Painting & Coating Industry (PCI) logo Powder coating summit logo
search
cart
facebook twitter linkedin youtube
  • Sign In
  • Create Account
  • Sign Out
  • My Account
Painting & Coating Industry (PCI) logo Powder coating summit logo
  • NEWS
    • Latest News
    • Market Trends & Reports
    • Finishing News
    • Price Alerts
    • Subscribe to Newsletters
    • Global Top 10/ PCI 25
    • Weekly Featured Article
    • COATLE Word Game
  • PRODUCTS
    • Product News
    • Featured Products
    • Must See Products and Services
  • MATERIALS
    • Additives
    • Resins/Polymers
    • Pigments
    • Equipment
    • Distributors
  • TECHNOLOGIES
    • Adhesives
    • Architectural Coatings
    • Finishing Articles
    • Finishing Technologies
    • Finishing Equipment
    • Industrial Coatings
    • Nanotechnology
    • Powder Coatings
    • Solventborne
    • Special Purpose Coatings
    • Sustainability
    • UV Coatings
    • Waterborne
  • RESOURCES
    • Columns
      • Did you know?
      • Distribution Dive
      • Formulating With Mike
      • Innovation Insights
      • Powder Coating Perspectives
      • TiO2 Insider
    • Blogs
      • Editor's Viewpoint
      • Industry Insights
    • Coatings Supplier Handbook
    • Podcasts and Videos
      • COAT-IT! Podcast
      • Videos/PCI TV
    • PCI Store
    • Classifieds
    • eBooks
    • Sponsor Insights
    • White Papers
    • COATLE Word Game
  • EVENTS
    • Coatings Trends & Technologies Summit
    • Paint and Coatings Academy
    • Webinars
    • Calendar of Events
    • Lifetime Achievement Award
  • DIRECTORIES
    • Buyer's Guide
    • Equipment Directory
    • Materials Directory
  • EMAGAZINE
    • Current Issue
    • eMagazine Archive
    • China Issue Archive
    • Editorial Advisory Board
  • CONTACT
    • Contact Us
    • Advertise
    • Subscribe to eMagazine
    • Subscribe to Newsletters
  • SIGN UP!

Prince Minerals Adds "Brick Belt" Capacity for High-Quality Colorant

April 1, 2009


Prince Minerals, Inc. is a leading producer of specialty mineral products with emphasis on naturally occurring minerals and pigment applications. Its products are used in bricks, refractories, glass, ceramics, foundries, cement and other applications. The company operates six processing plants, including the newest, a 40,000 sq. ft. facility in Monroe, NC, which is also home to an extensive R&D lab and Technical Service Center. The North Carolina location, which began production in March, 2008, was chosen for its close proximity to the company’s growing “Brick Belt” customer base, which spans the Carolinas and Georgia.

Two main production “circuits” comprise the Monroe facility. A dedicated line for the manufacture of proprietary “through-the-body” pigment blends for the clay brick and colored mortar industries produces in bulk at a rate of 10 to 15 tons per shift. Colorant is stored in silos.

A second, commercial line, produces specialized dry-mix surface colorants for the structural clay brick and tile industries. For the design and manufacture of this larger line, Prince Minerals worked with Ingredient Masters, Cincinnati, OH. The firm specializes in precision batching systems and has extensive credentials in the brick (Redland Brick), ceramic (Oceanside Glasstile) refractories (Uni-Ref, Spar Refractories, Zedmark) and colorant (Englehard) industries.

Jon Attridge was Construction Facility Manager, and led the team that developed the requirements for the line. He brought to the project an unusual cache of qualifications. Explains Attridge, “I’m an R&D guy, a ceramic engineer whose focus is colorant development.”  For the 10 years Attridge has been with Prince Minerals, his area of specialty has been colorants for the brick industry.

Attridge’s family’s business, however, is mechanical contracting, and he has a background in that discipline as well. “Developing the line was the perfect challenge for me,” he says, “knowing I’d be senior at this plant, with a vested interest in its success both operationally, and financially.”

