Distribution Dive
      • Formulating With Mike
      • Innovation Insights
      • Powder Coating Perspectives
      • TiO2 Insider
    • Blogs
      • Editor's Viewpoint
      • Industry Insights
    • Coatings Supplier Handbook
    • Podcasts and Videos
      • COAT-IT! Podcast
      • Videos/PCI TV
    • PCI Store
    • Classifieds
    • eBooks
    • Sponsor Insights
    • White Papers
    • COATLE Word Game
  • EVENTS
    • Coatings Trends & Technologies Summit
    • Paint and Coatings Academy
    • Webinars
    • Calendar of Events
    • Lifetime Achievement Award
  • DIRECTORIES
    • Buyer's Guide
    • Equipment Directory
    • Materials Directory
  • EMAGAZINE
    • Current Issue
    • eMagazine Archive
    • China Issue Archive
    • Editorial Advisory Board
  • CONTACT
    • Contact Us
    • Advertise
    • Subscribe to eMagazine
    • Subscribe to Newsletters
  • SIGN UP!

Formulating Solutions: Meeting VOC Regulations with Coalescents

February 1, 2005
For decades, contractors and consumers have used latex paints in architectural applications, coating the interior and exterior walls of homes and businesses. The ease of soap and water cleanup and lower odor than in solventborne systems has led to an increase in the use of waterborne paints in architectural, industrial maintenance and automotive coatings.

Recently, increasingly stringent environmental regulations have required changes in how latex paints used in architectural applications are formulated. A variety of formulating methods and new raw materials have been developed to help paint manufacturers meet the new regulations. Now formulators can meet VOC regulations while maintaining performance properties in architectural coatings. The following provides an overview of formulation techniques to help balance performance and regulatory compliance in latex paints for architectural applications.

Regulatory Issues

Paint formulators in certain U.S. regions struggle to achieve the correct balance between meeting today's stringent VOC requirements while maintaining the performance properties of architectural coatings. The two main additives that add VOC to a latex paint are antifreeze/open-time additives (i.e., ethylene and propylene glycol) and coalescents. Conventional coalescents add VOC, but mixing and matching with other types of coalescents can actually reduce the VOC of latex paints.

Coalescents

Architectural latex paints are made from a variety of different polymers that are selected based on performance requirements and cost. The monomers used in these polymers determine the glass transition temperature (Tg), which characterizes the hardness of the final polymer at a given temperature. The Tg and polymer type influence the amount and type of solvent required to coalesce the polymer. Substrate, application, dry time, compatibility, VOC regulations, and efficiency all play a role in determining the type of solvent or combination of solvents to be used.

A conventional coalescent temporarily lowers the Tg, providing mobility to the polymer chains. The softened polymer can then flow and fuse with other polymer chains in the system, creating a protective, decorative film. To be effective, the coalescent has to remain in the film after the water has evaporated to ensure that a homogeneous film develops. A conventional coalescent will evaporate out of the film after a period of time and the film will regain its initial Tg and hardness. Various coalescents can be used individually or in combination to help formulators optimize performance in architectural coatings, while meeting VOC regulations.

Formulating Options
Glycol Removal

There are many options for formulators striving to meet VOC requirements. One way, for example, is glycol removal. In a typical latex paint, the largest contributor to VOC comes from glycol, added for freeze/thaw stability and increased open-time. It is normally present at levels two to three times the amount of the coalescent. In most cases, formulators could meet VOC requirements by simply leaving out the glycol, but this can lead to problems in colder climates, where freezing can occur, and in paints where open-time is important.

Use of a Lower Tg Latex

Another method is to use a lower Tg latex, which requires little to no solvent to form a film. However, these latexes generally have limited formulation latitude. This option requires the formulator to reformulate and test the paint, which can be time-consuming and expensive. In addition, these polymers are inherently soft and remain soft throughout the life of the paint, never regaining hardness like conventional latexes that have been coalesced to form a film. In addition, these low-Tg latexes are susceptible to freezing unless formulated with glycol.

