Painting & Coating Industry (PCI) logo Powder coating summit logo
search
cart
facebook twitter linkedin youtube
  • Sign In
  • Create Account
  • Sign Out
  • My Account
Painting & Coating Industry (PCI) logo Powder coating summit logo
  • NEWS
    • Latest News
    • Market Trends & Reports
    • Finishing News
    • Price Alerts
    • Subscribe to Newsletters
    • Global Top 10/ PCI 25
    • Weekly Featured Article
    • COATLE Word Game
  • PRODUCTS
    • Product News
    • Featured Products
    • Must See Products and Services
  • MATERIALS
    • Additives
    • Resins/Polymers
    • Pigments
    • Equipment
    • Distributors
  • TECHNOLOGIES
    • Adhesives
    • Architectural Coatings
    • Finishing Articles
    • Finishing Technologies
    • Finishing Equipment
    • Industrial Coatings
    • Nanotechnology
    • Powder Coatings
    • Solventborne
    • Special Purpose Coatings
    • Sustainability
    • UV Coatings
    • Waterborne
  • RESOURCES
    • Columns
      • Did you know?
      • Distribution Dive
      • Formulating With Mike
      • Innovation Insights
      • Powder Coating Perspectives
      • TiO2 Insider
    • Blogs
      • Editor's Viewpoint
      • Industry Insights
    • Coatings Supplier Handbook
    • Podcasts and Videos
      • COAT-IT! Podcast
      • Videos/PCI TV
    • PCI Store
    • Classifieds
    • eBooks
    • Sponsor Insights
    • White Papers
    • COATLE Word Game
  • EVENTS
    • Coatings Trends & Technologies Summit
    • Paint and Coatings Academy
    • Webinars
    • Calendar of Events
    • Lifetime Achievement Award
  • DIRECTORIES
    • Buyer's Guide
    • Equipment Directory
    • Materials Directory
  • EMAGAZINE
    • Current Issue
    • eMagazine Archive
    • China Issue Archive
    • Editorial Advisory Board
  • CONTACT
    • Contact Us
    • Advertise
    • Subscribe to eMagazine
    • Subscribe to Newsletters
  • SIGN UP!
FT Archives

Industry Forum: Replacing Chromium

June 14, 2004
For over 50 years chromium has been used as a corrosion-inhibiting element for metal surfaces. Its high solubility makes it an ideal corrosion inhibitor in paints, but can negatively impact the environment and humans if proper safety and health measures are not followed. In the aerospace industry, hexavalent chromium is used in conversion coatings and primers to protect the aluminum structure from corrosion. As long as aircraft are manufactured with aluminum, the need to protect aluminum from corrosion will be a critical issue.

Most aerospace aluminum structure is protected with chrome in two ways. First, the aluminum is treated with a chromate conversion coating. The conversion coating provides some corrosion protection and improves subsequent paint adhesion. The structure is then coated with a chromated primer. The chromated primer provides the majority of the corrosion protection.

The current OSHA Permissible Exposure Limit (PEL) for Cr+6 is 52 mg/m3 (ceiling limit). OSHA is currently considering a PEL in the range of 0.5 mg/m3 to 5 mg/m3 with a possible final rule date of Jan. 18, 2006.

OSHA's expanded standard could include enhanced training, medical surveillance, enhanced personal protective equipment and designated changing areas. Finding a suitable, environmentally friendly replacement for chromium would be a major effort for the coatings industry.

The word "suitable" is critical. No one wants to sacrifice corrosion resistance when implementing a nonchrome protective coating.

The Boeing Co. has worked hard to develop nonchrome corrosion inhibitors suitable for protecting aluminum aircraft structures and has tested more than 100 nonchrome primers over the past few years. Getting a nonchrome primer to successfully perform on all the various aluminum alloys used on aircraft is a significant challenge. While laboratory-accelerated corrosion methods are used in the industry, operational testing is needed as a real life method of determining nonchrome primers' effectiveness.

Boeing had the opportunity to lead a nonchrome primer evaluation program sponsored by the Joint Group for Pollution Prevention (JG-PP) beginning in 1995. The charter of this effort called for evaluating existing state-of-the-art nonchrome primer technology, and performing an extensive field evaluation of the leading candidate coatings. Multiple nonchrome primers were tested, and the best primers were found to be approximately 80% as good as the chromate control in corrosion protection. Even though the nonchrome primer did not meet the laboratory testing requirements of chromated primer, the stakeholders chose to proceed with operational testing.

The plan was to evaluate performance for two years, but the project was extended since no discernable differences were noted after two years. Nonchrome primers were test flown on multiple military aircraft for up to six years with no discernible corrosion performance deficiencies.

Additional military aircraft painted in 2000 and 2001 continue to be monitored. To minimize risk, the primers were only applied to external surfaces that can be easily inspected for corrosion. Internal structure, where most corrosion occurs, will someday need to be field-evaluated with nonchrome primers. The latest field evaluation of the JG-PP aircraft shows the nonchrome primers to be performing as good as the chromated primers when used with a chromate conversion coating pretreatment.

