Painting & Coating Industry (PCI) logo Powder coating summit logo
search
cart
facebook twitter linkedin youtube
  • Sign In
  • Create Account
  • Sign Out
  • My Account
Painting & Coating Industry (PCI) logo Powder coating summit logo
  • NEWS
    • Latest News
    • Market Trends & Reports
    • Finishing News
    • Price Alerts
    • Subscribe to Newsletters
    • Global Top 10/ PCI 25
    • Weekly Featured Article
    • COATLE Word Game
  • PRODUCTS
    • Product News
    • Featured Products
    • Must See Products and Services
  • MATERIALS
    • Additives
    • Resins/Polymers
    • Pigments
    • Equipment
    • Distributors
  • TECHNOLOGIES
    • Adhesives
    • Architectural Coatings
    • Finishing Articles
    • Finishing Technologies
    • Finishing Equipment
    • Industrial Coatings
    • Nanotechnology
    • Powder Coatings
    • Solventborne
    • Special Purpose Coatings
    • Sustainability
    • UV Coatings
    • Waterborne
  • RESOURCES
    • Columns
      • Did you know?
      • Distribution Dive
      • Formulating With Mike
      • Innovation Insights
      • Powder Coating Perspectives
      • TiO2 Insider
    • Blogs
      • Editor's Viewpoint
      • Industry Insights
    • Coatings Supplier Handbook
    • Podcasts and Videos
      • COAT-IT! Podcast
      • Videos/PCI TV
    • PCI Store
    • Classifieds
    • eBooks
    • Sponsor Insights
    • White Papers
    • COATLE Word Game
  • EVENTS
    • Coatings Trends & Technologies Summit
    • Paint and Coatings Academy
    • Webinars
    • Calendar of Events
    • Lifetime Achievement Award
  • DIRECTORIES
    • Buyer's Guide
    • Equipment Directory
    • Materials Directory
  • EMAGAZINE
    • Current Issue
    • eMagazine Archive
    • China Issue Archive
    • Editorial Advisory Board
  • CONTACT
    • Contact Us
    • Advertise
    • Subscribe to eMagazine
    • Subscribe to Newsletters
  • SIGN UP!
FT Archives

On The Finishing Line

July 1, 2005

Preventing Paint Blisters

We have an old gas catalytic infrared oven that we use for drying air-dry, water-based liquid paint applied to wooden doors. Sometimes we have trouble getting the material to dry enough before we have to stack our parts. We slow the line down to get more time in the oven but then we sometimes get too hot in some areas and the paint blisters. Is there a way to get better control over the oven? Is there a better type of oven that we can use for our operation?

You will probably be able to improve your results by upgrading your oven with new or refurbished catalytic emitters and perhaps adding some zoning.

Gas catalytic emitters rely on a platinum catalyst to oxidize the gas. After a period of years, the catalyst can migrate causing hot spots and cold spots across the face of the emitter. Because these "flameless" emitters do not glow, this problem cannot be detected by the naked eye. You can use a hand held infrared thermometer to take temperature measurements across the face or use a thermal-imaging camera to detect this problem. If you find that your emitters are no longer uniform, you can replace them with new units or have them rebuilt.

Having more than one zone in the direction of travel can make a big difference in fine tuning any process, and this is especially true for drying paint. In the first zone, where the product is at its lowest temperature, you can set your emitters at a high output to quickly ramp up the temperature of the product. The next zone(s) can be set at a lower output to hold the product at the required temperature. If the entire oven is only a single zone, then the ramping occurs all the way through the oven and it is harder to make subtle changes and harder to make it repeatable.

In addition, you may be able to benefit from vertical zoning. With only one zone in the vertical direction, the top of the part can get overheated. By adding vertical zoning, you can add as much heat as needed to the bottom, without overheating the top.

Blistering occurs when the outside surface of the paint forms a dry skin while the inside layer of paint is still too wet. As heat is conducted to the inside layer of paint, the evaporating water or solvent blisters up through the dried skin usually popping and leaving a crater with a pin hole. This commonly occurs when trying to push product through an oven too quickly.

In a convection oven, the air directly heats the outside surface of the paint. The inside layers of the paint are then heated by conduction through the layers of paint. It is the rate of conductive heat transfer through the paint that limits this process. If the air temperature is too high, and the rate of heat transfer to the outside layer of paint greatly exceeds the rate of conductive heat transfer through the paint, then the dry skin forms. In a convection oven, the only solution is to use lower air temperature and a longer dwell time.

As you discovered, even an infrared oven can create blistering, but in an infrared oven, some of the radiant energy heats the surface of the paint, and some of the radiant energy is transmitted deeper into the paint. This means the drying process is not totally dependent on conduction through the paint and therefore not as limited by it. The infrared penetration can help to dry the inner layers before the surface skin forms.

The amount of energy that penetrates through the coating is dependent on the wavelengths emitted and the absorption characteristics of the paint. In general, as the emitter temperature increases, the amount of penetration increases. The lower the emitter temperature gets, the more it behaves like a convection oven. Having a higher temperature ramp zone at the oven entrance can help drive out water from the inside layers faster and sometimes minimize blistering.

