Painting & Coating Industry (PCI) logo Powder coating summit logo
search
cart
facebook twitter linkedin youtube
  • Sign In
  • Create Account
  • Sign Out
  • My Account
Painting & Coating Industry (PCI) logo Powder coating summit logo
  • NEWS
    • Latest News
    • Market Trends & Reports
    • Finishing News
    • Price Alerts
    • Subscribe to Newsletters
    • Global Top 10/ PCI 25
    • Weekly Featured Article
    • COATLE Word Game
  • PRODUCTS
    • Product News
    • Featured Products
    • Must See Products and Services
  • MATERIALS
    • Additives
    • Resins/Polymers
    • Pigments
    • Equipment
    • Distributors
  • TECHNOLOGIES
    • Adhesives
    • Architectural Coatings
    • Finishing Articles
    • Finishing Technologies
    • Finishing Equipment
    • Industrial Coatings
    • Nanotechnology
    • Powder Coatings
    • Solventborne
    • Special Purpose Coatings
    • Sustainability
    • UV Coatings
    • Waterborne
  • RESOURCES
    • Columns
      • Did you know?
      • Distribution Dive
      • Formulating With Mike
      • Innovation Insights
      • Powder Coating Perspectives
      • TiO2 Insider
    • Blogs
      • Editor's Viewpoint
      • Industry Insights
    • Coatings Supplier Handbook
    • Podcasts and Videos
      • COAT-IT! Podcast
      • Videos/PCI TV
    • PCI Store
    • Classifieds
    • eBooks
    • Sponsor Insights
    • White Papers
    • COATLE Word Game
  • EVENTS
    • Coatings Trends & Technologies Summit
    • Paint and Coatings Academy
    • Webinars
    • Calendar of Events
    • Lifetime Achievement Award
  • DIRECTORIES
    • Buyer's Guide
    • Equipment Directory
    • Materials Directory
  • EMAGAZINE
    • Current Issue
    • eMagazine Archive
    • China Issue Archive
    • Editorial Advisory Board
  • CONTACT
    • Contact Us
    • Advertise
    • Subscribe to eMagazine
    • Subscribe to Newsletters
  • SIGN UP!

Relief for Companies Caught in the Benzene Lawsuit Onslaught

By Kenneth Anspach
November 1, 2007

“The business of America is business.” So said President Calvin Coolidge on January 17, 1925, to the Society of American Newspaper Editors. Indeed, industry has been the backbone of the U.S. economy, growing over 50 percent during the period from the Second World War until 1992, alone.2 Yet, between 1992 and 2002, the number of the nation’s industrial establishments dwindled by seven percent.3 In 1960, the U.S. exported goods valued at more than $3.5 billion than it imported.4 By 2006, the U.S. was importing $765 billion more than it exported and had amassed a trade deficit of $1.46 trillion, the largest of any country.5 Yet, although the number of industrial establishments has declined, the number of lawyers has risen over 30 percent!6 And these lawyers aren’t just sitting on their hands. Many lawyers in the field of personal injury are filing what are known as toxic tort lawsuits against American industry. The typical toxic tort suit alleges injury from exposure to a product containing a hazardous substance. Currently a plethora of such lawsuits alleging benzene exposure has so traumatized American companies that they often are failing to take advantage of the insurance protection that they previously purchased. However, certain attorneys who specialize in representing policyholders can provide these businesses the protection to which they are entitled.

Toxic Tort Impact

Asbestos lawsuits provide a case study of the impact of toxic tort litigation on U.S. industry. Most people are under the impression that the asbestos lawsuits that clogged U.S. courts and caused numerous corporate bankruptcies in the 1980s are a thing of the past. Yet, according to the Wall Street Journal, “desperately ill plaintiffs have been eclipsed by a huge and growing number of relatively healthy people seeking awards for possible future illnesses.”7 Since January 2000, personal injury lawyers representing these individuals have “pushed at least 20 companies that sold or used asbestos products into bankruptcy protection…on top of 40 other asbestos-related corporate bankruptcies since the mid-seventies.”8 Now, “the sickest asbestos victims are…collecting far less than comparable victims did in the 1990s.”9

