Painting & Coating Industry (PCI) logo Powder coating summit logo
search
cart
facebook twitter linkedin youtube
  • Sign In
  • Create Account
  • Sign Out
  • My Account
Painting & Coating Industry (PCI) logo Powder coating summit logo
  • NEWS
    • Latest News
    • Market Trends & Reports
    • Finishing News
    • Price Alerts
    • Subscribe to Newsletters
    • Global Top 10/ PCI 25
    • Weekly Featured Article
    • COATLE Word Game
  • PRODUCTS
    • Product News
    • Featured Products
    • Must See Products and Services
  • MATERIALS
    • Additives
    • Resins/Polymers
    • Pigments
    • Equipment
    • Distributors
  • TECHNOLOGIES
    • Adhesives
    • Architectural Coatings
    • Finishing Articles
    • Finishing Technologies
    • Finishing Equipment
    • Industrial Coatings
    • Nanotechnology
    • Powder Coatings
    • Solventborne
    • Special Purpose Coatings
    • Sustainability
    • UV Coatings
    • Waterborne
  • RESOURCES
    • Columns
      • Did you know?
      • Distribution Dive
      • Formulating With Mike
      • Innovation Insights
      • Powder Coating Perspectives
      • TiO2 Insider
    • Blogs
      • Editor's Viewpoint
      • Industry Insights
    • Coatings Supplier Handbook
    • Podcasts and Videos
      • COAT-IT! Podcast
      • Videos/PCI TV
    • PCI Store
    • Classifieds
    • eBooks
    • Sponsor Insights
    • White Papers
    • COATLE Word Game
  • EVENTS
    • Coatings Trends & Technologies Summit
    • Paint and Coatings Academy
    • Webinars
    • Calendar of Events
    • Lifetime Achievement Award
  • DIRECTORIES
    • Buyer's Guide
    • Equipment Directory
    • Materials Directory
  • EMAGAZINE
    • Current Issue
    • eMagazine Archive
    • China Issue Archive
    • Editorial Advisory Board
  • CONTACT
    • Contact Us
    • Advertise
    • Subscribe to eMagazine
    • Subscribe to Newsletters
  • SIGN UP!

New "Eco-Friendly" Universal Corrosion Inhibitors

By Dr. Steve A. Hodges, Dr. Ricard March Raurell, Xavier Llovens
January 1, 2010
Human behavior has caused a great impact on the world; it has taken us time to understand the repercussions and the environmental accidents that have seriously compromised our own future. Chemical weapons, insecticides, fertilizers, industrial effluents, paints and organic solvents have damaged the health of the planet and its inhabitants to the point of contaminating even the most remote places.

In the eighties, due to several environmental scandals, different scientific publications, etc., prompted the need for a new environmentally friendly and transparent chemistry. Conventional coatings contain derived synthetic products from the petrochemical industry that can harm our health and the environment. The danger resides in the heavy metals such as lead, cadmium, mercury, etc., and in VOCs such as xylene, toluene, phenols and formaldehydes, which are emitted by paints and varnishes when applied, or while they dry.

The challenges currently faced by the coatings industry are not just to reduce cost and improve performance but also to fulfill strict legal requirements. In an American technical magazine the technical director of a major national paint company recently reported that his staff spends nearly 40% of its time reformulating their paint in order to meet increasingly stringent VOC regulation. Forty percent of his staff’s time is a lot of time, and is robbing energy and efforts that could be devoted elsewhere, such as toward new developments.

The technical director was expressing a universal phenomenon in the paint industry. Large amounts of manpower are focused on correcting current formulations to new eco-green developments: replacing products containing hexavalent chromium or lead, among other heavy metals, and reducing or eliminating VOCs. This also avoids any undesired labelling that may be associated with toxicity in general.

In terms of corrosion inhibitors, some of the most effective and widely used anticorrosive pigments such as red lead (PbO4), lead silica-chromate (4 (PbCrO4 · PbO) +3 (SiO2 · 4 PbO)), zinc chromate (ZnCrO4), zinc tetraoxychromate (ZnCrO4 · 4 Zn(OH)2), and strontium chromate (SrCrO4), have been and continue to be under heavy scrutiny due to the hazards posed to humans and the environment. Lead compounds are deemed toxic, zinc and strontium chromate are classified as carcinogenic and most recently, according to the EU Directive 004/73/CE, zinc phosphate has been determined to be a danger to the aquatic media.

