Company News / Breaking News

Perstorp to Increase Capacity in China

PERSTORP, Sweden – Perstorp plans to increase its production of aliphatic polyisocyanates in response to growing market demand in Asia, particularly China.

The company will commence implementation of a new production structure in China in 2012. At maturity, this production capacity should reach 12,000 tons per annum. Perstorp also plans to debottleneck existing plants to support growth outside Asia.

Perstorp produces solvent-based Tolonate® and self-emulsifiable-into-water Easaqua™ aliphatic polyisocyanates for high-performance polyurethane coatings. With an average expected annual growth rate of six percent, aliphatic isocyanates specialty materials represent a highly attractive market.

You must register or login in order to post comments.

Multimedia

Videos

Image Galleries

American Coating Show 2012

The American Coatings Show and Conference, held every two years, took place May 7-10 at the Indiana Convention Center in Indianapolis, IN, in the heart of the Manufacturing Belt, the oldest and largest concentration of industrial companies in the Midwest.

Podcasts

PCI Top 5 - January 12, 2012
PCI's Podcast series on the five most e-mailed/shared articles and stories for the week.

More Podcasts

THE MAGAZINE

PCI Magazine

PCI may 2012 cover

2012 May

Check out PCI's May issue!!

TABLE OF CONTENTS SUBSCRIBE

iPad

Do you own/use an iPad?
If yes, do you use your iPad for business or personal reasons?
Have you purchased a business app within the last 6 months?
See Poll Results Poll Archive

THE PCI STORE

PCI-June-2011-Coversmall.gif
PCI Additives Handbook

Encyclopedia of information on the properties and uses of coatings additives.

More Products

Clear Seas Research

Clear Seas ResearchWith access to over one million professionals and more than 60 industry-specific publications,Clear Seas Research offers relevant insights from those who know your industry best. Let us customize a market research solution that exceeds your marketing goals.

Virtual Brochures

PageCollageClick on the Virtual Brochures page to view multiple categories that list downloadable product literature from leading industry suppliers.

STAY CONNECTED

Facebook Twitter  LinkedIn YouTube