Benzene Litigation

And while industry laments the advent of these “greedy [asbestos] lawsuits [that] dishonor the legitimately injured…and take limited restitution money away from the truly deserving workers and their families,”10 the new “soup de jour” of the plaintiffs’ bar is so-called benzene litigation. Individuals suffering from acute myelogeneous leukemia (AML) and other leukemia diseases are claiming that they were exposed to benzene-containing products at their places of work, thereby resulting in these serious and often fatal medical conditions. Benzene is present in crude oil, and is a component of gasoline fuels, typically less than 3%.11 Benzene is classified as a Group 1 human carcinogen by the International Agency for Research on Cancer, and there is general agreement that benzene can cause leukemia in highly exposed individuals.12 About 11,930 new cases of AML are diagnosed each year in the United States.13 AML results from acquired genetic damage to the DNA of developing cells in the bone marrow.14 The effects are the uncontrolled, exaggerated growth and accumulation of cells called “leukemic blasts” which fail to function as normal blood cells, and the blockade of the production of normal marrow cells, leading to a deficiency of red cells and platelets and normal white cells in the blood.15

While workplace exposure to benzene is a recognized cause of AML,16 many of these so-called benzene exposure cases do not involve benzene at all. Rather, while the lawsuits’ allegations claim benzene exposure, the defendants being sued often never manufactured products known to contain benzene. Rather, their products may contain xylene, toluene, paint thinner, kerosene and similar chemicals that may contain trace amounts of benzene, sometimes resulting from the fractional distillation process used at oil refineries.17 The amounts of benzene in these products are denominated as “trace” because they are present, if at all, in concentrations of less than 0.1 percent, and are not listed as an ingredient on applicable material data safety sheets.18 In contrast to benzene, “there is no direct epidemiological evidence concerning the carcinogenicity of toluene and xylenes, and only limited evidence from animal studies.”19 It is accepted that epidemiological studies are the most informative in evaluating a purported causal link between a chemical agent and a particular disease.20 Yet, even in the absence of such causal links, many companies that safely made products containing toluene and xylenes are being caught in a tangled web of such lawsuits. In the legal vernacular, these suits are known as “trace benzene” cases.21

Once a particular company’s name appears on a list of defendants in one such case, it is a virtual certainty that its name will be included by plaintiffs’ lawyers in dozens of unrelated cases. These claims are being filed in assembly-line fashion by law firms seemingly hell-bent on squeezing the last buck from American industries already reeling from skyrocketing raw materials and transportation costs resulting from the run-up in petroleum prices, pressures from low-wage, low-price competition from overseas markets, and price ceilings imposed by global cut-rate retailers. This feeding frenzy on the carcass of U.S. manufacturing has led to a new American growth industry: a recent Web search of the term “benzene personal injury lawyers” yielded a staggering 427,000 hits! 

Ironically, benzene barratry has seemingly replaced manufacturing as America’s business. Are there really enough benzene exposure cases to justify all this interest from personal injury lawyers? Given the advent of the “trace benzene” case, every Tom, Dick or Harry who ever wielded a paintbrush has now become fodder for the benzene plaintiffs’ bar. This phenomenon led one industry executive recently served with such a suit to refer to the experience as a “corporate stick-up.”

Insurance Coverage

Many such corporate executives caught in the grip of this tidal wave of lawsuits do not realize that they need not face this onslaught alone. Businesses facing these new types of suits will likely have insurance designed to cover their losses. Trace benzene and other toxic tort suits involve products to which exposure is alleged to have occurred over the entire working career of the plaintiff, i.e., a period of decades. Companies who manufactured such products over that time period are very likely to have purchased comprehensive general liability insurance covering such liabilities. Given that the occurrences alleged in these lawsuits arose from exposure throughout such extended time period, the insurance that the companies purchased during this period remains viable to cover them now.

This principle was established by such groundbreaking cases as Zurich Insurance Company v. Raymark Industries, Inc., 118 Ill.2d 23 (1987), where the Illinois Supreme Court held that insurance coverage is triggered both at the time of the alleged exposure to the hazardous substance as well as at the time of manifestation of the sickness or disease. Yet, despite that the existence of such coverage is widely known in the legal community, its availability to deal with the spate of recent toxic tort suits such as those of the trace benzene ilk is, surprisingly, not yet widely known. For example, a recent spot search of benzene cases filed in Madison County, IL, resulted in finding that many of the defendants in these suits were not represented and had never filed appearances. Had these parties filed claims with their liability insurance carriers, the carriers would have been obliged to defend and indemnify them. In other words, the parties would have had the cost of their defense covered and any judgments or settlements paid by the insurers. The insurers must honor this contractual duty to defend and indemnify even if the lawsuit is frivolous, which is often the situation in the trace benzene cases.