In general, the latest global trend is to design coatings that comply with the environmental regulations that now exist. These “Eco-Friendly” or “Green” coating systems contain only non-toxic, non-reportable raw materials to ensure no hazard to humans and the environment. The industry has found it very difficult to obtain the same level of performance with the eco-friendly systems as compared to the non-compliant systems.

What is an Eco-Friendly Coating?

Coatings that meet the eco-friendly definition are high- or 100%-solids systems, powder coatings, UV- or EB-curing coatings, low/zero VOC, no heavy metal content, zinc-free or systems that contain no reportable compounds or ingredients in order to meet green label compliant status. Therefore, eco-friendly corrosion inhibitors should not contain heavy metals or non-reportable compounds, and be zinc-free in order to meet the green label compliant standard.

Ever since the use of chromates was restricted, we have been forced to use a variety of different non-toxic corrosion inhibitors specifically designed for a given substrate or resin type in an attempt to match the efficiency and versatility that chrome-based inhibitors offered. But now coatings formulators are demanding today’s non-toxic inhibitors offer as much universal application in a wide range of binders and protective coatings as their toxic counterparts.

What is an Eco-Friendly Corrosion Inhibitor?

Zinc phosphate (Zn3(PO4)2 · X H2O) was the first and most widely used non-toxic inhibitor for replacing lead- and chrome-based inhibitors. Historically, standard zinc phosphate has demonstrated acceptable performance in real outdoor exposure, but less efficiency compared to chromates in marine environments and in accelerated weathering tests such as salt spray and cyclic corrosion (i.e., Prohesion). However its user-friendly, low cost, universal application, and good package stability in a variety of general-purpose industrial and protective coating applications, made zinc phosphate the most popular choice early on for replacing chrome- and lead-based inhibitors

Today, in order to meet the eco-friendly labelling demands, zinc phosphate and modified zinc-containing inhibitors can no longer be used. This has caused yet another dilemma for the inhibitor suppliers, as the current offering of non-zinc inhibitors on the market have generally shown inferior anti-corrosion performance in accelerated corrosion tests, especially on steel substrates, as compared to most zinc-based inhibitors. Also, current zinc-free inhibitors are very limited in their application scope, performing well in some coatings systems and poorly in others.

Our goal was to develop a zinc-free inhibitor that not only met all the environmental demands required for green label compliant coatings but also provided a high level of cost-effective corrosion resistance, exhibited good correlation in accelerated and real-world environments, and offered universal application similar across a wide variety of resin systems and substrates equivalent to its zinc-based counterparts.

Credit: Nubiola USA
Figure 1 Click to enlarge

Development Process for Eco-Friendly Corrosion Inhibitors

First we developed our targeted property list to give direction and scope to our experimental design:
 

  • direct anodic inhibitor;

  • modified metal phosphate complex;

  • universal application – water and solvent systems;

  • improve early (accelerated testing) corrosion resistance;

  • good correlation between accelerated testing and real world environments;

  • good multi-substrate performance;

  • user friendly – easy to incorporate;

  • application in thin-film (< 25µ d.f.t.) systems;
  • good package stability; and

  • greater price stability vs. zinc based inhibitors.

 

We knew this was not going to be an easy task, especially with the limited eco-friendly corrosive inhibitive chemistry available in conjunction with the cost-effective performance targets we set for this product.

Credit: Nubiola USA
Figure 2 Click to enlarge

We determined if we were going to be successful in meeting our development goals we needed to employ a unique combination of chemical and physical properties.

On the chemistry side we evaluated various metal phosphate-based complexes deposited on a variety of inert carriers or core pigments to determine what combinations would provide the best cost-effective, universal application. We also looked at the effect of organic modification on the various inorganic complexes. Standard zinc phosphate and several modified zinc and zinc-free inhibitors were used as controls. The controls and experimental offerings were then initially screened using a combination of surface compositional and structural analysis that included Electro-Impedance Spectroscopy (EIS) (Figure 1), SEM/EDX Mapping (Figures 2,3), XRD, and in-house solution potential techniques to determine which complexes provided the most contribution effect.

Credit: Nubiola USA
Figure 3 Click to enlarge

The respective coating systems were applied to a variety of applicable substrates and to a battery of accelerated corrosion tests that included standard salt spray (ASTM B 117), cyclic QUV/Prohesion testing (ASTM D 5894) (Figure 4), humidity testing and exterior exposure.

