Kemira Sells Stake in Scanspac to Saint-Gobain
VANTAA,
Finland - Alcro-Beckers AB, part of the Finnish Tikkurila that is responsible
for Kemira’s paints and coatings business, has signed an agreement to sell its
50-percent stake in the Swedish filler producer Scanspac to Gyproc AB, part of
the Gypsum Activity of Saint-Gobain. Net sales of Scanspac’s operations totaled
approximately €26 million in 2006.
Scanspac is currently owned 50/50 by Alcro-Beckers AB, a subsidiary of Tikkurila Oy, and maxit Group. Scanspac is the leading filler producer in the Nordic area with production units in Glanshammar and Sala in Sweden. Its customers are paint manufacturers, distributors and retailers who serve professional users and consumers. Scanspac’s products are distributed under customers’ brands and under its own brands of Dalapro, Gullspack and Breplasta.