Microfluidics Develops Methods for Processing Carbon Nanotubes

NEWTON, MA - Microfluidics, a wholly owned subsidiary of MFIC Corp., has devised a methodology to process, deagglomerate, and facilitate purification and stabilization of carbon nanotubes so they can be used in an optimal manner, thus achieving enhanced functionality and performance.
 
The company has identified and demonstrated several specific operational protocols utilizing its Microfluidizer® processor systems to prepare these bulk nanotubes for their ultimate specific uses. These applications capitalize on the unique mechanical, electrical and thermal properties of carbon nanotubes, and require dispersion of the nanotubes in liquid media and independent length reduction of the carbon nanotubes.
 
Carbon nanotubes are noted for their tubular shape, extremely small diameter with respect to length, and exceptional physical, mechanical and electrical properties. When prepared in diameters in the 10-50 nanometer range, the unique characteristics of strength, conductivity and quantum behavior become highly desirable and are thus incorporated into a multitude of commercial products.
 
Microfluidizer processors are ideal for conditioning carbon nanotubes (and nanomaterials in general) for applications that include high-tensile strength polymers, fabric treatments, lubricants, medical therapeutics, computer memory and chips, electronic devices, medical diagnostic biolabels, and photovoltaic cell components.
 
Microfluidics is a supplier of advanced fluid processing equipment and reaction technology for laboratory, pilot scale and manufacturing applications. The equipment enables the manufacture and formulation of numerous nanomaterials and nanoscale products and produces the most uniform and smallest liquid and suspended solid particles available.
 
Companies seeking to produce difficult-to-formulate products or to find better methods of bio-processing can take advantage of complimentary sample testing at one of three Microfluidics facilities. Visit www.microfluidicscorp.com, email mixinginfo@mfics.com or contact Microfluidics at 800/370.5452 for application information.
You must register or login in order to post comments.

Multimedia

Videos

Image Galleries

American Coating Show 2012

The American Coatings Show and Conference, held every two years, took place May 7-10 at the Indiana Convention Center in Indianapolis, IN, in the heart of the Manufacturing Belt, the oldest and largest concentration of industrial companies in the Midwest.

Podcasts

PCI Top 5 - January 12, 2012
PCI's Podcast series on the five most e-mailed/shared articles and stories for the week.

More Podcasts

THE MAGAZINE

PCI Magazine

PCI may 2012 cover

2012 May

Check out PCI's May issue!!

TABLE OF CONTENTS SUBSCRIBE

iPad

Do you own/use an iPad?
If yes, do you use your iPad for business or personal reasons?
Have you purchased a business app within the last 6 months?
See Poll Results Poll Archive

THE PCI STORE

PCI-June-2011-Coversmall.gif
PCI Additives Handbook

Encyclopedia of information on the properties and uses of coatings additives.

More Products

Clear Seas Research

Clear Seas ResearchWith access to over one million professionals and more than 60 industry-specific publications,Clear Seas Research offers relevant insights from those who know your industry best. Let us customize a market research solution that exceeds your marketing goals.

Virtual Brochures

PageCollageClick on the Virtual Brochures page to view multiple categories that list downloadable product literature from leading industry suppliers.

STAY CONNECTED

Facebook Twitter  LinkedIn YouTube