Credit: Nubiola USA
Figure 4 Click to enlarge

On the physical property side we chose to use the key characteristics of our top-performing, modified zinc-based inhibitors. We employed a spherical morphology particle shape, a very fine mean particle size (avg. 1.0 µ) and a narrow particle size distribution range that includes a very controlled percentage of nano particles (Figure 5). Our past research shows that this combination of physical properties provides ease of dispersability, excellent thin-film performance, and optimum pigment packing properties that synergistically enhanced the anti-corrosion performance.

Test Results

Credit: Nubiola USA
Figure 5 Click to enlarge

Finally, after screening over 250 experimental offerings and testing over 2,000+ test panels, we found the mixed metal calcium-strontium phosphate complex deposited on a silicate core provided the best overall performance (Appendix, Figure 10-13). We also discovered an organo-modified version of this same complex produced some additional advantages in the area of film formation, adhesion promotion, and substrate wetting (Appendix, Figures 14-18).

The basic formula for these products is shown in Figure 6. Both experimental prototypes, 301 and 302, provided excellent direct anodic inhibition from the combination of the calcium and strontium cations, but also provided good cathodic inhibition due to the basicity/alkalinity of the silica core. Its basic nature reduces the amount of oxygen needed to passivate the formation of rust.
 

Credit: Nubiola USA
Figure 6 Click to enlarge 

The organic surface treatment used in prototype 302 showed improved mechanical properties in terms of better wetting in organic systems without decreasing its performance in waterborne systems, reduced pigment – binder interface, which makes the flow of water and electrolytes through the organic coating difficult and at the same time protects the pigment making it more inert when reactive resins or those with high acid values are used.

Credit: Nubiola USA
Table 1 Click to enlarge

The pigment’s chemical activity is a result of the active chemical substance’s solubility (270 mg/L). Its small particles provide easier solubility due to greater specific surface (Table 1), which is one of the keys to its anti-corrosive effectiveness.

At the same time, the organic surface treatment facilitates the dispersion of active nano-particles within the system. The photographs in Figure 7 show the difference in agglomeration between both pigments.

Credit: Nubiola USA
Figure 7 Click to enlarge

A strong contribution margin was also obtained due to the unique particle morphology and high aspect ratio of the fine, narrow particle size distribution (Figure 8).

Credit: Nubiola USA
Figure 8 Click to enlarge

Good package stability was seen in all systems tested with Prototype 301 and 302. We were especially encouraged with the compatibility of both prototypes in high reactive systems such as acid catalyzed and 2K polyurethanes where it provided good cost-effective performance without affecting the pot-life or cure properties of these systems. Figure 9 shows the good stability in terms of viscosity change over time as compared to the same system containing standard zinc phosphate.

Credit: Nubiola USA
Figure 9 Click to enlarge

Summary

To sum up, based on our project design and extensive validation testing, we found experimental prototypes 301 and 302 to provide the best overall universal anti-corrosion performance of all the zinc-free offerings. These uniquely designed calcium-strontium mixed metal phosphate complexes provided comparable, and in some cases, improved cost-effective performance over standard zinc phosphate and the modified zinc and zinc-free inhibitors they were compared against. The zinc-free chemistry of prototypes 301 and 302 also provided good package stability in a variety of resin systems, including high acid value, acid catalyzed, and 2K urethanes.

Credit: Nubiola USA
Figure 10-13 Click to enlarge

Overall we feel experimental prototypes 301 and 302 meet the performance, cost, and most importantly, the environmental requirements for a universal, eco-friendly, zinc-free inhibitor.

Credit: Nubiola USA
Figure 14-18 Click to enlarge

Appendix

 

Share This Story

Looking for a reprint of this article?
From high-res PDFs to custom plaques, order your copy today!

Nubiola Inorganic Pigments, Nubiola USA, Norcross, GA
Nubiola Inorganic Pigments, Norcross, GA
Nubiola Inorganic Pigments, Barcelona, Spain

Recommended Content

JOIN TODAY
to unlock your recommendations.

Already have an account? Sign In

  • pci1022-Kinaltek-Lead-1170.jpg

    A Novel Pigment Production Technology

    Following an extensive R&D program that demonstrated...
    Paint and Coating Pigments
    By: Jawad Haidar and Nitin Soni
  • pci global top 10

    2025 Global Top 10: Top Paint and Coatings Companies

    The following is PCI’s annual ranking of the top 10...
    Paint and Coating Market Reports
    By: Courtney Bassett
  • 2025 pci 25

    2025 PCI 25: Top Paint and Coatings Companies

    PCI's annual ranking of the top 25 North American paint...
    Global Top 10 and PCI 25
    By: Courtney Bassett
You must login or register in order to post a comment.