The goal for the commercial circuit, according to Attridge, was to build “a flexible batching line that would produce consistently high-quality product, with virtually zero rework. We also wanted to optimize the ergonomics of the operation by eliminating manual tasks, such as bag cutting, and have the cleanest possible work environment, by preventing material from becoming airborne when dispensed. Finally, we looked for a system concept that was industrial, rather than food grade or something else,” adds Attridge, “and a supplier with an understanding of the industrial environment.”

After substantial research and consideration of the approaches of several manufacturers of batching systems, Prince Minerals chose the system concept recommended by Ingredient Masters.

The heart of this system is a sequence of 54 cu. ft. polyethylene dispensers, each with a bulk bag lifting frame. The dispensers are arranged in facing rows of a dozen each and have a common support structure and dust pickup system.

Each dispenser holds a single ingredient and is modular in that it can be easily removed from the line. Bulk bags – “Super Sacks” – of raw material are suspended above the bins at a 12’ elevation.

Beneath the bins, an operator-driven, motorized scale cart moves on a track. Ingredients, target weight and tote locations applicable to the selected recipe are entered into a program. The cart then moves down the track and the correct proportions of each ingredient are released through a valve into the cart’s hopper. Materials can also be added from Super Sacks, or in bulk from an outside silo. Batch accuracy is +.2 lbs.

When the batch is complete, the hopper is retrieved by a forklift and emptied into a mixer. After blending and testing, finished product is conveyed pneumatically to one of the storage silos, then to the bagging facility. Fifty percent of the finished product is packaged into 50-lb. bags; the rest in bulk bags of 1000 to 2000 lbs. “We get precise weights into the Super Sacks just by hitting a button and spec’ing the weight,” says Attridge, “but that’s not the end of the story. There’s still a 24-hour quality control process before batches can be shipped.”

Explains Attridge, “a master standard has been established for each color blend. Finished products are tested for fired color that follows customer firing parameters. Incoming raw materials are subject to quality protocols we developed. In either case, a sample is taken from each batch and tagged for firing and rheological tests. Samples are suspended in water, applied to test substrates or tiles, and fired at 1900 to 2000 oF. The next morning, they’re read with a spectrophotometer, which gauges color against the standard.

“If approved,” he continues, “that batch is OK’d for shipment. If alterations are required, material is returned to the mixer, adjusted for color and rheology, re-sampled and tested again.”

The system engineered for Prince Minerals is a lean, manual system that offers exceptional flexibility and the ability to automate or expand as needs evolve. Says Ingredient Masters President and Owner Scott Culshaw, “Prince Minerals has a commitment to supply a pre-qualified, pre-checked product. They needed to know when it’s shipped to a customer and fired as designed, it will be accurate to the standard.”

Another advantage of this equipment, according to Culshaw, is that Prince Minerals’ customers “have no need to maintain inventory, but rather just a dozen or so preblended formulas.”

In addition to the primary production line, Ingredient Masters also supplied equipment for a third line, similar in design, that incorporates three feed hoppers, mounted above a 200 cu. ft. mixer.

Contact information: sales@ingredientmasters.com or Scott Culshaw, Ingredient Masters  513/231.7432.

Share This Story

Looking for a reprint of this article?
From high-res PDFs to custom plaques, order your copy today!

Recommended Content

JOIN TODAY
to unlock your recommendations.

Already have an account? Sign In

  • pci1022-Kinaltek-Lead-1170.jpg

    A Novel Pigment Production Technology

    Following an extensive R&D program that demonstrated...
    Paint and Coating Pigments
    By: Jawad Haidar and Nitin Soni
  • pci global top 10

    2025 Global Top 10: Top Paint and Coatings Companies

    The following is PCI’s annual ranking of the top 10...
    Global Top 10 and PCI 25
    By: Courtney Bassett
  • 2025 pci 25

    2025 PCI 25: Top Paint and Coatings Companies

    PCI's annual ranking of the top 25 North American paint...
    Paint and Coating Market Reports
    By: Courtney Bassett
You must login or register in order to post a comment.