Use of Non-Fugitive or Reactive Coalescents

An additional option is to replace some of the conventional solvents used in latex paints with a higher boiling film former, which is either non- or partially fugitive. Recently, non-fugitive film formers have been advertised to help companies formulate low-VOC paints while using their current latexes. Non-fugitive implies that the coalescent remains in the film for the life of the coating, or at least much longer than a conventional coalescent. A non-fugitive coalescent allows the formulator to lower VOC while minimizing any adverse affects, such as hardness development. Care should be taken to evaluate the impact of these materials on surface properties such as dirt pick-up and block resistance.

Another non-fugitive coalescent approach to lowering VOC is the use of materials that react or crosslink at ambient temperature after paint application. Reactive coalescents are said to crosslink using an alkyd-like oxidative cure mechanism. One issue with this type of system is that unsaturation can cause yellowing in a latex emulsion. There is little evidence to suggest that reactive coalescents lead to crosslinking significant enough to positively influence paint properties. If a formulator needs to use a low-VOC film former, then it is best to use one that is non-yellowing

Formulation Alternatives to Achieve Desired VOC Levels

For some time, the paint industry has used 2,2,4-trimethyl-1,3-pentanediol monoisobutyrate (trade name: Texanol Ester Alcohol) as the standard coalescent for architectural paints (Table 1). However, in regions where formulators are hindered by VOC limits, it may be necessary to replace one coalescent with another that is more efficient, or blend it with a film former that does not contribute to the volatility of the paint. The volatility of paint components can be tested by ASTM D 2369, which is one of the tests outlined in EPA's Method 24. A formulator could replace all or some of the coalescent with one that is more efficient in lowering the Tg of the polymer, such as Eastman EEH solvent (Table 2). Another possibility is to substitute a portion of the conventional coalescent with a low-VOC film former like Optifilm Enhancer 400 (Table 3). Optifilm Enhancer 400 is only about 2% VOC when the neat material is measured by ASTM D 2369.

Summary

Historically, paint formulators have always had to deal with making high-quality paint while keeping the overall cost as low as possible. Today's VOC regulations create additional challenges to formulating paint. Formulators must meet these environmental regulations while still maximizing the original performance qualities of their coatings. In order to remain competitive in an ever-changing market, formulators will need to learn what products can enable them to offer the best value to their customers with minimum compromise.

Jerry M. Mitchell has been with Eastman Chemical Company for the last 12 years. He is currently a Coatings Technologist with the Technical Service Department of Eastman's Coatings Technology Division, serving as the technical contact for Eastman's coalescing aids and plasticizers for coatings with a focus on water-based architectural paints.

Share This Story

Looking for a reprint of this article?
From high-res PDFs to custom plaques, order your copy today!

Recommended Content

JOIN TODAY
to unlock your recommendations.

Already have an account? Sign In

  • pci1022-Kinaltek-Lead-1170.jpg

    A Novel Pigment Production Technology

    Following an extensive R&D program that demonstrated...
    Paint and Coating Pigments
    By: Jawad Haidar and Nitin Soni
  • pci global top 10

    2025 Global Top 10: Top Paint and Coatings Companies

    The following is PCI’s annual ranking of the top 10...
    Global Top 10 and PCI 25
    By: Courtney Bassett
  • 2025 pci 25

    2025 PCI 25: Top Paint and Coatings Companies

    PCI's annual ranking of the top 25 North American paint...
    Paint and Coating Market Reports
    By: Courtney Bassett
You must login or register in order to post a comment.

Report Abusive Comment

Manage My Account
  • eMagazine
  • Newsletters
  • Online Registration
  • Subscription Customer Service

More Videos

Sponsored Content

Sponsored Content is a special paid section where industry companies provide high quality, objective, non-commercial content around topics of interest to the PCI audience. All Sponsored Content is supplied by the advertising company and any opinions expressed in this article are those of the author and not necessarily reflect the views of PCI or its parent company, BNP Media. Interested in participating in our Sponsored Content section? Contact your local rep!

close
  • wooden kitchen set and shelving
    Sponsored bySirca North America

    Leveraging Coatings to Meet ESG Goals in Manufacturing

  • man woodworking in workshop
    Sponsored byGemini Industries, Inc.