Report Abusive Comment

Manage My Account
  • eMagazine
  • Newsletters
  • Online Registration
  • Subscription Customer Service

More Videos

Sponsored Content

Sponsored Content is a special paid section where industry companies provide high quality, objective, non-commercial content around topics of interest to the PCI audience. All Sponsored Content is supplied by the advertising company and any opinions expressed in this article are those of the author and not necessarily reflect the views of PCI or its parent company, BNP Media. Interested in participating in our Sponsored Content section? Contact your local rep!

close
  • wooden kitchen set and shelving
    Sponsored bySirca North America

    Leveraging Coatings to Meet ESG Goals in Manufacturing

  • man woodworking in workshop
    Sponsored byGemini Industries, Inc.

    Waterborne Coatings Aren't the Future -- They're the New Performance Benchmark

Popular Stories

Akzo, SW, Nippon Logos

AkzoNobel Rejects Cash Offer From Nippon Paint, Sherwin-Williams

BASF SE Logo

BASF Announces Strategic Business Sale

AkzoSWNipponEndTalks

Nippon Paint, Sherwin-Williams End AkzoNobel Pursuit

POB-Point-and-Shoot

PCI Buyers Guide

Submit a Request for Proposal (RFP) to suppliers of your choice with details on what you need with a click of a button

Start your RFP

Browse our Buyers Guide for manufacturers and distributors of all types of coatings products and much more!

Find Suppliers

Events

September 4, 2025

N-Butylpyrrolidone (NBP) as a Green Solvent to Replace N-Methylpyrrolidone (NMP) in Industrial Coating Applications

ON DEMAND: EPA published a regulation proposal around N-methylpyrrolidone (NMP) in June 2024 to ban or limit NMP in many applications, such as paints and coatings and their removers. N-butylpyrrolidone (NBP) is a powerful and versatile solvent for a variety of industries looking for alternatives to substance of very high concern (SVHC)-listed solvents.

September 15, 2026

Coatings Trends & Technologies Summit

The Coatings Trends & Technologies (CTT) Summit is an annual conference for both liquid and powder coatings formulators and manufacturers to discuss innovations in coatings technology. This event combines high-quality technical presentations, a resource-rich exhibit hall, and dedicated networking opportunities to connect scientific minds, foster innovation, and cultivate game-changing new ideas!

View All Submit An Event

Poll

Longest-running laboratory experiment

What is the longest-running laboratory experiment?
View Results Poll Archive

Products

Automotive Paints and Coatings, 2nd Edition

Now in its second edition and still the only book of its kind, this is an authoritative treatment of all stages of the coating process.

See More Products
Inside the AI Shift in Coatings - See the article now

Related Articles

  • King Features New Resin Modifiers, Corrosion Inhibitors and Catalysts

    See More
  • Ciba Specialty Chemicals: corrosion inhibitors

    See More
  • Novel Corrosion Inhibitors

    See More

Related Products

See More Products
  • corrosion of linings.jpg

    Corrosion of Linings & Coatings: Cathodic and Inhibitor Protection and Corrosion Monitoring

  • corrosion.jpg

    Corrosion Control Through Organic Coatings 2nd Edition

  • intelligent.jpg

    Intelligent Coatings for Corrosion Control 1st Edition

See More Products
×

Keep the info flowing with our eNewsletters!

Get the latest industry updates tailored your way.

JOIN TODAY!
  • RESOURCES
    • Advertise
    • Contact Us
    • Directories
    • Store
    • Want More
    • Manufacturing Division
  • SIGN UP TODAY
    • Create Account
    • eMagazine
    • Newsletters
    • Customer Service
    • Manage Preferences
  • SERVICES
    • Marketing Services
    • Reprints
    • Market Research
    • List Rental
    • Survey & Sample
  • STAY CONNECTED
    • LinkedIn
    • Facebook
    • Youtube
    • X (Twitter)
  • PRIVACY
    • PRIVACY POLICY
    • TERMS & CONDITIONS
    • DO NOT SELL MY PERSONAL INFORMATION
    • PRIVACY REQUEST
    • ACCESSIBILITY

Copyright ©2026. All Rights Reserved BNP Media, Inc. and BNP Media II, LLC.

Design, CMS, Hosting & Web Development :: ePublishing