Painting & Coating Industry (PCI) logo Powder coating summit logo
search
cart
facebook twitter linkedin youtube
  • Sign In
  • Create Account
  • Sign Out
  • My Account
Painting & Coating Industry (PCI) logo Powder coating summit logo
  • NEWS
    • Latest News
    • Market Trends & Reports
    • Finishing News
    • Price Alerts
    • Subscribe to Newsletters
    • Global Top 10/ PCI 25
    • Weekly Featured Article
    • COATLE Word Game
  • PRODUCTS
    • Product News
    • Featured Products
    • Must See Products and Services
  • MATERIALS
    • Additives
    • Resins/Polymers
    • Pigments
    • Equipment
    • Distributors
  • TECHNOLOGIES
    • Adhesives
    • Architectural Coatings
    • Finishing Articles
    • Finishing Technologies
    • Finishing Equipment
    • Industrial Coatings
    • Nanotechnology
    • Powder Coatings
    • Solventborne
    • Special Purpose Coatings
    • Sustainability
    • UV Coatings
    • Waterborne
  • RESOURCES
    • Columns
      • Did you know?
      • Distribution Dive
      • Formulating With Mike
      • Innovation Insights
      • Powder Coating Perspectives
      • TiO2 Insider
    • Blogs
      • Editor's Viewpoint
      • Industry Insights
    • Coatings Supplier Handbook
    • Podcasts and Videos
      • COAT-IT! Podcast
      • Videos/PCI TV
    • PCI Store
    • Classifieds
    • eBooks
    • Sponsor Insights
    • White Papers
    • COATLE Word Game
  • EVENTS
    • Coatings Trends & Technologies Summit
    • Paint and Coatings Academy
    • Webinars
    • Calendar of Events
    • Lifetime Achievement Award
  • DIRECTORIES
    • Buyer's Guide
    • Equipment Directory
    • Materials Directory
  • EMAGAZINE
    • Current Issue
    • eMagazine Archive
    • China Issue Archive
    • Editorial Advisory Board
  • CONTACT
    • Contact Us
    • Advertise
    • Subscribe to eMagazine
    • Subscribe to Newsletters
  • SIGN UP!
FT Archives

POWDERCOATING

By Chris Merritt
October 15, 2003
POWDERCOATING

Chris Merritt



Choosing a Powder Booth

I am about to buy a powder booth and I have three quotes with different prices. My boss wants me to buy the least expensive one, but I know that there is more to picking a booth than just price. What are some other factors that affect the value of the different quotes?

This is a difficult question to answer without understanding the goals that you want to achieve with your new booth. However, the fundamentals for evaluation of the proposals are always the same. By starting with a spread sheet, you can look at the various attributes for each of the designs and compare them directly. For a booth evaluation, there are several areas that will affect the performance and value. These include: opening sizes (Are they all the same?); layout (proximity to one another); recovery type (cyclone recovery technology requires higher static pressure performance and horsepower from the fan vs. cartridge recovery technology); recovery volume (When comparing the volume of the system, you need to be sure that when you compare the booths the openings used are consistent square footage from booth to booth. If you divide the cfm capability of the recovery by the square footage, the recovery should be able to produce a minimum of 120 lfpm, or higher, across all of the booth openings, depending on the application); the type, quantity and performance of the filtration system; fan design (belt or direct drive); noise level (typically measured within 3 feet of the unit); construction (stainless steel, engineered plastic, fiberglass, etc., will affect the cost of construction); lighting level (Are lights included, room lighting, side mounted?); controls (What comes standard with the booth, such as reclaim control, level control, triggering, etc?)

These are just a few of the main variables. In most cases, the booth supplier will be happy to provide a breakdown of what exactly they are providing for your evaluation.



Lighting Considerations

We need to add more lighting to our powder booth and application area. What codes or other issues should we consider in the selection and installation of light fixtures in and around the powder booth?

As far as the application area is concerned, the lights that are provided need to be dust-tight fixtures. If it is an environmental room and you put the lights into the ceiling, keeping them flush mount will help with both appearance and cleanliness. If the lights will be suspended, be sure that they are stable and located at least three feet beyond any of the booth openings. If you plan to add lights to the booth cabin, they will usually be placed near the operator openings. Any lights that are placed within three feet of a booth opening must be Class II, Division II, approved light fixtures. As always, when installing light fixtures, be sure to pay attention to how you will be able to access them for service or replacement bulbs.



Three-Minute Color Changes?

We have heard rumors of companies that are able to change colors in a powder system in less than three minutes. Is this true, and how do they do it?

There are a variety of ways to change color quickly with powder. In the case of larger systems utilizing automatic guns, roll on/off configurations with multiple booths are often the best solution. Some of the designs that have been brought in from Europe more recently can provide quick reclaim-to-reclaim times. However, they are typically in the five- to 10-minute range, depending on how dramatic the color change is (red to white or white to black typically take a little longer).