In any type of oven, a safe way to address blistering is to slow down the drying process and be more patient. But with a multi-zone infrared oven, you can also experiment with higher temperatures in the first zone to address the problem.

Share This Story

Looking for a reprint of this article?
From high-res PDFs to custom plaques, order your copy today!

Recommended Content

JOIN TODAY
to unlock your recommendations.

Already have an account? Sign In

  • pci1022-Kinaltek-Lead-1170.jpg

    A Novel Pigment Production Technology

    Following an extensive R&D program that demonstrated...
    Paint and Coating Pigments
    By: Jawad Haidar and Nitin Soni
  • pci global top 10

    2025 Global Top 10: Top Paint and Coatings Companies

    The following is PCI’s annual ranking of the top 10...
    Paint and Coating Market Reports
    By: Courtney Bassett
  • 2025 pci 25

    2025 PCI 25: Top Paint and Coatings Companies

    PCI's annual ranking of the top 25 North American paint...
    Global Top 10 and PCI 25
    By: Courtney Bassett
You must login or register in order to post a comment.

Report Abusive Comment

Manage My Account
  • eMagazine
  • Newsletters
  • Online Registration
  • Subscription Customer Service

More Videos

Sponsored Content

Sponsored Content is a special paid section where industry companies provide high quality, objective, non-commercial content around topics of interest to the PCI audience. All Sponsored Content is supplied by the advertising company and any opinions expressed in this article are those of the author and not necessarily reflect the views of PCI or its parent company, BNP Media. Interested in participating in our Sponsored Content section? Contact your local rep!

close
  • wooden kitchen set and shelving
    Sponsored bySirca North America

    Leveraging Coatings to Meet ESG Goals in Manufacturing

  • man woodworking in workshop
    Sponsored byGemini Industries, Inc.

    Waterborne Coatings Aren't the Future -- They're the New Performance Benchmark

Popular Stories

Akzo, SW, Nippon Logos

AkzoNobel Rejects Cash Offer From Nippon Paint, Sherwin-Williams

BASF SE Logo

BASF Announces Strategic Business Sale

AkzoSWNipponEndTalks

Nippon Paint, Sherwin-Williams End AkzoNobel Pursuit

POB-Point-and-Shoot

PCI Buyers Guide

Submit a Request for Proposal (RFP) to suppliers of your choice with details on what you need with a click of a button

Start your RFP

Browse our Buyers Guide for manufacturers and distributors of all types of coatings products and much more!

Find Suppliers

Events

September 4, 2025

N-Butylpyrrolidone (NBP) as a Green Solvent to Replace N-Methylpyrrolidone (NMP) in Industrial Coating Applications

ON DEMAND: EPA published a regulation proposal around N-methylpyrrolidone (NMP) in June 2024 to ban or limit NMP in many applications, such as paints and coatings and their removers. N-butylpyrrolidone (NBP) is a powerful and versatile solvent for a variety of industries looking for alternatives to substance of very high concern (SVHC)-listed solvents.

September 15, 2026

Coatings Trends & Technologies Summit

The Coatings Trends & Technologies (CTT) Summit is an annual conference for both liquid and powder coatings formulators and manufacturers to discuss innovations in coatings technology. This event combines high-quality technical presentations, a resource-rich exhibit hall, and dedicated networking opportunities to connect scientific minds, foster innovation, and cultivate game-changing new ideas!

View All Submit An Event

Poll

Longest-running laboratory experiment

What is the longest-running laboratory experiment?
View Results Poll Archive

Products

Automotive Paints and Coatings, 2nd Edition

Now in its second edition and still the only book of its kind, this is an authoritative treatment of all stages of the coating process.

See More Products
Inside the AI Shift in Coatings - See the article now

Related Articles

  • On the Finishing Line

    See More
  • On The Finishing Line

    See More
  • On the Finishing Line

    See More

Related Products

See More Products
  • durability.jpg

    Increasing the Durability of Paint and Varnish Coatings in Building Products and Construction 1st Edition

  • Kevin-Biller-PC-BOOK.jpg

    Powder Coatings - Foundation for the Novice Formulator (ebook)

See More Products
×

Keep the info flowing with our eNewsletters!

Get the latest industry updates tailored your way.

JOIN TODAY!
  • RESOURCES
    • Advertise
    • Contact Us
    • Directories
    • Store
    • Want More
    • Manufacturing Division
  • SIGN UP TODAY
    • Create Account
    • eMagazine
    • Newsletters
    • Customer Service
    • Manage Preferences
  • SERVICES
    • Marketing Services
    • Reprints
    • Market Research
    • List Rental
    • Survey & Sample
  • STAY CONNECTED
    • LinkedIn
    • Facebook
    • Youtube
    • X (Twitter)
  • PRIVACY
    • PRIVACY POLICY
    • TERMS & CONDITIONS
    • DO NOT SELL MY PERSONAL INFORMATION
    • PRIVACY REQUEST
    • ACCESSIBILITY

Copyright ©2026. All Rights Reserved BNP Media, Inc. and BNP Media II, LLC.

Design, CMS, Hosting & Web Development :: ePublishing