    Waterborne Coatings Aren't the Future -- They're the New Performance Benchmark

Popular Stories

Akzo, SW, Nippon Logos

AkzoNobel Rejects Cash Offer From Nippon Paint, Sherwin-Williams

BASF SE Logo

BASF Announces Strategic Business Sale

AkzoSWNipponEndTalks

Nippon Paint, Sherwin-Williams End AkzoNobel Pursuit

POB-Point-and-Shoot

PCI Buyers Guide

Submit a Request for Proposal (RFP) to suppliers of your choice with details on what you need with a click of a button

Start your RFP

Browse our Buyers Guide for manufacturers and distributors of all types of coatings products and much more!

Find Suppliers

Events

September 4, 2025

N-Butylpyrrolidone (NBP) as a Green Solvent to Replace N-Methylpyrrolidone (NMP) in Industrial Coating Applications

ON DEMAND: EPA published a regulation proposal around N-methylpyrrolidone (NMP) in June 2024 to ban or limit NMP in many applications, such as paints and coatings and their removers. N-butylpyrrolidone (NBP) is a powerful and versatile solvent for a variety of industries looking for alternatives to substance of very high concern (SVHC)-listed solvents.

September 15, 2026

Coatings Trends & Technologies Summit

The Coatings Trends & Technologies (CTT) Summit is an annual conference for both liquid and powder coatings formulators and manufacturers to discuss innovations in coatings technology. This event combines high-quality technical presentations, a resource-rich exhibit hall, and dedicated networking opportunities to connect scientific minds, foster innovation, and cultivate game-changing new ideas!

View All Submit An Event

Poll

Longest-running laboratory experiment

What is the longest-running laboratory experiment?
View Results Poll Archive

Products

Automotive Paints and Coatings, 2nd Edition

Now in its second edition and still the only book of its kind, this is an authoritative treatment of all stages of the coating process.

See More Products
Inside the AI Shift in Coatings - See the article now

Related Articles

  • industry insights O’Shaughnessy,

    High Solids Epoxy: A Solution to the EPA’s VOC Regulations

    See More
  • High Solids Epoxy: A Solution to the EPA’s VOC Regulations

    High Solids Epoxy: A Solution to the EPA’s VOC Regulations

    See More
  • New VOC Regulations on AIM Coatings Looming in Northeast, Mid-Atlantic States

    See More

Related Directories

  • UNISIL

    Unisil is a manufacturer of advanced organosilicon materials for high-performance applications. Our portfolio includes silicone fluids, emulsions, resins, and siliconates used in paints and coatings, CASE, construction chemicals, and building materials. We support customers globally with consistent quality, reliable supply, strong technical expertise, and application development and formulation support.
  • Formulator Software LLC

    At Formulator Software, we understand the precision and complexity involved in perfecting formulations. Our software is designed specifically for chemists, lab technicians, researchers, and manufacturers, providing essential tools to streamline the entire formulation process. Formed in 2002, Formulator Software is trusted by thousands to manage their raw materials, formulations, QC, SDS, COA, costing and more!
×

Keep the info flowing with our eNewsletters!

Get the latest industry updates tailored your way.

JOIN TODAY!
  • RESOURCES
    • Advertise
    • Contact Us
    • Directories
    • Store
    • Want More
    • Manufacturing Division
  • SIGN UP TODAY
    • Create Account
    • eMagazine
    • Newsletters
    • Customer Service
    • Manage Preferences
  • SERVICES
    • Marketing Services
    • Reprints
    • Market Research
    • List Rental
    • Survey & Sample
  • STAY CONNECTED
    • LinkedIn
    • Facebook
    • Youtube
    • X (Twitter)
  • PRIVACY
    • PRIVACY POLICY
    • TERMS & CONDITIONS
    • DO NOT SELL MY PERSONAL INFORMATION
    • PRIVACY REQUEST
    • ACCESSIBILITY

Copyright ©2026. All Rights Reserved BNP Media, Inc. and BNP Media II, LLC.

Design, CMS, Hosting & Web Development :: ePublishing