Report Abusive Comment

Manage My Account
  • eMagazine
  • Newsletters
  • Online Registration
  • Subscription Customer Service

More Videos

Sponsored Content

Sponsored Content is a special paid section where industry companies provide high quality, objective, non-commercial content around topics of interest to the PCI audience. All Sponsored Content is supplied by the advertising company and any opinions expressed in this article are those of the author and not necessarily reflect the views of PCI or its parent company, BNP Media. Interested in participating in our Sponsored Content section? Contact your local rep!

close
  • wooden kitchen set and shelving
    Sponsored bySirca North America

    Leveraging Coatings to Meet ESG Goals in Manufacturing

  • man woodworking in workshop
    Sponsored byGemini Industries, Inc.

    Waterborne Coatings Aren't the Future -- They're the New Performance Benchmark

Popular Stories

Akzo, SW, Nippon Logos

AkzoNobel Rejects Cash Offer From Nippon Paint, Sherwin-Williams

BASF SE Logo

BASF Announces Strategic Business Sale

AkzoSWNipponEndTalks

Nippon Paint, Sherwin-Williams End AkzoNobel Pursuit

POB-Point-and-Shoot

PCI Buyers Guide

Submit a Request for Proposal (RFP) to suppliers of your choice with details on what you need with a click of a button

Start your RFP

Browse our Buyers Guide for manufacturers and distributors of all types of coatings products and much more!

Find Suppliers

Events

September 4, 2025

N-Butylpyrrolidone (NBP) as a Green Solvent to Replace N-Methylpyrrolidone (NMP) in Industrial Coating Applications

ON DEMAND: EPA published a regulation proposal around N-methylpyrrolidone (NMP) in June 2024 to ban or limit NMP in many applications, such as paints and coatings and their removers. N-butylpyrrolidone (NBP) is a powerful and versatile solvent for a variety of industries looking for alternatives to substance of very high concern (SVHC)-listed solvents.

September 15, 2026

Coatings Trends & Technologies Summit

The Coatings Trends & Technologies (CTT) Summit is an annual conference for both liquid and powder coatings formulators and manufacturers to discuss innovations in coatings technology. This event combines high-quality technical presentations, a resource-rich exhibit hall, and dedicated networking opportunities to connect scientific minds, foster innovation, and cultivate game-changing new ideas!

View All Submit An Event

Poll

Longest-running laboratory experiment

What is the longest-running laboratory experiment?
View Results Poll Archive

Products

Automotive Paints and Coatings, 2nd Edition

Now in its second edition and still the only book of its kind, this is an authoritative treatment of all stages of the coating process.

See More Products
Inside the AI Shift in Coatings - See the article now

Related Articles

  • ROSS High-Shear Mixer for High Quality Dispersions and Emulsions.jpg

    ROSS High-Shear Mixer for High Quality Dispersions and Emulsions

    See More
  • Clever Adhesives for High-Quality Woods

    See More
  • Evonik Launches New Leveling Agent for High-Quality Automotive Clear Coatings.jpg

    Evonik Launches New Leveling Agent for High-Quality Automotive Clear Coatings

    See More

Related Products

See More Products
  • Kevin-Biller-PC-BOOK.jpg

    Powder Coatings - Foundation for the Novice Formulator (ebook)

See More Products
×

Keep the info flowing with our eNewsletters!

Get the latest industry updates tailored your way.

JOIN TODAY!
  • RESOURCES
    • Advertise
    • Contact Us
    • Directories
    • Store
    • Want More
    • Manufacturing Division
  • SIGN UP TODAY
    • Create Account
    • eMagazine
    • Newsletters
    • Customer Service
    • Manage Preferences
  • SERVICES
    • Marketing Services
    • Reprints
    • Market Research
    • List Rental
    • Survey & Sample
  • STAY CONNECTED
    • LinkedIn
    • Facebook
    • Youtube
    • X (Twitter)
  • PRIVACY
    • PRIVACY POLICY
    • TERMS & CONDITIONS
    • DO NOT SELL MY PERSONAL INFORMATION
    • PRIVACY REQUEST
    • ACCESSIBILITY

Copyright ©2026. All Rights Reserved BNP Media, Inc. and BNP Media II, LLC.

Design, CMS, Hosting & Web Development :: ePublishing