PITTSBURGH – PPG Industries is planning to build its first manufacturing plant in Russia. The company has signed an investment agreement with the administration of the Kaluga Region, Russia, to build an automotive coatings and industrial coatings plant about 70 kilometers southwest of Moscow.
 
The plant will manufacture coatings for automotive and other industrial customers. The facility, which will be fully owned by PPG, will employ about 70 people and be located just north of the city of Kaluga in the Vorsino Industrial Park, according to Bill Wulfsohn, PPG Senior Vice President, Coatings.
 
"The Russian economy is booming and automotive production is growing quickly. To best serve the market, we must have local manufacturing capabilities," Wulfsohn said. Currently, seven new automotive assembly plants are in the planning or construction phase in Russia and are expected to come online within the next three years.
You must register or login in order to post comments.

Multimedia

Videos

Image Galleries

American Coating Show 2012

The American Coatings Show and Conference, held every two years, took place May 7-10 at the Indiana Convention Center in Indianapolis, IN, in the heart of the Manufacturing Belt, the oldest and largest concentration of industrial companies in the Midwest.

Podcasts

PCI Top 5 - January 12, 2012
PCI's Podcast series on the five most e-mailed/shared articles and stories for the week.

More Podcasts

THE MAGAZINE

PCI Magazine

PCI may 2012 cover

2012 May

Check out PCI's May issue!!

TABLE OF CONTENTS SUBSCRIBE

iPad

Do you own/use an iPad?
If yes, do you use your iPad for business or personal reasons?
Have you purchased a business app within the last 6 months?
See Poll Results Poll Archive

THE PCI STORE

PCI-June-2011-Coversmall.gif
PCI Additives Handbook

Encyclopedia of information on the properties and uses of coatings additives.

More Products

Clear Seas Research

Clear Seas ResearchWith access to over one million professionals and more than 60 industry-specific publications,Clear Seas Research offers relevant insights from those who know your industry best. Let us customize a market research solution that exceeds your marketing goals.

Virtual Brochures

PageCollageClick on the Virtual Brochures page to view multiple categories that list downloadable product literature from leading industry suppliers.

STAY CONNECTED

Facebook Twitter  LinkedIn YouTube