Given that these companies paid the premiums for their insurance coverage, why are they not contacting their insurers? Often, the companies simply do not know and have not been advised that insurance purchased many years ago is still viable and applicable today. They do not consider that policies literally gathering dust in a backroom filing cabinet may be worth hundreds of thousands or even millions of dollars in defense and indemnification costs. Not every corporate lawyer knows the coverage area. However, lawyers who specialize in coverage for the policyholder know how to get the insured the access to the defense and indemnity dollars to which they are entitled. It is time for American industry to get the coverage it deserves. The spate of lawsuits may not be stopped, but the insurers can be required to defend against them, and the business of America will then be business once more.



References

2 Statistical Abstract of the United States, 71st Ed., 1950, page 756; Statistical Abstract of the United States, 2000, 120th Ed., Table 865, page 542.

3 Statistical Abstract of the United States, 2000, 120th Ed., Table, 865, page 542; Statistical Abstract of the United States, 2006, 126th Ed., Table 736, page 495.

4 U.S. Census Bureau, Foreign Trade Division, “U.S. Trade in Goods and Services – Balance of Payments 1960 thru 2006, http://www.census.gov/goreigh-trade/statistics/historical/gands.txt.

5 U.S. Census Bureau, Foreign Trade Division, “U.S. Trade in Goods and Services – Balance of Payments 1960 thru 2006, http://www.census.gov/goreigh-trade/statistics/historical/gands.txt; Max Morgenthaler, “The Death of American Manufacturing,” unpublished paper, 2006, page 4.

6 Survey on Lawyer Disciplinary Systems, 1998, ABA Center for Professional Responsibility, Chart I, “State by State Processing Statistics, 1998; Survey on Lawyer Disciplinary Systems, 2005, ABA Center for Professional Responsibility, Chart I, “Layer Population and Agency Caseload Volume, 2005.

7 Susan Warren, “As Asbestos Mess Spreads, Sickest See Payouts Shrink,” Wall Street Journal, April 25, 2002.

8 Id.

9 Id.

10 Fiberglass Information Network, Home Page, Copyright 1991-2002, Fiberglass Information Network.

11 Deborah C. Glass et al., “Leukemia Risk Associated with Low-Level Benzene Exposure,” Epidemiology, Vol. 14, No. 5, September 2003, page 569.

12 Id.

13 Leukemia & Lymphoma Society website, www.leukemia-lymphoma.org.

14 Id.

15 Id.

16 Id.

17 Howard E. Jarvis, Esq. and Dean T. Howell, Esq., “Trace Benzene Cases in the Real World:  Is a Trace Benzene Case Really a Benzene Case?” Litigation Watch: Benzene, June 2005, page 1.

18 Kevin C. Mayer and Ashley M. Silberfeld, “Tracing the Path through Trace Benzene Litigation: The Road Goes through the Experts,” Toxic Torts and Environmental Law, page 109, March, 2007

19 A.J. McMichael, “Carcinogenicity of Benzene, Toluene and Xylene:  Epidemiological and Experimental Evidence,” IARC Sci. Publ. 1988;(85):3-18.

20 Castello v. Chevron USA, 97 F. Supp. 2d 780, 786 (S.D. Tex. 2000).

21 Id.

Share This Story

Looking for a reprint of this article?
From high-res PDFs to custom plaques, order your copy today!

Kenneth Anspach, Attorney | Anspach & Associates, Chicago, IL
Kenneth Anspach is a Chicago attorney (Anspach & Associates, 8 South Michigan Avenue, Suite 3400, Chicago, IL 60603; 312-407-7888) concentrating in insurance coverage and environmental litigation. He represents manufacturers, environmental entities and financial institutions. Mr. Anspach is a former Illinois Assistant Attorney General and Hearing Officer for the Illinois Pollution Control Board.

Recommended Content

JOIN TODAY
to unlock your recommendations.

Already have an account? Sign In

  • pci1022-Kinaltek-Lead-1170.jpg

    A Novel Pigment Production Technology

    Following an extensive R&D program that demonstrated...
    Paint and Coating Pigments
    By: Jawad Haidar and Nitin Soni
  • pci global top 10

    2025 Global Top 10: Top Paint and Coatings Companies

    The following is PCI’s annual ranking of the top 10...
    Global Top 10 and PCI 25
    By: Courtney Bassett
  • 2025 pci 25

    2025 PCI 25: Top Paint and Coatings Companies

    PCI's annual ranking of the top 25 North American paint...
    Global Top 10 and PCI 25
    By: Courtney Bassett
You must login or register in order to post a comment.