For some customers, the solution can be as simple as not reclaiming the oversprayed material. This can dramatically reduce color change time by limiting the amount of equipment that must be exchanged or cleaned. Spray-to-waste color-change times can easily range from one to five minutes. The ultimate solution comes with combining power-and-free conveyor arrangements where booths may be set up for color ranges (reduces cleaning and set-up time) and the product may then be directed through the use of gates or switches to the appropriate booth. This is still the quickest scenario when full reclaim capability is required.

Share This Story

Looking for a reprint of this article?
From high-res PDFs to custom plaques, order your copy today!

Director Systems

ITW Gema

Recommended Content

JOIN TODAY
to unlock your recommendations.

Already have an account? Sign In

  • pci1022-Kinaltek-Lead-1170.jpg

    A Novel Pigment Production Technology

    Following an extensive R&D program that demonstrated...
    Paint and Coating Pigments
    By: Jawad Haidar and Nitin Soni
  • pci global top 10

    2025 Global Top 10: Top Paint and Coatings Companies

    The following is PCI’s annual ranking of the top 10...
    Global Top 10 and PCI 25
    By: Courtney Bassett
  • 2025 pci 25

    2025 PCI 25: Top Paint and Coatings Companies

    PCI's annual ranking of the top 25 North American paint...
    Paint and Coating Market Reports
    By: Courtney Bassett
You must login or register in order to post a comment.

Report Abusive Comment

Manage My Account
  • eMagazine
  • Newsletters
  • Online Registration
  • Subscription Customer Service

More Videos

Sponsored Content

Sponsored Content is a special paid section where industry companies provide high quality, objective, non-commercial content around topics of interest to the PCI audience. All Sponsored Content is supplied by the advertising company and any opinions expressed in this article are those of the author and not necessarily reflect the views of PCI or its parent company, BNP Media. Interested in participating in our Sponsored Content section? Contact your local rep!

close
  • wooden kitchen set and shelving
    Sponsored bySirca North America

    Leveraging Coatings to Meet ESG Goals in Manufacturing

  • man woodworking in workshop
    Sponsored byGemini Industries, Inc.

    Waterborne Coatings Aren't the Future -- They're the New Performance Benchmark

Popular Stories

Akzo, SW, Nippon Logos

AkzoNobel Rejects Cash Offer From Nippon Paint, Sherwin-Williams

BASF SE Logo

BASF Announces Strategic Business Sale

AkzoSWNipponEndTalks

Nippon Paint, Sherwin-Williams End AkzoNobel Pursuit

POB-Point-and-Shoot

PCI Buyers Guide

Submit a Request for Proposal (RFP) to suppliers of your choice with details on what you need with a click of a button

Start your RFP

Browse our Buyers Guide for manufacturers and distributors of all types of coatings products and much more!

Find Suppliers

Events

September 4, 2025

N-Butylpyrrolidone (NBP) as a Green Solvent to Replace N-Methylpyrrolidone (NMP) in Industrial Coating Applications

ON DEMAND: EPA published a regulation proposal around N-methylpyrrolidone (NMP) in June 2024 to ban or limit NMP in many applications, such as paints and coatings and their removers. N-butylpyrrolidone (NBP) is a powerful and versatile solvent for a variety of industries looking for alternatives to substance of very high concern (SVHC)-listed solvents.

September 15, 2026

Coatings Trends & Technologies Summit

The Coatings Trends & Technologies (CTT) Summit is an annual conference for both liquid and powder coatings formulators and manufacturers to discuss innovations in coatings technology. This event combines high-quality technical presentations, a resource-rich exhibit hall, and dedicated networking opportunities to connect scientific minds, foster innovation, and cultivate game-changing new ideas!

View All Submit An Event

Poll

Longest-running laboratory experiment

What is the longest-running laboratory experiment?
View Results Poll Archive

Products

Automotive Paints and Coatings, 2nd Edition

Now in its second edition and still the only book of its kind, this is an authoritative treatment of all stages of the coating process.

See More Products
Inside the AI Shift in Coatings - See the article now

Related Articles

  • POWDERCOATING

    See More
  • Roobol to Retire from NR Consultants - Posted 12/5/07

    See More
  • Roobol On Painting

    See More
×

Keep the info flowing with our eNewsletters!

Get the latest industry updates tailored your way.

JOIN TODAY!
  • RESOURCES
    • Advertise
    • Contact Us
    • Directories
    • Store
    • Want More
    • Manufacturing Division
  • SIGN UP TODAY
    • Create Account
    • eMagazine
    • Newsletters
    • Customer Service
    • Manage Preferences
  • SERVICES
    • Marketing Services
    • Reprints
    • Market Research
    • List Rental
    • Survey & Sample
  • STAY CONNECTED
    • LinkedIn
    • Facebook
    • Youtube
    • X (Twitter)
  • PRIVACY
    • PRIVACY POLICY
    • TERMS & CONDITIONS
    • DO NOT SELL MY PERSONAL INFORMATION
    • PRIVACY REQUEST
    • ACCESSIBILITY

Copyright ©2026. All Rights Reserved BNP Media, Inc. and BNP Media II, LLC.

Design, CMS, Hosting & Web Development :: ePublishing