It may take multiple nonchrome corrosion-inhibiting compounds to provide corrosion protection comparable to chromium. Chrome has been used for many years, yet its mechanism of corrosion protection has only recently been understood. Understanding the mechanism of the nonchrome corrosion inhibitors is also needed to aid further development efforts.

Finding a replacement for chromium is a daunting challenge, but progress continues to be made. As the clock ticks down to OSHA's impending expanded chromium standard, industry continues to search for a safe and effective replacement for chromium.

Share This Story

Looking for a reprint of this article?
From high-res PDFs to custom plaques, order your copy today!

Recommended Content

JOIN TODAY
to unlock your recommendations.

Already have an account? Sign In

  • pci1022-Kinaltek-Lead-1170.jpg

    A Novel Pigment Production Technology

    Following an extensive R&D program that demonstrated...
    Paint and Coating Pigments
    By: Jawad Haidar and Nitin Soni
  • pci global top 10

    2025 Global Top 10: Top Paint and Coatings Companies

    The following is PCI’s annual ranking of the top 10...
    Paint and Coating Market Reports
    By: Courtney Bassett
  • 2025 pci 25

    2025 PCI 25: Top Paint and Coatings Companies

    PCI's annual ranking of the top 25 North American paint...
    Global Top 10 and PCI 25
    By: Courtney Bassett
You must login or register in order to post a comment.

Report Abusive Comment

Manage My Account
  • eMagazine
  • Newsletters
  • Online Registration
  • Subscription Customer Service

More Videos

Sponsored Content

Sponsored Content is a special paid section where industry companies provide high quality, objective, non-commercial content around topics of interest to the PCI audience. All Sponsored Content is supplied by the advertising company and any opinions expressed in this article are those of the author and not necessarily reflect the views of PCI or its parent company, BNP Media. Interested in participating in our Sponsored Content section? Contact your local rep!

close
  • wooden kitchen set and shelving
    Sponsored bySirca North America

    Leveraging Coatings to Meet ESG Goals in Manufacturing

  • man woodworking in workshop
    Sponsored byGemini Industries, Inc.

    Waterborne Coatings Aren't the Future -- They're the New Performance Benchmark

Popular Stories

Akzo, SW, Nippon Logos

AkzoNobel Rejects Cash Offer From Nippon Paint, Sherwin-Williams

BASF SE Logo

BASF Announces Strategic Business Sale

AkzoSWNipponEndTalks

Nippon Paint, Sherwin-Williams End AkzoNobel Pursuit

POB-Point-and-Shoot

PCI Buyers Guide

Submit a Request for Proposal (RFP) to suppliers of your choice with details on what you need with a click of a button

Start your RFP

Browse our Buyers Guide for manufacturers and distributors of all types of coatings products and much more!

Find Suppliers

Events

September 4, 2025

N-Butylpyrrolidone (NBP) as a Green Solvent to Replace N-Methylpyrrolidone (NMP) in Industrial Coating Applications

ON DEMAND: EPA published a regulation proposal around N-methylpyrrolidone (NMP) in June 2024 to ban or limit NMP in many applications, such as paints and coatings and their removers. N-butylpyrrolidone (NBP) is a powerful and versatile solvent for a variety of industries looking for alternatives to substance of very high concern (SVHC)-listed solvents.

September 15, 2026

Coatings Trends & Technologies Summit

The Coatings Trends & Technologies (CTT) Summit is an annual conference for both liquid and powder coatings formulators and manufacturers to discuss innovations in coatings technology. This event combines high-quality technical presentations, a resource-rich exhibit hall, and dedicated networking opportunities to connect scientific minds, foster innovation, and cultivate game-changing new ideas!

View All Submit An Event

Poll

Longest-running laboratory experiment

What is the longest-running laboratory experiment?
View Results Poll Archive

Products

Automotive Paints and Coatings, 2nd Edition

Now in its second edition and still the only book of its kind, this is an authoritative treatment of all stages of the coating process.

See More Products
Inside the AI Shift in Coatings - See the article now

Related Articles

  • Industry Forum

    See More
  • TZMI.jpg

    TZMI to Host TiO2 Industry Forum in Columbus

    See More
  • INDUSTRY FORUM: Looking Back and Looking Forward

    See More

Related Products

See More Products
  • Automotive Paints and Coatings, 2nd Edition

See More Products
×

Keep the info flowing with our eNewsletters!

Get the latest industry updates tailored your way.

JOIN TODAY!
  • RESOURCES
    • Advertise
    • Contact Us
    • Directories
    • Store
    • Want More
    • Manufacturing Division
  • SIGN UP TODAY
    • Create Account
    • eMagazine
    • Newsletters
    • Customer Service
    • Manage Preferences
  • SERVICES
    • Marketing Services
    • Reprints
    • Market Research
    • List Rental
    • Survey & Sample
  • STAY CONNECTED
    • LinkedIn
    • Facebook
    • Youtube
    • X (Twitter)
  • PRIVACY
    • PRIVACY POLICY
    • TERMS & CONDITIONS
    • DO NOT SELL MY PERSONAL INFORMATION
    • PRIVACY REQUEST
    • ACCESSIBILITY

Copyright ©2026. All Rights Reserved BNP Media, Inc. and BNP Media II, LLC.

Design, CMS, Hosting & Web Development :: ePublishing