Report Abusive Comment

Manage My Account
  • eMagazine
  • Newsletters
  • Online Registration
  • Subscription Customer Service

More Videos

Sponsored Content

Sponsored Content is a special paid section where industry companies provide high quality, objective, non-commercial content around topics of interest to the PCI audience. All Sponsored Content is supplied by the advertising company and any opinions expressed in this article are those of the author and not necessarily reflect the views of PCI or its parent company, BNP Media. Interested in participating in our Sponsored Content section? Contact your local rep!

close
  • wooden kitchen set and shelving
    Sponsored bySirca North America

    Leveraging Coatings to Meet ESG Goals in Manufacturing

  • man woodworking in workshop
    Sponsored byGemini Industries, Inc.

    Waterborne Coatings Aren't the Future -- They're the New Performance Benchmark

Popular Stories

Akzo, SW, Nippon Logos

AkzoNobel Rejects Cash Offer From Nippon Paint, Sherwin-Williams

BASF SE Logo

BASF Announces Strategic Business Sale

AkzoSWNipponEndTalks

Nippon Paint, Sherwin-Williams End AkzoNobel Pursuit

POB-Point-and-Shoot

PCI Buyers Guide

Submit a Request for Proposal (RFP) to suppliers of your choice with details on what you need with a click of a button

Start your RFP

Browse our Buyers Guide for manufacturers and distributors of all types of coatings products and much more!

Find Suppliers

Events

September 4, 2025

N-Butylpyrrolidone (NBP) as a Green Solvent to Replace N-Methylpyrrolidone (NMP) in Industrial Coating Applications

ON DEMAND: EPA published a regulation proposal around N-methylpyrrolidone (NMP) in June 2024 to ban or limit NMP in many applications, such as paints and coatings and their removers. N-butylpyrrolidone (NBP) is a powerful and versatile solvent for a variety of industries looking for alternatives to substance of very high concern (SVHC)-listed solvents.

September 15, 2026

Coatings Trends & Technologies Summit

The Coatings Trends & Technologies (CTT) Summit is an annual conference for both liquid and powder coatings formulators and manufacturers to discuss innovations in coatings technology. This event combines high-quality technical presentations, a resource-rich exhibit hall, and dedicated networking opportunities to connect scientific minds, foster innovation, and cultivate game-changing new ideas!

View All Submit An Event

Poll

Longest-running laboratory experiment

What is the longest-running laboratory experiment?
View Results Poll Archive

Products

Automotive Paints and Coatings, 2nd Edition

Now in its second edition and still the only book of its kind, this is an authoritative treatment of all stages of the coating process.

See More Products
Inside the AI Shift in Coatings - See the article now

Related Articles

  • pci0221-Apollo-1174350493-900.jpg

    Like a Sheen Caught in Headlights

    See More
  • LyondellBasell Contributing to Relief Efforts for Japan

    See More
  • Lincoln Memorial Pool Coating

    Lawsuit Puts Reflecting Pool Coating Project in the Spotlight

    See More

Related Products

See More Products
  • durability.jpg

    Increasing the Durability of Paint and Varnish Coatings in Building Products and Construction 1st Edition

  • Kevin-Biller-PC-BOOK.jpg

    Powder Coatings - Foundation for the Novice Formulator (ebook)

See More Products

Related Directories

  • The Kish Company LLC

    Established in 1986, The Kish Company has been a leading supplier of industrial minerals, extenders, additives, and pigments to the plastics, paint, rubber, ink, adhesive, and sealant industries.
×

Keep the info flowing with our eNewsletters!

Get the latest industry updates tailored your way.

JOIN TODAY!
  • RESOURCES
    • Advertise
    • Contact Us
    • Directories
    • Store
    • Want More
    • Manufacturing Division
  • SIGN UP TODAY
    • Create Account
    • eMagazine
    • Newsletters
    • Customer Service
    • Manage Preferences
  • SERVICES
    • Marketing Services
    • Reprints
    • Market Research
    • List Rental
    • Survey & Sample
  • STAY CONNECTED
    • LinkedIn
    • Facebook
    • Youtube
    • X (Twitter)
  • PRIVACY
    • PRIVACY POLICY
    • TERMS & CONDITIONS
    • DO NOT SELL MY PERSONAL INFORMATION
    • PRIVACY REQUEST
    • ACCESSIBILITY

Copyright ©2026. All Rights Reserved BNP Media, Inc. and BNP Media II, LLC.

Design, CMS, Hosting & Web Development :: ePublishing